Characterizations of precipitation behavior of Al-Mg-Si alloys under different heat treatments

被引:0
|
作者
Hui Li [1 ,2 ]
Jia-yi Wang [3 ]
Hai-tao Jiang [3 ]
Zheng-feng Lü [2 ]
Zhen-feng Zhu [1 ]
机构
[1] College of Engineering, Yantai Nanshan University
[2] National Engineering Research Center for Plastic Working of Aluminum Alloys, Shandong Nanshan Aluminum Co., Ltd.
[3] Institute of Engineering Technology, University of Science and Technology Beijing
关键词
Al-Mg-Si alloy; heat treatment; precipitation behavior; electrical resistivity;
D O I
暂无
中图分类号
TG166.3 [铝及其合金的热处理];
学科分类号
080201 ; 080503 ;
摘要
The solidification-precipitation behavior of Al-Mg-Si multicomponent alloys has long been an absorbing topic. Experiments were carried out to analyze the precipitation behaviors of Al-Mg-Si alloys under different heat treatments. All specimens were homogenized at 570 °C for 8 h, and then solution treated at 540 °C for 55 min. Subsequently, the specimens were age treated for different times at temperatures of 100 °C, 150 °C and 180 °C, respectively. The experimental results show that the occurrence of dispersed free zones(DFZ) is caused by the uneven distribution of dispersed phase. During the aging process, pre-β″ phases form at the initial stage and an aging temperature of 100 °C is too low to complete the transformation of pre-β″ to β″. At 150 °C, the precipitation sequence is concluded as SSSS-pre-β″-pre-β″+β″-β″-β′-β. Moreover, changes in sizes and densities of the pre-β″, β″and β′ phases during the aging process has an important influence on the evolution of microhardness and electrical resistivity. The microhardness peak value of 150 °C is similar to that of 180 °C, which is ~141 HV. While, at 100 °C, the microhardness increases slowly, and the attainable value is 127 HV up to 19 days. When the aging temperature is 100 °C, the electrical resistivity has the highest average value. When the aging temperature exceeds 100 °C, with the occurrence and growth of β″and β′, the resistivity has a distinct decrease with prolonged aging time.
引用
收藏
页码:89 / 96
页数:8
相关论文
共 50 条
  • [41] Effects of Cu additions on the precipitation activation energy and mechanical properties of prestrained Al-Mg-Si alloys
    Cui, Min
    Jo, Yong Hee
    Kayani, Saif Haider
    Kim, Hyoung-Wook
    Lee, Je-Hyun
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 20 : 2629 - 2637
  • [42] STUDY ON THE KINETICS OF PHASE TRANSFORMATION β → α IN THE HOMOGENEOUS HEAT TREATMENT OF Al-Mg-Si SERIES ALLOYS
    Cao Lingyong
    Guo Mingxing
    Cui Hua
    Cai Yuanhua
    Zhang Qiaoxia
    Hu Xiaoqian
    Zhang Jishan
    ACTA METALLURGICA SINICA, 2013, 49 (04) : 428 - 434
  • [43] Corrosion mechanism associated with Mg2Si and Si particles in Al-Mg-Si alloys
    Zeng Feng-li
    Wei Zhong-ling
    Li Jin-feng
    Li Chao-xing
    Tan Xing
    Zhang Zhao
    Zheng Zi-qiao
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2011, 21 (12) : 2559 - 2567
  • [44] Effect of Cu and excess Si on mechanical properties in Al-Mg-Si alloys
    Matsuda, K
    Kido, K
    Uetani, Y
    Ikeno, S
    PRICM 4: FORTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, VOLS I AND II, 2001, : 2619 - 2622
  • [45] Variation of age-hardening behavior of TM-addition Al-Mg-Si alloys
    Wang, Shumei
    Matsuda, Kenji
    Kawabata, Tokimasa
    Yamazaki, Toshinari
    Ikeno, Susumu
    JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (41) : 9876 - 9883
  • [46] Research on the ultra-low temperature tensile deformation mechanism of Al-Mg-Si alloys in different heat treatment states
    Fu, Yunfan
    Chen, Canyang
    Liu, Xuefeng
    Huang, Shiquan
    Mao, Juncheng
    Yi, Youping
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
  • [47] Natural ageing clustering under different quenching conditions in an Al-Mg-Si alloy
    Yang, Zi
    Jiang, Xiaohe
    Zhang, Xingpu
    Liu, Meng
    Liang, Zeqin
    Leyvraz, David
    Banhart, John
    SCRIPTA MATERIALIA, 2021, 190 : 179 - 182
  • [48] Influence of Minor Zn Addition on Precipitation Behavior and Intergranular Corrosion Properties of Al-Mg-Si Alloy
    Chi, Shuiqing
    Deng, Yunlai
    Xu, Xuehong
    Guo, Xiaobin
    MATERIALS, 2020, 13 (03)
  • [49] Effect of cold rolling and aging treatment on mechanical property and precipitation behavior in a Al-Mg-Si alloy
    Kang, SB
    Zhen, L
    Kim, HW
    Lee, ST
    ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 1996, 217 : 827 - 832
  • [50] Optimizing the strength-ductility balance of microalloyed Al-Mg-Si casting alloys
    Luo, T. R.
    Fan, Z. Z.
    Hu, H. X.
    Tian, Y. Z.
    MATERIALS LETTERS, 2025, 378