Rietveld refinement, microstructure and high-temperature oxidation characteristics of low-density high manganese steels

被引:0
作者
Zhenyi Huang [1 ,2 ]
Yueshang Jiang [1 ,2 ]
Along Hou [1 ,2 ]
Ping Wang [1 ,2 ,3 ]
Qi Shi [2 ,3 ]
Qingyu Hou [1 ,2 ]
Xianghua Liu [1 ]
机构
[1] School of Metallurgical Engineering, Anhui University of Technology
[2] Key Laboratory of Metallurgical Emission Reduction & Resources Recycling, Ministry of Education, Anhui University of Technology
[3] Industrial & Commercial College, Anhui University of Technology
基金
中国国家自然科学基金;
关键词
High manganese steel; Low-density steel; Rietveld method; Microstructure; Oxidation;
D O I
暂无
中图分类号
TG142.1 [钢的组织与性能];
学科分类号
080502 ;
摘要
Three forged low-density high manganese steels Mn28Al10,Mn28Al8 and Mn20Al10 were used as experimental materials in this study.The forged microstructure and external oxidation characteristics at 1323 K and 1373 K for 5–25 h in air were investigated by microstructural observation and X-ray diffraction(XRD)technique.The phase compositions and abundance in the forged and oxidized samples were quantitatively obtained by Rietveld method on the basis of XRD pattern analysis.The results showed that an austenitic microstructure formed in steels Mn28Al10 and Mn28Al8,and 18.02 wt%ferrite could be found in Mn20Al10.The relative amount of;.28 wt%-carbide(Fe;AlC;)in Mn28Al10 was far greater than that in Mn28Al8 and Mn20Al10.The oxidation kinetics of forged steels oxidized at 1323 K for 5–25 h had two-stage parabolic rate laws;and the oxidation rate of the first stage was lower than that of the second stage.When they were oxidized at 1373 K for 5–25 h,the oxidation kinetics followed only a parabolic law and the oxidation rates were respectively greater than those at 1323 K for 5–25 h.When they were oxidized at 1323 K for 25 h,detached external scales contained Fe;MnO;and-Fe;O;oxides.-Al;O;and(Fe,Mn);O;oxides could only be indexed in steels Mn28Al8 and Mn28Al10,respectively.When they were oxidized at 1373 K for 25 h,Fe;MnO;,Fe;O;,-Fe;O;and-Al;O;oxides could all be indexed in the external detached scales.The main phase of detached external scales was Fe;MnO;;and the relative amount of-Al;O;in steel Mn28Al8 was higher than that in steels Mn28Al10 and Mn20Al.The external oxidation layers of these three forged steels oxidized at 1323 K and 1373 K for 25 h were essentially followed the sequence of-Al;O;,Fe;MnO;,Fe;O;,FeMnO;,and Fe;O;from the substrate to the outside surface.The forged Mn28Al10 steel with austenitic microstructure and a certain amount of-carbide(;.28 wt%in the present work)possessed a better combination of strength,ductility,specific strength,and oxidation rate when compared to that of the forged Mn28Al8 and Mn20Al10 steels.
引用
收藏
页码:1531 / 1539
页数:9
相关论文
共 50 条
  • [31] Effect of microstructure on the low temperature toughness of high strength pipeline steels
    Zeng, Yan-ping
    Zhu, Peng-yu
    Tong, Ke
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2015, 22 (03) : 254 - 261
  • [32] Effect of microstructure on the low temperature toughness of high strength pipeline steels
    Yan-ping Zeng
    Peng-yu Zhu
    Ke Tong
    International Journal of Minerals Metallurgy and Materials, 2015, 22 (03) : 254 - 261
  • [33] Effect of microstructure on the low temperature toughness of high strength pipeline steels
    Yan-ping Zeng
    Peng-yu Zhu
    Ke Tong
    International Journal of Minerals, Metallurgy, and Materials, 2015, 22 : 254 - 261
  • [34] High-Temperature Air and Steam Oxidation and Oxide Layer Characteristics of Alloy 617
    Archana, M.
    Rao, Ch Jagadeeswara
    Ningshen, S.
    Philip, John
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (02) : 931 - 943
  • [35] High-temperature oxidation of graphite
    Ariharan, S.
    Balani, Kantesh
    Hazra, Manis
    NANOMATERIALS AND ENERGY, 2018, 7 (02) : 37 - 43
  • [36] High-temperature oxidation behavior and scale morphology of Si-containing steels
    Kusabiraki, Kiyoshi
    Watanabe, Ryoko
    Ikehata, Tomoharu
    Takeda, Mikako
    Onishi, Takashi
    Guo, Xiping
    ISIJ INTERNATIONAL, 2007, 47 (09) : 1329 - 1334
  • [37] High-temperature antioxidant silicate coating of low-density Nb-Ti-Al alloy: A review
    Tang, Xiaohuan
    Zhao, Gang
    Liu, Jian
    Wang, Qiang
    Bai, Xiaodong
    Wang, Lifei
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2024, 43 (01)
  • [38] Achieving excellent strength and ductility synergy by δ phase strengthening in low-density high-manganese steel
    Niu, Gang
    Jin, Donghao
    Gong, Na
    Misra, R. D. K.
    MATERIALS TECHNOLOGY, 2023, 38 (01)
  • [39] Study on high-temperature oxidation of TiZrHfNbTaV high-entropy alloy
    Shangguan, Zixuan
    Ma, Shuo
    Li, Jun
    Liu, Panmei
    Wang, Zumin
    MATERIALS LETTERS, 2024, 360
  • [40] High-Temperature Oxidation Behavior of Cr-Ni-Mo Hot-Work Die Steels
    Zhang, Yuqi
    Zhang, Cheng
    Li, Fei
    Wang, Zhou
    Wang, Xiaodong
    Wang, Changji
    Zhang, Chen
    Huang, Jinfeng
    Mao, Feng
    Chen, Chong
    Jiang, Tao
    Wei, Shizhong
    Xiong, Mei
    Hu, Jinmeng
    MATERIALS, 2022, 15 (15)