共 50 条
Dielectric and electrical properties of Sm2/3Cu3Ti4O12 and Co- V doped Sm2/3Cu3Ti4O12 fabricated by semi wet route
被引:0
作者:
Kumar, Anup
[1
]
Singh, Laxman
[2
]
Verma, Harish
[3
]
Lee, Youngil
[4
]
Singh, N. B.
[5
]
Tiwary, Dhanesh
[1
]
Mandal, Kamdeo
[1
]
机构:
[1] Banaras Hindu Univ, Indian Inst Technol, Dept Chem, Varanasi 221005, Uttar Pradesh, India
[2] Siddharth Univ, Dept Chem, Siddharth Nagar 272202, Uttar Pradesh, India
[3] Banaras Hindu Univ, Indian Inst Technol, Dept Phys, Varanasi 221005, Uttar Pradesh, India
[4] Univ Ulsan, Dept Chem, 93 Deahak Ro, Ulsan 44610, South Korea
[5] Univ Maryland, Dept Chem & Biochem & Comp Sci & Elect Engn, 1000 Hilltop Circle, Baltimore, MD 21250 USA
关键词:
XRD;
XPS;
HR-SEM;
TEM;
EDS;
Dielectric properties;
CACU3TI4O12;
D O I:
10.1016/j.inoche.2025.114211
中图分类号:
O61 [无机化学];
学科分类号:
070301 ;
081704 ;
摘要:
Perovskite oxide has taken the significant consideration of research scholars due to its large dielectric constant and uses in different field of daily life. Sm2/3Cu3Ti4O12 (SCTO) and Sm2/3Cu3Ti3.95Co0.025V0.025O12 (SCTCVO) ceramic materials were synthesized by using cost effective chemical wet route. XRD pattern analysis confirms successful synthesis of SCTO and SCTCVO ceramic. Oxidation states of each element was verified by XPS analysis. EDS spectroscopy proved the presence of each element in both ceramics. Dielectric constant of SCTO ceramic peaked at 1562, measured at 513 K and 1 kHz, whereas SCTCVO peaked at 966, measured at 473 K and 1 kHz. Both ceramics exhibited Maxwell relaxation behavior. However, their lowest recorded values were 307 at 303 K and 1 kHz for SCTO and 282 at 303 K and 1 kHz for SCTCVO. The maximum tangent loss value for SCTO and SCTCVO ceramics were noted as 174 and 128, respectively, at frequencies of 1 kHz and temperatures of 543 K and 563 K.