Influence of CaO/SiO2 on the performance of alkali-activated slag cement

被引:0
作者
Li, Mengmeng [1 ]
He, Juan [1 ,2 ]
Bai, Wenbin [1 ]
Sang, Guochen [3 ]
Chang, Xiulong [4 ]
Song, Xuefeng [1 ]
机构
[1] Xian Univ Architecture & Technol, Coll Mat Sci & Engn, Xian 710055, Peoples R China
[2] XAUAT Engn Technol Co Ltd, Xian 710055, Peoples R China
[3] Xian Univ Technol, Sch Civil Engn & Architecture, Xian 710048, Peoples R China
[4] China Western Construct Acad Bldg Mat Co Ltd, Chengdu 610213, Peoples R China
来源
JOURNAL OF BUILDING ENGINEERING | 2025年 / 103卷
基金
中国国家自然科学基金;
关键词
Alkali-activated slag cement; Molar ratio of CaO/SiO 2; Hydration heat evolution; Mechanical strength; Hydration product; C-S-H; FLY-ASH; AUTOGENOUS SHRINKAGE; MITIGATION STRATEGIES; EARLY HYDRATION; STRENGTH; GEL; FTIR; CARBONATION; RESISTANCE;
D O I
10.1016/j.jobe.2025.111981
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The properties of alkali-activated slag (AAS) cement were mainly affected by granulated blast furnace slag (GBFS) and activators. Due to the difference of raw materials and production technology, the composition of GBFS discharged from different steel plants and periods fluctuated greatly. The ratio of CaO/SiO2 (C/S) showed a great influence on the performance of AAS cement, in addition, even if the mix proportion was the same, there will be some differences in its performance. In the paper, AAS cement with different C/S was prepared by adjusting the constituent, and the effects of C/S on the its properties were studied, including fluidity, setting time, mechanical strength, autogenous shrinkage, pH, hydration heat evolution and hydrated products. The results showed that when C/S increased from 1.3 to 1.7, the performance development was relatively uniform and stable. The fluidity was good, and the setting time fluctuated little. The 28d compressive strength of AAS mortar exceeded 50 MPa.When C/S increased, the [SiO4]4chain length and the degree of polymerization of C-(A)-S-H gel decreased. Therefore, the C/S of AAS cement was recommended between 1.3 and 1.7.
引用
收藏
页数:16
相关论文
共 56 条
  • [1] Redden R., Neithalath N., Microstructure, strength, and moisture stability of alkali activated glass powder-based binders, Cem. Concr. Compos., 45, pp. 46-56, (2014)
  • [2] Bakharev T., Sanjayan J.G., Cheng Y.B., Resistance of alkali-activated slag concrete to acid attack, Cement Concr. Res., 33, 10, pp. 1607-1611, (2003)
  • [3] Jin Y., Feng W., Zheng D., Dong Z., Cui H., Li M., Sang G., Tang W., Study on the interaction mechanism between slags and alkali silicate activators: a hydration kinetics approach, Constr. Build. Mater., 250, (2020)
  • [4] Tanzer R.R., Buchwald A., Stephan D., Effect of slag chemistry on the hydration of alkali-activated blast-furnace slag, Mater. Struct., 48, 3, pp. 629-664, (2014)
  • [5] Jiang F., A study on the composition, structure and propertie of slag-fines cementing materials alkali-activated, Xi ’an, Xi ’an univ. Archit, Technol., 3, (2008)
  • [6] Zhang J., Shi C., Zhang Z., Effect of Na<sub>2</sub>O concentration and water/binder ratio on carbonation of alkali-activated slag/fly ash cements, Constr. Build. Mater., 269, 12, (2020)
  • [7] Nedeljkovic M., Bahmanvan der Laan, SiegerLi, ZhenmingYe, Guang, Effect of curing conditions on the pore solution and carbonation resistance of alkali-activated fly ash and slag pastes, Cement Concr. Res., 116, pp. 146-158, (2019)
  • [8] Navarro A R., Zornoza A E., Sanchez a I., Alcocel B E.G., Influence of the type and concentration of the activator on the microstructure of alkali activated SiMn slag pastes, Constr. Build. Mater., 342, (2022)
  • [9] Kapeluszna E., Kotwica L., Rozycka A., Golek L., Incorporation of Al in C-A-S-H gels with various Ca/Si and Al/Si ratio: microstructural and structural characteristics with DTA/TG, XRD, FTIR and TEM analysis, Constr. Build. Mater., 155, pp. 643-653, (2017)
  • [10] L'Hopital E., Lothenbach B., Kulik D.A., Influence of calcium to silica ratio on aluminium uptake in calcium silicate hydrate, Cement Concr. Res., 85, pp. 111-121, (2016)