Mechanical properties and microstructure of the C70600 copper-nickel alloy and C46500 brass joint using brazing technique

被引:0
作者
Mehdikhani, Hesam [1 ]
Mostafapour, Amir [1 ]
Binesh, Behzad [2 ]
机构
[1] Univ Tabriz, Fac Mech Engn, Tabriz, Iran
[2] Univ Bonab, Dept Mat Sci & Engn, Bonab, Iran
关键词
Cu-Nil alloy; Naval brass; Brazing; Microstructure; Mechanical properties; INTERFACIAL REACTIONS; BRAZED JOINTS; CU; FAILURE; ZN; DEFORMATION; SOLDER;
D O I
10.1016/j.jajp.2025.100294
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Naval brass (C46500), due to the presence of tin in this alloy, it exhibits high resistance to atmospheric and aqueous corrosion. This type of brass is widely used in various industries, including marine applications, electrical components, etc. The C70600 copper-nickel alloy, due to the formation of a solid solution, maintains high ductility while increasing tensile strength. High resistance to seawater corrosion, attributed to significant amounts of manganese and iron, are among the key characteristics of this alloy. The joining of these alloys in marine applications are required. Considering the formation of solid solutions and intermetallic compounds and their impact on mechanical properties, controlling their amounts is crucial for achieving optimal results. Brazing is known as an effective method to join these base materials. Since temperature and time are two critical parameters in brazing, influencing the formation of precipitates, this study focuses on optimizing these conditions to achieve desirable microstructural and mechanical properties. The brazing process was performed under 16 different conditions including 650, 680, 710, and 740 degrees C for 1, 5, 15, and 30 mins. To study the microstructure of joints, and the related phase transformations in the joint region, optical microscopy, scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDS), and X-ray diffraction (XRD) were used. Mechanical properties of the samples were evaluated through strength testing and micro hardness measurements. The results indicate that with increasing temperature and duration of the joining process, the width of the thermally solidified zone decreases due to the increased diffusion rate, while the width of the isothermal solidification zone increases. Moreover, increasing the brazing time promotes phase segregation. The highest strength, measured at 106.4 MPa, was achieved for the sample joined at 710 degrees C for 15 mins, with the fracture surface displaying a mixed ductile-brittle mode.
引用
收藏
页数:12
相关论文
共 38 条
[1]   Recent Advances in Brazing Fillers for Joining of Dissimilar Materials [J].
Ahn, Byungmin .
METALS, 2021, 11 (07)
[2]   Interfacial reactions between sapphire and Ag-Cu-Ti-based active braze alloys [J].
Ali, Majed ;
Knowles, Kevin M. ;
Mallinson, Phillip M. ;
Fernie, John A. .
ACTA MATERIALIA, 2016, 103 :859-869
[3]  
[Anonymous], 1992, AWS A5.8
[4]   Investigating the microstructure and mechanical properties in furnace brazing Ti-6Al-4V to 17-4 PH stainless steel dissimilar joint with BNi-2 filler metal [J].
Ardalani, Amirreza ;
Naffakh-Moosavy, Homam .
JOURNAL OF ADVANCED JOINING PROCESSES, 2024, 9
[5]  
Astm D., 2005, Standard Test Method For Apparent Shear Strength of Single-Lap-Joint Adhesively Bonded Metal Specimens by Tension Loading (Metalto-Metal), P1002
[6]  
Atabaki MM, 2012, WELD J, V91, p35S
[7]   Pulsed electrodeposition of nanocrystalline Cu-Ni alloy films and evaluation of their characteristic properties [J].
Baskaran, I. ;
Narayanan, T. S. N. Sankara ;
Stephen, A. .
MATERIALS LETTERS, 2006, 60 (16) :1990-1995
[8]  
Brandes E.A., 1983, SMITHELLS METALS REF
[9]   Effect of Silver Content on Microstructure and Properties of Brass/steel Induction Brazing Joint Using Ag-Cu-Zn-Sn Filler Metal [J].
Cao, J. ;
Zhang, L. X. ;
Wang, H. Q. ;
Wu, L. Z. ;
Feng, J. C. .
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2011, 27 (04) :377-381
[10]   Interfacial reactions in Ag-Sn/Cu couples [J].
Chen, SW ;
Yen, YW .
JOURNAL OF ELECTRONIC MATERIALS, 1999, 28 (11) :1203-1208