Flexural strength, surface roughness, and color stability of various CAD-CAM denture teeth materials

被引:0
|
作者
Orgev, Ahmet [1 ]
Cakmak, Gulce [2 ]
Peng, Chin-chun [3 ]
Lavrentiadis, Grigoris [4 ]
Li, Rui [1 ]
机构
[1] SUNY Buffalo, Sch Dent Med, Dept Restorat Dent, 235 Squire Hall,3435 Main St, Buffalo, NY 14214 USA
[2] Univ Bern, Sch Dent Med, Dept Reconstruct Dent & Gerodontol, Bern, Switzerland
[3] Univ Washington, Dept Restorat Dent, Seattle, WA USA
[4] Prosthodont & Implantol Tsimiski 111, Thessaloniki, Greece
来源
JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY | 2024年
关键词
denture teeth; flexural strength; surface roughness; thermocycling; RESTORATIVE MATERIALS; MECHANICAL-PROPERTIES; BASE; CAD/CAM;
D O I
10.1111/jopr.13987
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To assess the flexural strength (FS), surface roughness, and color stability of additive manufactured (AM) and subtractive manufactured (SM) denture teeth materials, as well as the effect of thermocycling on these properties. Materials and Methods: Eighty strips (20/material type; 64x10x3.3 mm) and 60 discs (15/material type; 12x4 mm) were fabricated from four different denture teeth materials (Straumann, Flexcera, Ivoclar, and Candulor). The specimens were divided into two subgroups (nonthermal cycled and 5000 thermal cycled,10 per subgroup), and subjected to a 3-point test for FS using a universal testing machine at a crosshead speed of 5.0 mm/min. Surface roughness (R-a, mu m) and color differences (Delta E-00) of disc specimens were measured before and after thermocycling using a noncontact optical profilometer and a spectrophotometer, respectively. The CIEDE2000 formula was used to calculate the color differences (Delta E-00) before and after thermocycling. Data were analyzed using 2-way ANOVA followed by post hoc multiple comparison tests (alpha = 0.05). Results: There was no significant difference in flexural strength between nonthermal cycled SM materials (p = 0.15), which were significantly higher than AM materials (p < 0.001). The flexural strength values of all tested materials were significantly reduced after thermocycling (p < 0.05). The material type had a significant effect on the R-a values (p < 0.001), whereas thermocycling did not (p = 0.81). After thermocycling, all materials exhibited color changes lower than the clinical perceptible threshold (Delta E-00 = 2.7). Conclusions: Thermocycling decreased the FS of denture teeth materials manufactured with AM and SM, but did not affect the surface roughness. The FS values of SM groups were significantly higher than AM materials, irrespective of thermocycling. No clinically significant color changes of the denture teeth material were noted.
引用
收藏
页数:7
相关论文
共 50 条
  • [41] Effect of aging on color, gloss and surface roughness of CAD/CAM composite materials
    Papathanasiou, Ioannis
    Zinelis, Spiros
    Papavasiliou, George
    Kamposiora, Phophi
    JOURNAL OF DENTISTRY, 2023, 130
  • [42] Influence of Simulated Gastric Juice on Surface Roughness, Morphology and Micro Hardness of CAD-CAM Materials (An In Vitro Study)
    Abdulameer, Ghadeer S.
    Hameed, Mohammed R.
    JOURNAL OF RESEARCH IN MEDICAL AND DENTAL SCIENCE, 2022, 10 (08): : 58 - +
  • [43] Evaluation of the Effect of Different Construction Techniques of CAD-CAM Milled, 3D-Printed, and Polyamide Denture Base Resins on Flexural Strength: An In Vitro Comparative Study
    Zeidan, Ahmed Abd El-Latif
    Sherif, Ahmed Fadlallah
    Baraka, Yasser
    Abualsaud, Reem
    Abdelrahim, Ramy Abdallah
    Gad, Mohammed M.
    Helal, Mohamed A.
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2023, 32 (01): : 77 - 82
  • [44] Effect of denture cleansers on color stability and surface roughness of denture bases fabricated from three different techniques: Conventional heat-polymerizing, CAD/CAM additive, and CAD/CAM subtractive manufacturing
    Takhtdar, Mehrab
    Azizimoghadam, Nahid
    Kalantari, Mohammad Hasan
    Mohaghegh, Mina
    CLINICAL AND EXPERIMENTAL DENTAL RESEARCH, 2023, 9 (05): : 840 - 850
  • [45] Tensile bond strength of auto-polymerizing and heat-polymerizing denture reliners on the conventional and CAD-CAM denture base materials
    Alfaraj, Amal
    Chu, Tien-Min G.
    Alouthah, Hesham
    Yang, Chao-Chieh
    Lin, Wei-Shao
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2023, 32 : 87 - 95
  • [46] Bond strength of CAD/CAM denture teeth to a denture base resin in a milled monolithic unit
    Mohamed, Amr
    Takaichi, Atsushi
    Kajima, Yuka
    Takahashi, Hidekazu
    Wakabayashi, Noriyuki
    JOURNAL OF PROSTHODONTIC RESEARCH, 2023, 67 (04) : 610 - 618
  • [47] Effect of surface finishing treatments on the color stability of CAD/CAM materials
    Ozen, Funda
    Demirkol, Nermin
    Oz, Ozge Parlar
    JOURNAL OF ADVANCED PROSTHODONTICS, 2020, 12 (03) : 150 - 156
  • [48] Effects of polishing press-on force on surface roughness and gloss of CAD-CAM composites
    Yu, Peng
    Luo, Hao
    Yap, Adrian U.
    Tian, Fu-Cong
    Wang, Xiao-Yan
    JOURNAL OF ORAL SCIENCE, 2023, 65 (02) : 131 - 135
  • [49] Effect of toothbrushing on surface roughness and gloss of CAD-CAM versus conventional interim materials with different surface treatments
    Sattawatthamrong, Sarasinee
    Kamonkhantikul, Krid
    Homsiang, Woraporn
    Arksornnukit, Mansuang
    JOURNAL OF PROSTHETIC DENTISTRY, 2025, 133 (01) : 282e1 - 282e12
  • [50] Effectiveness of Porcelain Polishing Methods on the Roughness and Color Stability of CAD-CAM Ceramics after Orthodontic Bracket Debonding
    Haralur, Satheesh B.
    Shiban, Abdullah Saeed
    Alqahtani, Nasser Mohammed
    MATERIALS, 2023, 16 (14)