Assessing Pore Formation due to Nitrogen Partitioning in a Hypoeutectic Cast Iron

被引:0
作者
Queiros, Ricardo [1 ]
Domeij, Bjorn [1 ]
Dioszegi, Attila [1 ]
机构
[1] Jonkoping Univ, Dept Mat & Mfg, S-55111 Jonkoping, Sweden
关键词
cast iron; component casting; solidification; microsegregation; nitrogen; MN;
D O I
10.1007/s40962-024-01521-3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Pore formation in cast iron castings is driven both by shrinkage and dissolved gases, where the latter stems from supersaturated gaseous species, such as nitrogen. During solidification, nitrogen partitions between the austenite and the liquid according to the ratio of its solubility in each phase. This ratio, known as the partition coefficient, is essential to characterize, as accumulation in the liquid phase can lead to critical supersaturation for pore formation. However, there is conflicting information in CALPHAD databases and literature regarding its partitioning behavior. This work evaluates nitrogen partitioning between the primary austenite and the liquid in a hypoeutectic lamellar cast iron alloy. To investigate this, a cylindrical specimen was produced and remelted under an inert atmosphere, allowing the austenite and the liquid to establish a solute equilibrium. After 6 days of holding at 1175 degrees C within the solid-liquid biphasic range, the specimen was quenched, and samples were extracted from the austenitic and liquid regions, which had transformed into martensite and ledeburite, respectively. The nitrogen concentration was measured by inert gas fusion (IGF), resulting in a nitrogen partition coefficient kN gamma/L\documentclass[12pt]{minimal} \usepackage{amsmath} \usepackage{wasysym} \usepackage{amsfonts} \usepackage{amssymb} \usepackage{amsbsy} \usepackage{mathrsfs} \usepackage{upgreek} \setlength{\oddsidemargin}{-69pt} \begin{document}$${k}_{N}<^>{\gamma /L}$$\end{document} = 0.72 +/- 0.08, which represents partition in the opposite direction suggested by thermodynamic databases. The results indicate that there are opportunities to further explore nitrogen partitioning in other compositions and highlight the importance of selecting databases that more accurately represent the phenomena of interest. Moreover, a better understanding of nitrogen partitioning can enhance the control of porosity in cast iron processing.
引用
收藏
页数:10
相关论文
共 50 条
[41]   Formation of the Cast Iron Coatings Plasma-Sprayed at Different Substrate Temperatures [J].
Xing, Ya-Zhe ;
Jiang, Chao-Ping ;
Chen, Hong ;
Hao, Jian-Min .
FRONTIERS OF MANUFACTURING AND DESIGN SCIENCE, PTS 1-4, 2011, 44-47 :2144-2147
[42]   Surface feature formation mechanism during finish milling of gray cast iron [J].
Kyle Odum ;
Nicholas Raymond ;
Derek Pell ;
Masakazu Soshi .
The International Journal of Advanced Manufacturing Technology, 2017, 92 :459-469
[43]   Effect of bacterial communities on the formation of cast iron corrosion tubercles in reclaimed water [J].
Jin, Juntao ;
Wu, Guangxue ;
Guan, Yuntao .
WATER RESEARCH, 2015, 71 :207-218
[44]   Surface feature formation mechanism during finish milling of gray cast iron [J].
Odum, Kyle ;
Raymond, Nicholas ;
Pell, Derek ;
Soshi, Masakazu .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2017, 92 (1-4) :459-469
[45]   RESEARCH ON PROMOTING THE FORMATION AND CLUSTERS OF TiN PHASE IN HIGH PURITY CAST IRON [J].
Dai, B. ;
Ma, Y. ;
Yu, F. ;
Yuan, M. ;
Chu, J. ;
Xu, Y. .
METALURGIJA, 2023, 62 (01) :53-56
[46]   BIOFILM FORMATION ON CAST-IRON SUBSTRATA IN WATER DISTRIBUTION-SYSTEMS [J].
DONLAN, RM ;
PIPES, WO ;
YOHE, TL .
WATER RESEARCH, 1994, 28 (06) :1497-1503
[47]   Effect of nitrogen on the formation and oxidation behavior of iron aluminide coatings [J].
Zhang, Y ;
Pint, BA ;
Cooley, KM ;
Haynes, JA .
SURFACE & COATINGS TECHNOLOGY, 2005, 200 (5-6) :1231-1235
[48]   Some Factors Affecting on the Structure- formation and Mechanical Properties of As-Cast High Toughness Nodular Cast Iron [J].
Enoukidze Nodar A ;
连金江 ;
钟伟珍 ;
戎豫 .
北京科技大学学报, 1989, (06) :544-550
[49]   Nitrogen inventory of iron meteorite parent bodies constrained by nitrogen partitioning between Fe-rich solid and liquid alloys [J].
Pathak, Debjeet ;
Dasgupta, Rajdeep .
GEOCHIMICA ET COSMOCHIMICA ACTA, 2024, 371 :199-213
[50]   Improving impact toughness of a high chromium cast iron regarding joint additive of nitrogen and titanium [J].
Ding, Hongsheng ;
Liu, Shiqiu ;
Zhang, Hailong ;
Guo, Jingjie .
MATERIALS & DESIGN, 2016, 90 :958-968