Repair Bond Strength of Composite Resin to Dental Ceramic Using Various Surface Treatments: An In Vitro Study

被引:0
|
作者
Al-Askary, Raghad A. [1 ]
Al-Ashou, Wiaam M. O. [1 ]
Hassoon, Saif Nadhim [1 ]
机构
[1] Univ Mosul, Coll Dent, Dept Conservat Dent, Mosul 41002, Iraq
来源
JOURNAL OF INTERNATIONAL SOCIETY OF PREVENTIVE AND COMMUNITY DENTISTRY | 2024年 / 14卷 / 05期
关键词
Cracked ceramic; IPS E-Max CAD; repairing system; surface treatment; universal adhesive; ZIRCONIA; ADHESIVE; CEMENT;
D O I
10.4103/jispcd.jispcd_71_24
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Aim: This research aims to evaluate and compare the effect of various surface treatments and adhesive types on the bond strength between composite resin and two types of ceramic materials. Materials and Methods: A total of 98 disk-shaped of 10 mm diameter and 4 mm thickness were fabricated for each of the zirconia (H. C. Starck) and lithium disilicate (IPS E-Max computer-aided design), which were implanted individually in the acrylic resin mold leaving one surface exposed. The disks in each group were sub-divided according to the surface treatments into seven groups (n = 14): [hydrofluoric acid (HF, 9.5%), air abrasion, bur, laser, HF + bur, HF + air abrasion, HF + laser]. Each sub-group was further divided into two groups (n = 7) according to the type of adhesive used for the repairing procedure [G-Premio Bond universal adhesive group and intraoral repair kit (BISCO) group]. Each adhesive was applied depending on manufacturer instructions and, then, the composite cylinder (4 mm in diameter and 4 mm in height) was built on the pre-determined treated ceramic surface area by the addition of rubber mold. Then the samples were stored in distal water for 24 h. After that, all groups were submitted to a shear bond test using an Instron testing machine (TSTM 02500; Elista Ltd., Istanbul, Turkey) at 0.5 mm/min a crosshead speed. The data were analyzed by three-way analysis of variance and Tukey post hoc test at (P <= 0.05). Results: The HF + air abrasion groups registered the higher bond strength but with no statistically significant difference from groups of HF + bur. While the laser groups showed the lowest mean bond strength. Generally, E-Max registered significantly higher bond strength in comparison to zirconia. Finally, the BISCO repair system registered a significantly higher bond strength value in comparison to G-Premio. Conclusion: Combined surface treatment of HF + air abrasion with an intraoral repair kit can provide a promising method for repairing cracked ceramic restorations. However, repairing lithium disilicate is more predictable and successful than zirconia.
引用
收藏
页码:388 / 395
页数:8
相关论文
共 50 条
  • [21] Bond Strength of Resin Composite of Bioactive Restorative Materials Using Different Surface Treatments
    Alsahhaf, Abdulaziz
    BIOSCIENCE BIOTECHNOLOGY RESEARCH COMMUNICATIONS, 2020, 13 (01): : 95 - 100
  • [22] Repair Bond Strength of a Resin Composite to Plasma-Treated or UV-Irradiated CAD/CAM Ceramic Surface
    Kameyama, Atsushi
    Haruyama, Akiko
    Tanaka, Akihiro
    Noro, Akio
    Takahashi, Toshiyuki
    Yoshinari, Masao
    Furusawa, Masahiro
    Yamashita, Shuichiro
    COATINGS, 2018, 8 (07):
  • [23] Shear Bond Strength of Aged CAD/CAM Ceramic Materials Repaired by Resin Composite In vitro Using Different Repair Adhesives
    Falah, Rand Mohammed
    Ameer, Zainab M. Abdul
    JOURNAL OF RESEARCH IN MEDICAL AND DENTAL SCIENCE, 2020, 8 (01): : 61 - 67
  • [24] Effect of ceramic surface treatments on the bond strength of different composite resins
    Yanikoglu, Nuran
    Duymus, Zeynep Yesil
    Alkurt, Murat
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2018, 32 (03) : 247 - 257
  • [25] Effect of surface treatments on the bond strength of indirect resin composite to resin matrix ceramics
    Celik, Ersan
    Sahin, Sezgi Cinel
    Dede, Dogu Omur
    JOURNAL OF ADVANCED PROSTHODONTICS, 2019, 11 (04): : 223 - 231
  • [26] Tensile bond strength of resin composite repair in vitro using different surface preparation conditionings to an aged CAD/CAM resin nanoceramic
    Stawarczyk, Bogna
    Krawczuk, Andreas
    Ilie, Nicoleta
    CLINICAL ORAL INVESTIGATIONS, 2015, 19 (02) : 299 - 308
  • [27] Repair Bond Strength of Two Shadeless Resin Composites Bonded to Various CAD-CAM Substrates with Different Surface Treatments
    AlOtaibi, AlFulwah A.
    Taher, Nadia M.
    COATINGS, 2023, 13 (07)
  • [28] Comparison of the Bond Strength of Composite Resin to Zirconia and Composite Resin to Polyether Ether Ketone: An In Vitro Study
    Sarfaraz, Hasan
    Rasheed, Mohammed N.
    Shetty, Sanath K.
    Prabhu, Uma M.
    Fernandes, Kevin
    Mohandas, Smrithi
    JOURNAL OF PHARMACY AND BIOALLIED SCIENCES, 2020, 12 : 504 - 509
  • [29] In Vitro Evaluation of the Effect of Different Surface Treatments of a Hybrid Ceramic on the Microtensile Bond Strength to a Luting Resin Cement
    Motevasselian, Fariba
    Amiri, Zahra
    Chiniforush, Nasim
    Mirzaei, Mansoreh
    Thompson, Van
    JOURNAL OF LASERS IN MEDICAL SCIENCES, 2019, 10 (04) : 297 - 303
  • [30] Effect of different surface treatments on the repair bond strength of resin composites with titanium
    Korkmaz, Fatih Mehmet
    Ates, Sabit Melih
    Caglar, Ipek Satiroglu
    Baygin, Ozgul
    Duymus, Zeynep Yesil
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2019, 33 (21) : 2385 - 2403