摘要
In order to explore the behavior laws of sinter reduction in TGR-OBF ( top gas recycling-oxygen blast furnace ), reduction experiments of sinter have been conducted by thermal balance mass loss method with different atmospheres , temperatures and volume flows.The changes of RI ( reduction degree of Fe 2 O 3 ), RI′ ( reduction rate of Fe 2 O 3 ) and r ( reduction degree of FeO ) have been examined.The results show that the reduction of sinter was significantly improved under TGR-OBF atmosphere , and the RIand r were measured up to 98.2%and 97.8%at 900℃ respectively.With increasing of the reduction temperature , the reduction of sinter speeded up greatly , and the reduction time-duration shortened from 117min at 900 ℃ to 63min at 1 100 ℃.Moreover , the reduction of sinter enhanced with increasing of the reductive gas flow.When the flow increased from 10to 15L / min , the initial reduction rate of sinter increased from 2.47% / min to 3.73% / min.While increasing H2and CO contents in the reductive atmosphere , the reduction of sinter was promoted.Besides , H 2 influenced more evidently than CO to the reduction of sinter , especially in the later stage of the reduction process , for instance , the reduction of wustite will be improved enormously when increasing the H2content in the reductive atmosphere.
引用
收藏
页码:13 / 19
页数:7
相关论文
共 50 条
  • [21] Numerical analysis of carbon saving potential in a top gas recycling oxygen blast furnace
    She, Xue-feng
    An, Xiu-wei
    Wang, Jing-song
    Xue, Qing-guo
    Kong, Ling-tan
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2017, 24 (06) : 608 - 616
  • [22] REDUCTION BEHAVIOR OF SINTER UNDER BLAST-FURNACE CONDITIONS
    OKAMOTO, A
    NAITO, M
    ONO, K
    HAYASHI, Y
    INOUE, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (10): : 1529 - 1536
  • [23] REDUCTION DEGRADATION BEHAVIOR OF SINTER IN THE BLAST-FURNACE SHAFT
    NAKAJIMA, R
    SUMIGAMA, T
    WAKIMOTO, K
    NAGANO, S
    KAWATA, H
    SAKURAI, M
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 73 (15): : 1964 - 1971
  • [24] Numerical analysis of blast furnace operations with top gas recycling
    Nogami, H.
    Chu, M.
    Yagi, J.-I.
    REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES, 2005, 102 (03): : 189 - 197
  • [25] Optimization of Blast Furnace Operation Under Top Gas Recycling
    Helle, Hannu
    Helle, Mikko
    Pettersson, Frank
    Saxen, Henrik
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2009, 16 : 613 - 618
  • [26] Mathematical Modeling of the Energy Consumption and Carbon Emission for the Oxygen Blast Furnace with Top Gas Recycling
    Jin, Peng
    Jiang, Zeyi
    Bao, Cheng
    Lu, Yuanxiang
    Zhang, Jianliang
    Zhang, Xinxin
    STEEL RESEARCH INTERNATIONAL, 2016, 87 (03) : 320 - 329
  • [27] BEHAVIOR OF SINTER IN THE BLAST FURNACE.
    Kong Lingtan
    Kang T'ieh/Iron and Steel (Peking), 1982, 17 (11): : 18 - 32
  • [28] Top gas recycling blast furnace developments for 'green' and sustainable ironmaking
    van der Stel, J.
    Louwerse, G.
    Sert, D.
    Hirsch, A.
    Eklund, N.
    Pettersson, M.
    IRONMAKING & STEELMAKING, 2013, 40 (07) : 483 - 489
  • [29] Effects of top gas recycling on in-furnace status, productivity, and energy consumption of oxygen blast furnaceN
    Liu, Lianzhi
    Jiang, Zeyi
    Zhang, Xinru
    Lu, Yuanxiang
    He, Junkai
    Wang, Jingsong
    Zhang, Xinxin
    ENERGY, 2018, 163 : 144 - 150
  • [30] REDUCTION DEGRADATION OF SINTER IN BLAST-FURNACE
    SOMA, H
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1988, 28 (07) : 590 - 590