Thermal conductivity of chemical vapor deposition diamond enriched with 13C isotope

被引:0
|
作者
Inyushkin, A. V. [1 ]
Ralchenko, V. G. [2 ,3 ]
Bolshakov, A. P. [2 ]
Khomich, A. A. [4 ]
Chernodubov, D. A. [1 ]
Taldenkov, A. N. [1 ]
Saraykin, V. V. [1 ]
Kilin, S. Ya. [5 ]
机构
[1] Natl Res Ctr Kurchatov Inst, Moscow 123182, Russia
[2] Russian Acad Sci, Prokhorov Inst Gen Phys, Moscow 119991, Russia
[3] Harbin Inst Technol, Harbin 150080, Peoples R China
[4] Russian Acad Sci, Kotelnikov Inst Radio Engn & Elect, Fryazino 141120, Russia
[5] Natl Res Nucl Univ MEPhI, Moscow 115409, Russia
关键词
RAMAN-SCATTERING; PHONON-SCATTERING; LATTICE-DYNAMICS; HIGH-RESOLUTION; CRYSTALS; TRANSPORT; NITROGEN; SPECTRA; MODEL;
D O I
10.1063/5.0255049
中图分类号
O59 [应用物理学];
学科分类号
摘要
Thermal conductivity kappa(T) of single-crystal CVD diamond enriched with C-13 isotope to 98.16% was measured by the method of steady-state longitudinal heat flow in the temperature range from 6 to 410 K. This crystal with low nitrogen impurity content ( <50 ppb) showed thermal conductivity 2010 +/- 50 W m(-1) K-1 at 300 K (with a maximum of 12 100 W m(-1) K-1 at 83 K), which is significantly lower than that of diamond with natural isotopic composition: kappa(300K) = 2360 +/- 50 W m(-1) K-1. The measured data were analyzed using first-principles theory and the Callaway model, taking into account phonon scattering in three-phonon processes, scattering at sample boundaries and at isotopes. The first-principles calculations overestimate the thermal conductivity compared to the measured one near and to the right of the kappa(T) peak, indicating the presence of significant additional phonon scattering by lattice defects in the studied chemically pure diamond samples. The results of both theoretical approaches for thermal conductivity at 300 K are in good agreement with our measured data and other published experimental data for isotopically modified diamonds. First-principles calculations yield a thermal conductivity ratio of kappa(12)(T)/kappa(13)(T)=1.072 for monoisotopic defect-free C-12 and C-13 crystals at 300 K. This ratio decreases at high temperatures to a value of 1.041 according to the Leibfried-Schlomann theory and to a value of 0.921 at very low temperatures. (c) 2025 Author(s). All article content, except where otherwise noted, is licensed under a Creative Commons Attribution-NonCommercial 4.0International (CC BY-NC) license (https://creativecommons.org/licenses/by-nc/4.0/).
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Isotope Effect in Thermal Conductivity of Polycrystalline CVD-Diamond: Experiment and Theory
    Inyushkin, Alexander, V
    Taldenkov, Alexander N.
    Ralchenko, Victor G.
    Bolshakov, Andrey P.
    Khomich, Alexander, V
    CRYSTALS, 2021, 11 (04):
  • [22] The use of 13C diamond as pressure and temperature sensor for diamond-anvil-cell experiments
    Munsch, Pascal
    Bureau, Helene
    El Yakoubi, Marouan
    Khodja, Hicham
    Zaitsev, Alexander
    EUROPEAN JOURNAL OF MINERALOGY, 2015, 27 (03) : 365 - 375
  • [23] Carbon Isotope Ratios in Planetary Nebulae: The Unexpected Enhancement of 13C
    Ziurys, L. M.
    Schmidt, D. R.
    Woolf, N. J.
    ASTROPHYSICAL JOURNAL LETTERS, 2020, 900 (02)
  • [24] SiV Color Centers in Si-Doped Isotopically Enriched 12C and 13C CVD Diamonds
    Sedov, Vadim
    Boldyrev, Kirill
    Krivobok, Vladimir
    Nikolaev, Sergei
    Bolshakov, Andrey
    Khomich, Alex
    Khomich, Andrew
    Krasilnikov, Anatoly
    Ralchenko, Victor
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2017, 214 (11):
  • [25] A Study of the Structural and Vibrational Properties of Diamond Nanoparticles Grown by Chemical Vapor Deposition
    Chakraborty, Rajarshi
    Sharma, Suresh C.
    LaRoque, J. Kyle
    JOURNAL OF NANO RESEARCH, 2010, 12 : 123 - 130
  • [26] Synthesis of Nitrogen-Doped Graphene on Copper Nanowires for Efficient Thermal Conductivity and Stability by Using Conventional Thermal Chemical Vapor Deposition
    Park, Minjeong
    Ahn, Seul-Ki
    Hwang, Sookhyun
    Park, Seongjun
    Kim, Seonpil
    Jeon, Minhyon
    NANOMATERIALS, 2019, 9 (07):
  • [27] Enhancement of crystalline quality of homoepitaxial (100) diamond by microwave plasma chemical vapor deposition with a tungsten wire
    Yang, Tzu-, I
    Chuang, Chia-Yen
    Chang, Li
    DIAMOND AND RELATED MATERIALS, 2025, 154
  • [28] Doping of vanadium to nanocrystalline diamond films by hot filament chemical vapor deposition
    Zhang, Yaozhong
    Zhang, Liying
    Zhao, Jiang
    Wang, Liang
    Zhao, Gang
    Zhang, Yafei
    NANOSCALE RESEARCH LETTERS, 2012, 7
  • [29] Two- and three-photon absorption in chemical vapor deposition diamond
    Kozak, Martin
    Trojanek, Frantisek
    Dzurnak, Branislav
    Maly, Petr
    JOURNAL OF THE OPTICAL SOCIETY OF AMERICA B-OPTICAL PHYSICS, 2012, 29 (05) : 1141 - 1145
  • [30] Diamond-graphite nanorods produced by microwave plasma chemical vapor deposition
    Rakha, Sobia Allah
    Yu, Guojun
    Cao, Jianqing
    He, Suixia
    Zhou, Xingtai
    DIAMOND AND RELATED MATERIALS, 2010, 19 (04) : 284 - 287