Effect of low-temperature degradation treatment on hardness, color, and translucency of single layers of multilayered zirconia

被引:6
作者
Park, Mi-Gyoung [1 ]
机构
[1] Catholic Univ Pusan, Coll Hlth Sci, Dept Dent Lab Sci, Busan, South Korea
关键词
FLEXURAL STRENGTH; MONOLITHIC ZIRCONIA; FRACTURE; SURVIVAL; CERAMICS;
D O I
10.1016/j.prosdent.2023.01.023
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem: Evaluating the effect of low-temperature degradation (LTD) on multilayered zirconia blocks is important for the long-term life of zirconia restorations. Purpose: The purpose of this in vitro study was to analyze the changes in color, translucency, and hardness of a single layer of multilayered zirconia after an LTD treatment. Material and methods: Ninety multilayered 10x10x1.0-mm zirconia specimens (3M Lava Esthetic) were designed using Auto CAD 2006 (Autodesk) and divided into 6 groups (n=15) based on LTD (no treatment, LTD treatment) and the inherent layer type (incisal, transition, and body). The hardness of each specimen was measured using a microVickers hardness tester. The CIELab color coordinates were measured using a spectrophotometer, and the data were used to calculate the color difference and translucency (TP). Data were analyzed using 2-way ANOVA and the Scheff & eacute; test (alpha=.05). Results: LTD treatment did not alter the hardness of multilayered zirconia (P=.572). A significant difference was found in the hardness between the layers of multilayered zirconia (P<.001). LTD treatment did not alter the b & lowast; or L & lowast; values (P=.773, P=.701) but did change the a & lowast; values (P<.001). On LTD treatment, the a & lowast; value was found to decrease. The L & lowast;, a & lowast;, and b & lowast; values differed based on the respective layer within the material (P<.001). As layers progress from the incisal to the body, the L & lowast; value decreased and the a & lowast; and b & lowast; values increased. In all groups, the color difference values were highest in the following order: the incisal and transition layers < the transition and body layers < the incisal and body layers. On LTD treatment, the color difference between the layers decreased. The LTD treatment did not affect the TP value (P=.208), but the TP value for each layer showed a significant difference (P<.001). Conclusions: LTD treatment did not affect the optical properties or hardness of the multilayered zirconia. The hardness of the multilayered zirconia increased from the incisal to the body layer. In multilayered zirconia, the brightness decreased from the incisal to the body layer, and red and yellow color changes were observed. The TP of multilayered zirconia increased from the incisal to the body layer.
引用
收藏
页码:258 / 263
页数:6
相关论文
共 28 条
[1]  
[Anonymous], 2015, ISO 13356:2015
[2]   Translucency of IPS e.max and cubic zirconia monolithic crowns [J].
Baldissara, Paolo ;
Wandscher, Vinicius Felipe ;
Estivalete Marchionatti, Ana Maria ;
Parisi, Candida ;
Monaco, Carlo ;
Ciocca, Leonardo .
JOURNAL OF PROSTHETIC DENTISTRY, 2018, 120 (02) :269-275
[3]   In vitro performance of full-contour zirconia single crowns [J].
Beuer, Florian ;
Stimmelmayr, Michael ;
Gueth, Jan-Frederik ;
Edelhoff, Daniel ;
Naumann, Michael .
DENTAL MATERIALS, 2012, 28 (04) :449-456
[4]  
Beuer F, 2010, QUINTESSENCE INT, V41, P631
[5]   Effect of varying core thicknesses and artificial aging on the color difference of different all-ceramic materials [J].
Dikicier, Sibel ;
Ayyildiz, Simel ;
Ozen, Julide ;
Sipahi, Cumhur .
ACTA ODONTOLOGICA SCANDINAVICA, 2014, 72 (08) :623-629
[6]   Computable translucency as a function of thickness in a multi-layered zirconia [J].
Erdelt, Kurt ;
Pinheiro Dias Engler, Madalena Lucia ;
Beuer, Florian ;
Gueth, Jan-Frederik ;
Liebermann, Anja ;
Schweiger, Josef .
JOURNAL OF PROSTHETIC DENTISTRY, 2019, 121 (04) :683-689
[7]   ACCELERATED AGING CHARACTERISTICS OF THREE YTTRIA-STABILIZED TETRAGONAL ZIRCONIA POLYCRYSTALLINE DENTAL MATERIALS [J].
Flinn, Brian D. ;
deGroot, Dirk A. ;
Mancl, Lloyd A. ;
Raigrodski, Ariel J. .
JOURNAL OF PROSTHETIC DENTISTRY, 2012, 108 (04) :223-230
[8]   Effect of accelerated aging on the fracture toughness of zirconias [J].
Harada, Kosuke ;
Shinya, Akikazu ;
Gomi, Harunori ;
Hatano, Yasuo ;
Shinya, Akiyoshi ;
Raigrodski, Ariel J. .
JOURNAL OF PROSTHETIC DENTISTRY, 2016, 115 (02) :215-223
[9]  
Heintze SD, 2010, INT J PROSTHODONT, V23, P493
[10]   Probing the interfacial strength of novel multi-layer zirconias [J].
Kaizer, Marina R. ;
Kolakarnprasert, Nantawan ;
Rodrigues, Camila ;
Chai, Herzl ;
Zhang, Yu .
DENTAL MATERIALS, 2020, 36 (01) :60-67