Structure and electrochemical characteristics of LaNi5-Ti0.10Zr0.16V0.34Cr0.10Ni0.30 composite alloy electrode

被引:5
|
作者
王艳芝 [1 ,2 ]
赵敏寿 [1 ,2 ]
机构
[1] College of Environmental and Chemical Engineering, Yanshan University
[2] State Key Laboratory of Metastable Materials Science and Technology, Yanshan University
关键词
Ni/MH battery; metal hydride electrode; composite alloy; electrochemical properties; kinetic properties; rare earths;
D O I
暂无
中图分类号
O611.3 [性质];
学科分类号
070301 ; 081704 ;
摘要
Composite LaNi5+x wt.% Ti0.10Zr0.16V0.34Cr0.10Ni0.30 (x=0, 1, 5, 10) alloys were prepared by two-step re-melting. X-ray diffractometer (XRD), scanning electron microscopy (FESEM), energy dispersive spectrometry (EDS), inductively coupled plasma (ICP) and electrochemical impedance spectroscopy (EIS) analyses showed that the matrix phase of LaNi5 alloy with CaCu5 structure remained unchanged after additive alloy was added, the amount of the second phase increased with increasing x. The synergetic effect within constituent alloys appeared during the composite process. The electrochemical characteristics of the composite alloy electrodes were greatly improved, and the optimum composition was x=5, at which the low temperature dischargeability at 233 K was 87.37 %, and the maximum discharge capacity and the high rate dischargeability at discharge current density of 1800 mA/g were 326.1 mAh/g and 71.98 % at 303 K, respectively. The HRD was controlled by both the charge-transfer reaction of hydrogen on the electrode/electrolyte interface and hydrogen diffusion coefficient in the bulk of the alloys at discharge current density of 1800 mA/g.
引用
收藏
页码:774 / 780
页数:7
相关论文
共 34 条
  • [21] Microstructure and Self-discharge Characteristic of Ti-Zr-V-Cr-Ni-Ce Hydrogen Storage Electrode Alloy
    Qiao, Yu Qing
    Zhao, Min Shou
    Wang, Li Min
    RENEWABLE AND SUSTAINABLE ENERGY II, PTS 1-4, 2012, 512-515 : 1409 - +
  • [22] Effect of Ni addition on phase structure and electrochemical properties of Ti0.4Zr0.1V1.1Mn0.5Cr0.1 alloy
    Hang Zhou-Ming
    Zhao Min-Shou
    Qiao Yu-Qing
    Zhu Xin-Jian
    Cao Guang-Yi
    CHINESE JOURNAL OF INORGANIC CHEMISTRY, 2006, 22 (12) : 2141 - 2146
  • [24] Crystal structure and some dynamic performances of Ti0.25V0.34Dy0.01Cr0.1Ni 0.3 hydrogen storage electrode
    Qiao, Yu Qing
    Zhao, Min Shou
    Zhang, Qiu Ming
    Zhai, Jing
    CHINESE CHEMICAL LETTERS, 2011, 22 (01) : 93 - 96
  • [25] Examination of Multiphase (Zr,Ti)(V,Cr,Mn,Ni)2 Ni-MH Electrode Alloys: Part I. Dendritic Solidification Structure
    Boettinger, W. J.
    Newbury, D. E.
    Wang, K.
    Bendersky, L. A.
    Chiu, C.
    Kattner, U. R.
    Young, K.
    Chao, B.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2010, 41A (08): : 2033 - 2047
  • [26] Microstructure and some dynamic performances of Ti0.17Zr0.08V0.34RE0.01Cr0.1Ni0.3 (RE = Ce, Dy) hydrogen storage electrode alloys
    Qiao, Yuqing
    Zhao, Minshou
    Zhu, Xinjian
    Cao, Guangyi
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2007, 32 (15) : 3427 - 3434
  • [27] MICROSTRUCTURE AND ELECTROCHEMICAL CHARACTERISTICS OF Zr0.9Ti0.1(Ni1.1Mn0.7V0.2)x METAL HYDRIDE ELECTRODE
    S.M.Han
    M.S.Zhao
    Y.Z.Zeng
    Acta Metallurgica Sinica(English Letters), 2003, (03) : 192 - 196
  • [28] The phase structure and electrochemical properties of the melt-spun alloy Zr0.7Ti0.3Mn0.4V0.4Ni1.2
    Zhang, SK
    Wang, QD
    Lei, YQ
    Lü, GL
    Chen, LX
    Wu, F
    JOURNAL OF ALLOYS AND COMPOUNDS, 2002, 330 : 855 - 860
  • [29] Effects of Boron Addition on Microstructures and Electrochemical Properties of (Ti0.65Zr0.30)1.10(V0.5Mn0.3Cr0.4Ni0.8)Bx Hydrogen Storage Alloys
    Pan Chongchao
    Liu Xiaofang
    Yu Ronghai
    RARE METAL MATERIALS AND ENGINEERING, 2010, 39 (11) : 2023 - 2026
  • [30] Effect of substitution of chromium for nickel on structure and electrochemical characteristic of Ti0.26Zr0.07V0.24Mn0.1Ni0.33 multi-phase hydrogen storage alloy
    Li Shucun
    Zhao Minshou
    Zhai Jing
    Wang Fengyan
    MATERIALS CHEMISTRY AND PHYSICS, 2009, 113 (01) : 96 - 102