Surface damage in tungsten induced by high heat flux helium irradiation at high temperatures across melting point

被引:0
作者
Wang, Hanqing [1 ,2 ]
Yuan, Yue [1 ,2 ]
Fu, Baoqin [3 ]
Greuner, H. [4 ]
Boeswirth, B. [4 ]
Ren, Mengchong [1 ,2 ]
Nie, Yufei [1 ,2 ]
Zhang, Peng [5 ]
Cao, Xingzhong [5 ]
Lu, Guang-Hong [1 ,2 ]
机构
[1] Beihang Univ, Sch Phys, Beijing 100191, Peoples R China
[2] Beihang Univ, Beijing Key Lab Adv Nucl Mat & Phys, Beijing 100191, Peoples R China
[3] Sichuan Univ, Inst Nucl Sci & Technol, Minist Educ, Key Lab Radiat Phys & Technol, Chengdu 610064, Peoples R China
[4] Max Planck Inst Plasma Phys, Boltzmannstr 2, D-85748 Garching, Germany
[5] Chinese Acad Sci, Inst High Energy Phys, Beijing 100049, Peoples R China
基金
中国国家自然科学基金;
关键词
tungsten; high heat load; pinhole; helium diffusion; melting; PLASMA-FACING MATERIALS; LOW-ENERGY; BUBBLE FORMATION; DIFFUSION; MECHANISMS; RETENTION; EVOLUTION; BEHAVIOR; DEFECTS; METALS;
D O I
10.1088/1741-4326/ad9e02
中图分类号
O35 [流体力学]; O53 [等离子体物理学];
学科分类号
070204 ; 080103 ; 080704 ;
摘要
Understanding the behavior of tungsten (W) surface damage under the synergistic effects of high heat flux (HHF) loading and helium (He) irradiation is essential for predicting material performance during off-normal operations in ITER. In this study, surface modifications occurring at high temperatures (>2200 K) up to the melting point were investigated by conducting experiments involving two campaigns of vertical displacement events like HHF He neutral beam pulse irradiation on polycrystalline W samples at the test facility Garching LArge DIvertor Sample. As the surface temperature of W increased due to irradiation (2253-3683 K), pinholes appeared on the surface, showing a trend of increasing size and decreasing number density, indicating severe lattice damage. Accordingly, we proposed a model for pinhole growth under high-temperature He irradiation based on thermal activation diffusion of He. The calculated activation energy for He diffusion in this process was found to be 0.51 eV, which is considerably higher than the results obtained from previous simulations (0.021-0.157 eV) (Zhou et al 2010 Nucl. Fusion 50 115010; Becquart and Domain 2006 Phys. Rev. Lett. 97 1-4; Shu et al 2013 Nucl. Instrum. Methods Phys. Res. B 303 84-6; Fu et al 2021 J. Nucl. Mater. 543 152599). This suggests that extensive defects in the matrix have a significant impact on the diffusion of He in high-temperature environments, which is distinct from diffusion behavior at lower temperatures. However, as the surface temperature further increased beyond the melting point, the melting and re-solidification process nearly completely repaired almost all defects induced by He ion irradiation. The re-solidified grains were characterized by being intact, damage-free, and having lower residual stress. This study establishes a foundation for the quantitative analysis of helium migration mechanisms under high-temperature helium irradiation, which lays the foundation for understanding material structural damage behavior under off-normal operations for ITER.
引用
收藏
页数:14
相关论文
共 50 条
  • [31] The response of polycrystalline tungsten to 30 keV helium ion implantation at normal incidence and high temperatures
    Zenobia, Samuel J.
    Garrison, Lauren M.
    Kulcinski, Gerald L.
    JOURNAL OF NUCLEAR MATERIALS, 2012, 425 (1-3) : 83 - 92
  • [32] Surface hardening induced by high flux plasma in tungsten revealed by nano-indentation
    Terentyev, D.
    Bakaeva, A.
    Pardoen, T.
    Favache, A.
    Zhurkin, E. E.
    JOURNAL OF NUCLEAR MATERIALS, 2016, 476 : 1 - 4
  • [33] A route to standardised high heat flux testing: An example for tungsten
    Schoofs, Frank
    Gorley, Mike
    FUSION ENGINEERING AND DESIGN, 2019, 139 : 132 - 136
  • [34] Morphological and nanomechanical changes in tungsten in high heat flux conditions
    Seo, Minsuk
    Echols, John R.
    Winfrey, A. Leigh
    NPJ MATERIALS DEGRADATION, 2020, 4 (01)
  • [35] Erosion of a tungsten limiter under high heat flux in TEXTOR
    Sergienko, G.
    Bazylev, B.
    Huber, A.
    Kreter, A.
    Litnovsky, A.
    Rubel, M.
    Philipps, V.
    Pospieswzyk, A.
    Mertens, Ph.
    Samm, U.
    Schweer, B.
    Schmitz, O.
    Tokar, M.
    JOURNAL OF NUCLEAR MATERIALS, 2007, 363 (1-3) : 96 - 100
  • [36] The high-flux effect on deuterium retention in TiC and TaC doped tungsten at high temperatures
    Zibrov, Mikhail
    Bystrov, Kirill
    Mayer, Matej
    Morgan, Thomas W.
    Kurishita, Hiroaki
    JOURNAL OF NUCLEAR MATERIALS, 2017, 494 : 211 - 218
  • [37] Deuterium Retention in a Nanostructured Tungsten Surface Layer Formed during High-Temperature Irradiation with Helium Plasma
    Z. R. Harutyunyan
    O. V. Ogorodnikova
    A. S. Aksenova
    Yu. M. Gasparyan
    V. S. Efimov
    M. M. Kharkov
    A. V. Kaziev
    N. V. Volkov
    Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques, 2020, 14 : 1248 - 1253
  • [38] Deuterium Retention in a Nanostructured Tungsten Surface Layer Formed during High-Temperature Irradiation with Helium Plasma
    Harutyunyan, Z. R.
    Ogorodnikova, O., V
    Aksenova, A. S.
    Gasparyan, Yu M.
    Efimov, V. S.
    Kharkov, M. M.
    Kaziev, A., V
    Volkov, N. V.
    JOURNAL OF SURFACE INVESTIGATION, 2020, 14 (06): : 1248 - 1253
  • [39] Combined effects of crystallography, heat treatment and surface polishing on blistering in tungsten exposed to high-flux deuterium plasma
    Zayachuk, Y.
    Tanyeli, I.
    Van Boxel, S.
    Bystrov, K.
    Morgan, T. W.
    Roberts, S. G.
    NUCLEAR FUSION, 2016, 56 (08)
  • [40] Characterization of in situ damage to tungsten PFCs induced by transient heat flux during plasma disruption in EAST
    Xuan, Chuannan
    Zhu, Dahuan
    Wang, Yang
    Gao, Binfu
    Fu, Wenxue
    Guo, Zongxiao
    Ding, Rui
    Wang, Baoguo
    Zi, Pengfei
    Chen, Junling
    East Team
    NUCLEAR FUSION, 2025, 65 (04)