Metallurgical evaluation of austenitic stainless surfacing welding on SAE 4130 steel

被引:3
作者
de Souza Elias M. [1 ]
Paranhos R. [2 ]
机构
[1] IFF-Instituto Federal Fluminense, Macaé
[2] UENF-CCT-LAMAV, Campos dos Goytacazes
关键词
delta ferrite; microstructure; Schaeffler diagram; Surfacing welding;
D O I
10.1080/09507116.2015.1096559
中图分类号
学科分类号
摘要
Abstract: The objective of this study was to make a metallurgical evaluation of the austenitic stainless surfacing welding on the sealing area of the riser tubes made of SAE 4130 steel. The study was divided into two steps. The first step aims to determine the dilution rate and deposition rate for the minimum and maximum levels of heat input according to the welding procedure specification (WPS) for TIG and SMAW processes, followed by analysis and study on the Schaeffler diagram in order to identify the welding consumable best-suited to attend the established quality criteria. This study identified the electrode 312 as the filler material for the first layer, and the electrodes 309 and 308 for the second layer, both using the maximum heat input of the WPS and the SMAW process, with benefits to productivity. The second step has as its objective the validation of the empirical results found in the 1st step, with the execution of surfacing welds with two layers each, and the metallurgical characterization of the welded joints by mechanical testing and microstructural analysis by optical and electronic microscopy. The results of mechanical testing and microstructure were considered satisfactory, filling the adopted quality criteria. An austenitic-ferritic microstructure with delta ferrite content between 10 and 15% was observed for both layers of the surfacing. The electrode 312 assumed a prominent position in the application of the first layer of the surfacing weld on the SAE 4130 steel, according to its higher content of delta ferrite and chromium, avoiding hot cracks formation. For the second layer, both the 309 and 308 may be used. All welds were made with high heat input, ensuring increased productivity, without significant change in the physical and mechanical characteristics. © 2016 Informa UK Limited, trading as Taylor & Francis Group.
引用
收藏
页码:581 / 589
页数:8
相关论文
共 23 条
[1]  
Bhaduri A.K., Gill T.P.S., Albert S.K., Et al., Repair welding of cracked steam turbine blades using austenitic and martensitic stainless steel consumables, Nucl. Eng. Des, 206, pp. 249-259, (2001)
[2]  
Kacar R., Baylan O., An investigation of microstructure/property relationships in dissimilar welds between martensitic and austenitic stainless steel, Mater. Des, 25, pp. 317-329, (2004)
[3]  
Tsay L.W., Lin W.L., Hydrogen sulphide stress corrosion cracking of weld overlays for desulfurization reactors, Corros. Sci, 40, pp. 577-591, (1998)
[4]  
Sun Z., Han H.Y., Weldability and properties of martensitic/austenitic stainless steel joints, Mater. Sci. Technol, 10, pp. 823-829, (1994)
[5]  
Gomes J.H.F., Análise e otimização da soldagem de revestimento de chapas de aço ABNT 1020 utilização de arame tubular inoxidável austenítico, (2010)
[6]  
Welding handbook: welding processes. American Welding Society, 2, (1992)
[7]  
Specification for wellhead and Christmas tree equipment, API – specification 6A – 17th edition, (2004)
[8]  
Barbosa R.P., Tecnologia Mecânica – Metalurgia da soldagem, soldabilidade dos materiais, (2007)
[9]  
Cordeiro Filho A.C.J., Estudo da Soldabilidade e Avaliação de Corrosão Intergranular em Junta Soldada de Aço Inoxidável AISI 430 pelo Processo TIG, (2008)
[10]  
Modenesi P.J., Soldabilidade de algumas ligas metálicas, (Apostila), (2008)