摘要
The effect of hydrogen charging during plastic deformation was investigated on a ferritic steel containing TiC nano-precipitates. Specimens were subjected to a slow strain rate tensile test (SSRT) up to 0, 1, or 3% plastic engineering strain, held until a total duration of 2 h to saturate with hydrogen, then fast fractured. The specimens pre-strained elastically absorbed 2.36 wppm of hydrogen, which increased to 3.69 wppm for 3% plastic strain. Only 0.72 wppm is stored in non-dislocation traps such as precipitates, grain boundaries, and lattice sites, which makes dislocations the main contributor to hydrogen trapping. The increased hydrogen uptake did not lead to a decrease in fracture strain, which remained between 6 and 10% for all pre-strains, compared to 60% for full SSRT tests that were charged for a shorter time. This research highlights the necessity of high plastic strains and the presence of hydrogen in the environment during crack growth to cause HE in ductile steels.
引用
收藏
相关论文
共 50 条
  • [31] Measurement and prediction of hydrogen embrittlement in high strength carbon steel
    Duval, A.
    Robinson, M.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2009, 44 (05) : 340 - 346
  • [32] A cohesive zone model to simulate the hydrogen embrittlement effect on a high-strength steel
    Gobbi, G.
    Colombo, C.
    Vergani, L.
    FRATTURA ED INTEGRITA STRUTTURALE, 2016, (35): : 260 - 270
  • [33] Hydrogen embrittlement behavior of high strength bainitic rail steel: Effect of tempering treatment
    Zhang, Yongjian
    Xu, Zhibao
    Zhao, Xiaoli
    Gao, Guhui
    Hui, Weijun
    Weng, Yuqing
    ENGINEERING FAILURE ANALYSIS, 2018, 93 : 100 - 110
  • [34] Observation of hydrogen trap and hydrogen embrittlement of 430 ferritic stainless steel
    Wang, Tao
    Fang, Xueyang
    Zhang, Huiyun
    Lv, Wenjie
    Ma, Jinyao
    Liang, Wei
    Zheng, Liuwei
    MATERIALS LETTERS, 2022, 313
  • [35] Effect of cyclic plastic deformation on hydrogen diffusion behavior and embrittlement susceptibility of reeling-pipeline steel weldments
    Jiang, Yuanbo
    Li, Chengning
    Wang, Dongpo
    Di, Xinjie
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2021, 46 (58) : 30158 - 30172
  • [36] Effect of cold plastic deformation on steel impact strength
    Kaputkin, DE
    STEEL IN TRANSLATION, 1997, 27 (05) : 72 - 75
  • [37] PLASTIC-DEFORMATION - A MAJOR FACTOR IN HYDROGEN EMBRITTLEMENT OF LOW-ALLOY STEEL
    MAIER, HJ
    KAESCHE, H
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1989, 117 : L11 - L15
  • [38] Effect of vanadium on hydrogen embrittlement susceptibility of high-strength hot-stamped steel
    Chen, Wei-jian
    Gao, Peng-fei
    Wang, Shuai
    Lu, Hong-zhou
    Zhao, Zheng-zhi
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2021, 28 (02) : 211 - 222
  • [39] Effect of vanadium on hydrogen embrittlement susceptibility of high-strength hot-stamped steel
    Wei-jian Chen
    Peng-fei Gao
    Shuai Wang
    Hong-zhou Lu
    Zheng-zhi Zhao
    Journal of Iron and Steel Research International, 2021, 28 : 211 - 222
  • [40] Effect of in-situ nanoparticles on the mechanical properties and hydrogen embrittlement of high-strength steel
    Rong-jian Shi
    Zi-dong Wang
    Li-jie Qiao
    Xiao-lu Pang
    International Journal of Minerals Metallurgy and Materials, 2021, 28 (04) : 644 - 656