Spall response and microstructure evolution of additively manufactured AlSi10Mg alloy with different states

被引:4
作者
Shi, Tongya [1 ]
Nan, Xiaolong [2 ]
Ma, Cunqiang [3 ]
Wang, Xiaofeng [1 ]
Hu, Jianbo [2 ]
Wang, Yonggang [1 ]
机构
[1] Ningbo Univ, Key Lab Impact & Safety Engn, Minist Educ, Ningbo 315211, Zhejiang, Peoples R China
[2] CAEP, Inst Fluid Phys, Natl Key Lab Shock Wave & Detonat Phys, Mianyang 621999, Sichuan, Peoples R China
[3] Land Space Technol Corp Ltd, Beijing 100023, Peoples R China
基金
美国国家科学基金会;
关键词
Additive manufacturing; AlSi10Mg alloy; Spall; Microstructure; Texture; DYNAMIC-MECHANICAL BEHAVIOR; STRAIN-RATE; TENSILE PROPERTIES; HEAT-TREATMENT; LASER; PROPERTY; FAILURE; TEXTURE; STRESS;
D O I
10.1016/j.addma.2024.104588
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The spall response and microstructure evolution of additively manufactured AlSi10Mg alloy with different states were investigated systematically through plate impact experiments, microstructure and texture characterization and quasi-static tensile tests. The results show that the microstructure, texture and spall response are related to the impact velocity and material state. Before deformation and fracture failure occur, the as-built and annealed specimens possess the same < 001 > texture along the building direction; the former consists of numerous networks, columnar grains and fine equiaxed grains, and the latter is comprised of coarser grain structure and coarse particles. For both the as-built and annealed specimens, as the impact velocity increases, the Hugoniot elastic limit (HEL) stress and spall strength are slightly affected by the impact velocity; however, the peak shock stress tends to increase. Under the same impact velocity conditions, compared with the as-built specimen, the annealed specimen corresponds to a similar peak shock stress but a lower Hugoniot elastic limit stress and spall strength. Independent of the material state, as the impact velocity increases, the damage gradually increases, namely, from incipient spall to complete spall; the grain structure, including size and shape changes; and the texture remains almost unchanged. Under the same impact velocity conditions, compared with the as-built specimen, the annealed specimen has a coarser grain structure and a similar texture. Voids tend to nucleate at grain boundaries (at the bottom of the melt pool) and large particles. Compared with the as-built specimen, the annealed specimen has greater strain rate sensitivity. The effect of the material state on the tensile strength is dependent on the strain rate, and the annealing treatment may significantly decrease the tensile strength under low strain rate conditions; and weakly decrease it under high strain rate conditions. Finally, the spall strength dependence on the material state and the effect of the strain rate on the spall behavior were discussed.
引用
收藏
页数:20
相关论文
共 70 条
[1]   Effect of morphological changes of eutectic Si particles on the ambient and high temperature tensile properties of Zr containing Al-Si alloys [J].
Abdelaziz, Mohamed H. ;
Samuel, Agnes M. ;
Doty, Herbert W. ;
Samuel, Fawzy H. .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (03) :5962-5981
[2]   Post heat treatment of additive manufactured AlSi10Mg: On silicon morphology, texture and small-scale properties [J].
Alghamdi, F. ;
Song, X. ;
Hadadzadeh, A. ;
Shalchi-Amirkhiz, B. ;
Mohammadi, M. ;
Haghshenas, M. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 783
[3]   Effects of shell scanning and build orientation on dynamic properties of laser powder bed fusion AlSi10Mg alloy [J].
Amir, Ben ;
Lomnitz, Alon ;
Gale, Yuval ;
Friedlander, Lonia ;
Samuha, Shmuel ;
Sadot, Oren .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 883
[4]   On dynamic mechanical behavior of additively manufactured AlSi10Mg_200C [J].
Asgari, Hamed ;
Odeshi, Akindele ;
Hosseinkhani, Keyvan ;
Mohammadi, Mohsen .
MATERIALS LETTERS, 2018, 211 :187-190
[5]   Materials for additive manufacturing [J].
Bourell, David ;
Kruth, Jean Pierre ;
Leu, Ming ;
Levy, Gideon ;
Rosen, David ;
Beese, Allison M. ;
Clare, Adam .
CIRP ANNALS-MANUFACTURING TECHNOLOGY, 2017, 66 (02) :659-681
[6]   Influence of microstructure on the spall failure of aluminum materials [J].
Brewer, Jonathan L. ;
Dalton, D. Allen ;
Jackson, Evan D. ;
Bernstein, Aaron C. ;
Grigsby, Will ;
Taleff, Eric M. ;
Ditmire, Todd .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2007, 38A (11) :2666-2673
[7]   Additive manufacturing of metallic lattice structures: Unconstrained design, accurate fabrication, fascinated performances, and challenges [J].
Chen, Liang-Yu ;
Liang, Shun-Xing ;
Liu, Yujing ;
Zhang, Lai-Chang .
MATERIALS SCIENCE & ENGINEERING R-REPORTS, 2021, 146
[8]   Spall behavior of aluminum with varying microstructures [J].
Chen, X ;
Asay, JR ;
Dwivedi, SK ;
Field, DP .
JOURNAL OF APPLIED PHYSICS, 2006, 99 (02)
[9]   Intragranular void formation in shock-spalled tantalum: Mechanisms and governing factors [J].
Cheng, M. ;
Li, C. ;
Tang, M. X. ;
Lu, L. ;
Li, Z. ;
Luo, S. N. .
ACTA MATERIALIA, 2018, 148 :38-48
[10]   SPALL STUDIES IN URANIUM [J].
COCHRAN, S ;
BANNER, D .
JOURNAL OF APPLIED PHYSICS, 1977, 48 (07) :2729-2737