Impact of scandium on the microstructure, mechanical properties, corrosion behaviors and in-vitro biocompatibility of a Zn-0.1Li alloy

被引:0
|
作者
Huang, He [1 ,2 ]
Gong, Gencheng [2 ,3 ]
Yu, Hui [4 ]
Tong, Zhipei [2 ]
Jia, Qinggong [1 ]
Fang, Liudang [1 ]
Guan, Shaokang [1 ]
Nie, Jing-Jun [5 ]
Chen, Dafu [5 ]
Bai, Jing [6 ]
Bian, Dong [2 ]
Zheng, Yufeng [1 ,7 ]
机构
[1] Zhengzhou Univ, Sch Mat Sci & Engn, Zhengzhou 450003, Peoples R China
[2] Southern Med Univ, Guangdong Prov Peoples Hosp, Med Res Inst, Guangdong Acad Med Sci,Dept Orthoped, Guangzhou 510080, Peoples R China
[3] South China Univ Technol, Sch Med, Guangzhou 510006, Peoples R China
[4] Guangzhou Med Univ, Dept Orthopaed Surg, Guangzhou Key Lab Spine Dis Prevent & Treatment, Affiliated Hosp 3, Guangzhou 510515, Peoples R China
[5] Capital Med Univ, Beijing Res Inst Traumatol & Orthopaed, Natl Ctr Orthopaed, Beijing Jishuitan Hosp,Lab Bone Tissue Engn,Beijin, Beijing 100035, Peoples R China
[6] Southeast Univ, Coll Mat Sci & Engn, Nanjing 211189, Peoples R China
[7] Peking Univ, Sch Mat Sci & Engn, Beijing 100871, Peoples R China
来源
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY | 2025年 / 229卷
基金
中国国家自然科学基金;
关键词
Biodegradable zinc; Strengthening mechanism; Localized corrosion; Biocompatibility; ScZn12; phase; RECRYSTALLIZATION BEHAVIOR; PLASTIC-DEFORMATION; ZN; ZINC; CYTOCOMPATIBILITY; DIFFERENTIATION; MAGNESIUM; DESIGN; MG;
D O I
10.1016/j.jmst.2025.01.012
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The poor mechanical properties of pure zinc (Zn) restrain its applications in orthopedics, which requires high loading capacity. Alloying with lithium (Li) element can enhance strength, however, the workhardening rate is impaired with increased Li content. Here, introducing scandium (Sc) into a low Li- containing Zn-0.1Li alloy could effectively refine its microstructure, reducing the average grain size from 10 to 4 }m. The refinement in microstructure led to a significant improvement in tensile strength, improving from 257 MPa of Zn-0.1Li to 341 MPa of Zn-0.1Li-0.1Sc, meanwhile, the work-hardening rate remained positive during the whole plastic deformation stage. The addition of Sc-impaired elongation is due to numerous microcracks formed at the Zn/ScZn12 interfaces, as well as in the large-sized ScZn12 particles. Corrosion tests revealed an accelerated corrosion rate due to the galvanic effect between the Zn matrix and ScZn12 phase. Even so, the Zn-0.1Li-1.0Sc alloy still exhibited superior biocompatibility with rat/mouse mesenchymal stem cells and close osteogenesis capacity to the original Zn-0.1Li alloy. These findings demonstrated that the addition of Sc in low Li-containing alloys could improve mechanical strength without sacrificing the work-hardening rate and biocompatibility. (c) 2025 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
引用
收藏
页码:235 / 251
页数:17
相关论文
共 50 条
  • [41] Effects of solution treatment before extrusion on the microstructure, mechanical properties and corrosion of Mg-Zn-Gd alloy in vitro
    Miao, Hongwei
    Huang, Hua
    Shi, Yongjuan
    Zhang, Hua
    Pei, Jia
    Yuan, Guangyin
    CORROSION SCIENCE, 2017, 122 : 90 - 99
  • [42] Effects of alloying elements (Ca and Sr) on microstructure, mechanical property and in vitro corrosion behavior of biodegradable Zn-1.5Mg alloy
    Liu, Xiwei
    Sun, Jianke
    Qiu, Kejin
    Yang, Yinghong
    Pu, Zhongjie
    Li, Li
    Zheng, Yufeng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 664 : 444 - 452
  • [43] Microstructures, mechanical properties and in vitro corrosion behavior of biodegradable Zn alloys microalloyed with Al, Mn, Cu, Ag and Li elements
    Li, Lei
    Jiao, Huanzheng
    Liu, Congfu
    Yang, Lin
    Suo, Yusong
    Zhang, Ruixue
    Liu, Tie
    Cui, Jianzhong
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2022, 103 : 244 - 260
  • [44] Effect of Al Addition on Microstructure, Mechanical, and Corrosion Properties of Hot Extruded Mg-2.0Zn-0.4Mn Alloy
    Xiong, Yi
    Jiao, Yan-ke
    Zha, Xiao-qin
    Chen, Zheng-ge
    He, Tian-tian
    Wang, Shu-bo
    Cao, Wei
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (09) : 4620 - 4632
  • [45] Effect of nano-CaO particle on the microstructure, mechanical properties and corrosion behavior of lean Mg-1Zn alloy
    Shen, Guangxin
    Lyu, Shaoyuan
    Yu, Leiting
    Li, Tianlu
    You, Chen
    Wang, Xuewei
    Chen, Minfang
    Jiang, Bin
    JOURNAL OF MAGNESIUM AND ALLOYS, 2024, 12 (02) : 794 - 814
  • [46] Microstructure, Corrosion Behaviors in Different Simulated Body Fluids and Cytotoxicity of Zn-Li Alloy as Biodegradable Material
    Zhang, Yu
    Lu, Yujiao
    Xu, Xuemei
    Chen, Liangjian
    Xiao, Tao
    Luo, Xier
    Yan, Yang
    Li, Ding
    Dai, Yilong
    Yu, Kun
    MATERIALS TRANSACTIONS, 2019, 60 (04) : 583 - 586
  • [47] Effect of ECAP on Microstructure, Mechanical Properties, Corrosion Behavior, and Biocompatibility of Mg-Ca Alloy Composite
    Huang, Song-Jeng
    Wang, Chih-Feng
    Subramani, Murugan
    Fan, Fang-Yu
    JOURNAL OF COMPOSITES SCIENCE, 2023, 7 (07):
  • [48] In-vitro corrosion behavior and mechanical properties of biodegradable Zn alloys designed for gastrointestinal anastomosis
    Wang, Manli
    Wang, Kang
    Zhu, Xinglong
    Yang, Lijing
    Shen, Jianwei
    Lu, Ting
    Liu, Huinan Hannah
    Liu, Chen
    Song, Zhenlun
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 29 : 4941 - 4953
  • [49] Microstructure, Mechanical Properties, Corrosion Behavior and Biocompatibility of As-Extruded Biodegradable Mg-3Sn-1Zn-0.5Mn Alloy
    Hou, Lida
    Li, Zhen
    Zhao, Hong
    Pan, Yu
    Pavlinich, Sergey
    Liu, Xiwei
    Li, Xinlin
    Zheng, Yufeng
    Li, Li
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2016, 32 (09) : 874 - 882
  • [50] Microstructure evolution and enhanced mechanical properties of additive manufacturing Al-Zn-Mg-Li alloy via forging and aging treatment
    Zhang, Lihua
    Cao, Wanqing
    Zhang, Yun
    Jiang, Ripeng
    Li, Xiaoqian
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 18 : 4965 - 4979