Effects of grout sleeve defects on the seismic performance of precast concrete shear walls using grouting for low temperature

被引:0
|
作者
Song, Jie [1 ]
Zhao, Qingyang [1 ,2 ]
Yang, Zongjin [1 ,3 ]
Wang, Mingqian [4 ]
Zhao, Guodong [1 ,2 ]
Duan, Shixin [1 ,2 ]
Xin, Kangyuan [1 ,3 ]
Xu, Qingfeng [4 ]
机构
[1] Shandong Acad Bldg Res Co Ltd, Jinan 250031, Shandong, Peoples R China
[2] Shandong Construct Qual Inspect & Testing Ctr Co L, Jinan 250031, Shandong, Peoples R China
[3] Shandong Jianke Special Construct Engn Technol Ctr, Jinan 250031, Shandong, Peoples R China
[4] Shanghai Res Inst Bldg Sci Co Ltd, Shanghai 200032, Peoples R China
基金
国家重点研发计划;
关键词
Precast concrete shear wall; Seismic performance; Grout sleeve defect; Grouting for low temperature; BEHAVIOR;
D O I
10.1016/j.istruc.2025.108562
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This paper reports the results of an experimental study on effects of grout sleeve defects on the seismic performance of precast concrete shear walls using grouting for low temperature. Six full-scale precast concrete shear wall specimens were prepared and tested subjected to reversed cyclic loading. Test variables included grouting type, grouting curing condition and grouting defects. Test results indicated that concrete crushing failure and tensile fracture failure of the longitudinal rebars were typical failure modes of all specimens. Concrete around the grouting defects was damaged more seriously due to the stress concentration caused by the grouting defects. The lateral load capacity of W2 using grouting for low temperature and suffered from initial low temperature curing was very close to that of W1 with commonly used grouting cured at normal temperature. This indicated that the grouting for low temperature can mitigate the difficulty of grouting at low temperature. Distance between defect and neutral axis was critical for the hysteretic responses of the shear walls. The defects far away from the neutral axis can lead to more damage on the ductility and energy dissipation capacity than that with the defects near the neutral axis. When the grouting defects were subjected to tension, the lateral capacity decreased gradually with the increase of the distance of the defect to neutral axis. The maximum drop of the lateral capacity of W6 with two grouting defects of the longitudinal rebars in the boundary elements was up to 17 %. The debonding of the longitudinal rebars can cause serious damage to the ductility ratio. The maximum drop of the ductility ratio of W3 with grouting defect of the longitudinal rebar in the boundary elements was up to 32 %.
引用
收藏
页数:8
相关论文
共 50 条
  • [1] Study of effects of sleeve grouting defects on the seismic performance of precast concrete shear walls
    Xiao, Shun
    Wang, Zhuolin
    Li, Xiangmin
    Harries, Kent A.
    Xu, Qingfeng
    Gao, Rundong
    ENGINEERING STRUCTURES, 2021, 236
  • [2] Experimental study on seismic performance of precast concrete shear walls with treatment of sleeve grouting defects
    Xiao S.
    Li X.
    Xu Q.
    Jiang H.
    Gao R.
    Wang Z.
    Jianzhu Jiegou Xuebao/Journal of Building Structures, 2022, 43 (04): : 167 - 176
  • [3] Experimental investigation on seismic behaviors of precast concrete shear walls with sleeve grouting defects
    Yang, Jun
    Guo, Tong
    Wang, Wei
    Zhu, Ruizhao
    ADVANCES IN STRUCTURAL ENGINEERING, 2023, 26 (02) : 258 - 271
  • [4] Effects of grout sleeve defects and their repair on the seismic performance of precast concrete frame structures
    Li, Xiangmin
    Xiao, Shun
    Gao, Rundong
    Harries, Kent A.
    Wang, Zhuolin
    Xu, Qingfeng
    Xu, Qingfeng (xuqingfeng73@163.com), 1600, Elsevier Ltd (242):
  • [5] Effects of grout sleeve defects and their repair on the seismic performance of precast concrete frame structures
    Li, Xiangmin
    Xiao, Shun
    Gao, Rundong
    Harries, Kent A.
    Wang, Zhuolin
    Xu, Qingfeng
    ENGINEERING STRUCTURES, 2021, 242
  • [6] EXPERIMENTAL INVESTIGATION ON SEISMIC PERFORMANCE OF FULL-SCALE PRECAST CONCRETE COLUMNS CONNECTED USING SLEEVE WITH GROUTING DEFECTS
    Xie L.-L.
    Zhong B.-J.
    Chen X.
    Miao Q.-S.
    Liu Q.-M.
    Yang C.-T.
    Wang X.-Y.
    Gongcheng Lixue/Engineering Mechanics, 2023, 40 (08): : 68 - 76
  • [7] Experimental study on seismic performance of precast concrete shear walls with defective and repaired grouted sleeve
    Xie, Linlin
    Liu, Qiang
    Wang, Xinyu
    Yang, Cantian
    STRUCTURES, 2023, 57
  • [8] Seismic performance of precast short-leg shear wall using a grouting sleeve connection
    Wu, Min
    Liu, Xiang
    Liu, Hongtao
    Du, Xiuli
    ENGINEERING STRUCTURES, 2020, 208
  • [9] Experimental study on effect of sleeve grouting defects on seismic behavior of precast concrete columns
    Xiao S.
    Li X.
    Xu Q.
    Jiang H.
    Gao R.
    Wang Z.
    Jianzhu Jiegou Xuebao/Journal of Building Structures, 2022, 43 (05): : 112 - 121
  • [10] Experimental study on seismic behavior of precast concrete columns with treatment of sleeve grouting defects
    Li, Xiangmin
    Xiao, Shun
    Xu, Qingfeng
    Wang, Zhuolin
    Gao, Rundong
    Zhang, Fuwen
    Tumu Gongcheng Xuebao/China Civil Engineering Journal, 2021, 54 (05): : 15 - 26