Critical Cooling Rate for the Glass Formation of Ferromagnetic Fe80P13C7 Alloy
被引:1
作者:
Kai XU
[1
]
Yan WANG
[1
]
Jinfeng LI
[1
]
Qiang LI
[1
,2
]
机构:
[1] School of Physics Science and Technology, Xinjiang University
[2] State Key Laboratory of Powder Metallurgy, Central South University
基金:
中国国家自然科学基金;
关键词:
Glass formation ability;
Critical cooling rate;
Fe80P13C7;
alloy;
D O I:
暂无
中图分类号:
TG141 [黑色金属材料];
学科分类号:
080502 ;
摘要:
In this paper the critical cooling rate, Rc, for the glass formation of Fe80P13C7 alloy has been determined using both Uhlmann’s and Barandiaran-Colmenero’s method. In Uhlmann’s method, all kinds of the expressions of △Gl-s (T) and η (T) determined using the different modes and methods had been investigated. It is indicated that the R c for the glass formation of Fe80P13C7 alloy can be estimated to be 349 K/s by Uhlmann’s method based on the appropriate expressions of △Gl-s (T) and η (T). The calculated result accords with our experimental result. The R c for the glass formation of Fe80P13C7 alloy has also been determined to be 0.49 K/s using Barandiaran-Colmenero’s method. This resultant R c is unreasonable low and it indicates that Barandiaran-Colmenero’s method does not suit to Fe-based alloy.
引用
收藏
页码:56 / 62
页数:7
相关论文