High-temperature oxidation behavior of SiBN fibers in air

被引:0
|
作者
Xin LONG [1 ]
Zhenyu WU [1 ]
Changwei SHAO [1 ]
Xiaozhou WANG [1 ]
Yingde WANG [1 ]
机构
[1] Science and Technology on Ceramic Fibers and Composites Laboratory, College of Aerospace Science and Engineering, National University of Defense Technology
基金
中国国家自然科学基金;
关键词
D O I
暂无
中图分类号
V25 [航空用材料]; TQ342 [合成纤维];
学科分类号
0805 ; 080502 ;
摘要
SiBN fibers are one of the most admirable microwave-transparent reinforced materials for high Mach number aircrafts.Currently,the detailed high-temperature oxidation behavior of SiBN fibers has not been studied yet.In this work,we studied the high-temperature oxidation behavior of SiBN fibers with different boron contents at the temperature range of 1000–1400℃in air.Si BN fibers started to be oxidized at 1100℃,with SiNand BN phase oxidized to SiOand BO,respectively.Due to the gasification and the escape of molten BOat high temperatures,amorphous SiOcould be remained at the fiber surface.As the fiber further oxidized,the molten BOat the inside may infiltrate into the fiber interior to react with SiN,causing the precipitation of hexagonal boron nitride (h-BN) nanoparticles and the formation of SiO/BN layer.Finally,complex oxidation layers with two distinct concentric sublayers accompanied with two transition sublayers could be formed after the oxidizing treatment.
引用
收藏
页码:768 / 777
页数:10
相关论文
共 50 条
  • [21] OXIDATION BEHAVIOR OF BINARY TI-AL ALLOYS IN HIGH-TEMPERATURE AIR ENVIRONMENT
    SHIDA, Y
    ANADA, H
    MATERIALS TRANSACTIONS JIM, 1993, 34 (03): : 236 - 242
  • [22] OXIDATION OF ZIRCALOY-4 WITH HIGH-TEMPERATURE AIR
    SULISTIJONO
    BOUDEN, A
    CHERFAOUI, M
    BERANGER, G
    LAMBERTIN, M
    JOURNAL DE PHYSIQUE IV, 1993, 3 (C9): : 439 - 445
  • [24] HIGH-TEMPERATURE OXIDATION AND DESTRUCTION OF METAL FILAMENTS IN AIR
    Orlovskaya, S. G.
    Shkoropado, M. S.
    Karimova, F. F.
    UKRAINIAN JOURNAL OF PHYSICS, 2011, 56 (12): : 1311 - 1314
  • [25] HIGH-TEMPERATURE OXIDATION OF CHROMIUM(II) SULFIDE IN AIR
    BEREZANSKAYA, VI
    LAVRENKO, VA
    POMYTKIN, AP
    SHEMET, VZ
    SOVIET POWDER METALLURGY AND METAL CERAMICS, 1991, 30 (11): : 945 - 948
  • [26] HIGH-TEMPERATURE OXIDATION OF COMMERCIALLY PURE TITANIUM IN THE AIR
    TAKAYAMA, I
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (13): : 1639 - 1639
  • [27] HIGH-TEMPERATURE OXIDATION OF VANADIUM AND CARBIDE OXIDATION AT LOW AIR PRESSURES
    ASKAROVA, LK
    ZHILYAEV, VA
    ZHURNAL NEORGANICHESKOI KHIMII, 1994, 39 (07): : 1105 - 1108
  • [28] High-temperature oxidation behavior of Co-doped WB2 ceramics in air
    Ma, Ke
    Cao, Xiaozhou
    Xue, Xiangxin
    Xu, Jingjun
    Zuo, Jun
    Li, Meishuan
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2021, 99
  • [29] High-temperature stability and oxidation behavior of SiOC/HfO2 ceramic nanocomposite in air
    Sun, Jia
    Li, Tao
    Reitz, Andreas
    Fu, Qiangang
    Riedel, Ralf
    Yu, Zhaoju
    CORROSION SCIENCE, 2020, 175
  • [30] THE INFLUENCE OF TERNARY ELEMENT ADDITION ON THE OXIDATION BEHAVIOR OF TIAL INTERMETALLIC COMPOUND IN HIGH-TEMPERATURE AIR
    BHIDA, Y
    ANADA, H
    CORROSION SCIENCE, 1993, 35 (5-8) : 945 - 953