Investigation on hot deformation behavior of AZ31 magnesium alloy

被引:0
|
作者
汪凌云
机构
[1] Chongqing University Chongqing 400044
[2] College of Materials Science and Engineering
[3] P. R. China
关键词
magnesium alloy; deformation behavior; dynamic recrystallization;
D O I
暂无
中图分类号
TG146.2 [轻有色金属及其合金];
学科分类号
摘要
The hot compressive deformation of extruded AZ31magnesium alloy with the mass fractions of Al and Zn equal to 3 % and 1 % respectively is studied by a Gleeble-1500D thermal mechanical simulator over the temperature range from 200 ℃ to 400 ℃ and the strain rate from 10-3 s-1 to 100 s-1. The true stress-strain curves of the strain of 65 % are tested. The deformation activation energy is obtained and the flow stress model is established by analyzing the effects of strain rate and temperature on the flow stress. Zener-Hollomon parameter is introduced to describe the softening behaviors of AZ31 magnesium alloy resulted from dynamic recrystallization during the hot compressive deformation, whose natural logarithm is linear with the critical strain of dynamic recrystallization.
引用
收藏
页码:57 / 59
页数:3
相关论文
共 50 条
  • [1] Hot Deformation Kinetics of Magnesium Alloy AZ31
    汪凌云
    黄光杰
    Journal of Wuhan University of Technology(Materials Science Edition), 2006, (03) : 15 - 17
  • [2] Hot deformation kinetics of magnesium alloy AZ31
    Wang Lingyun
    Huang Guangjie
    Fan Yonge
    Lu Zhiwen
    Pan Fusheng
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2006, 21 (03): : 15 - 17
  • [3] Hot deformation kinetics of magnesium alloy AZ31
    Wang L.
    Huang G.
    Fan Y.
    Lu Z.
    Pan F.
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2006, 21 (3): : 15 - 17
  • [4] An investigation to double hit deformation behavior of AZ31 magnesium alloy
    Shamsi, M.
    Zarei Hanzaki, A.
    Naei, H.
    10TH ESAFORM CONFERENCE ON MATERIAL FORMING, PTS A AND B, 2007, 907 : 1301 - +
  • [5] Hot deformation behavior of a spray-deposited AZ31 magnesium alloy
    LI Yongbinga
    RareMetals, 2009, 28 (01) : 91 - 97
  • [6] Hot deformation behavior of a spray-deposited AZ31 magnesium alloy
    Li Yongbing
    Chen Yunbo
    Cui Hua
    Ding Jie
    Zuo Lingli
    Zhang Jishan
    RARE METALS, 2009, 28 (01) : 91 - 97
  • [7] Isochronal annealing behavior of magnesium alloy AZ31 after hot deformation
    Yang, XY
    Miura, H
    Sakai, T
    MATERIALS TRANSACTIONS, 2005, 46 (12) : 2981 - 2987
  • [8] Hot deformation behavior of a spray-deposited AZ31 magnesium alloy
    Yongbing Li
    Yunbo Chen
    Hua Cui
    Jie Ding
    Lingli Zuo
    Jishan Zhang
    Rare Metals, 2009, 28 : 91 - 97
  • [9] Effect of homogenization on the hot deformation behavior of cast AZ31 magnesium alloy
    Prasad, Y. V. R. K.
    Rao, K. P.
    MATERIALS & DESIGN, 2009, 30 (09) : 3723 - 3730
  • [10] Hot compressive deformation of rheocast AZ31 magnesium alloy
    Yang Bicheng
    Zhang Shaoming
    Xu Jun
    Shi Likai
    Fan, Z.
    SEMI-SOLID PROCESSING OF ALLOYS AND COMPOSITES, 2006, 116-117 : 742 - 745