How do water and acid in marine archaeological wood affect its mechanical properties?

被引:2
作者
Gao, Xunming [1 ]
Zhao, Jian [1 ,2 ,3 ]
Liu, Jiahui [1 ,2 ]
Fei, Lihua [4 ]
Zhao, Dong [1 ,2 ]
机构
[1] Beijing Forestry Univ, Sch Technol, Beijing 100083, Peoples R China
[2] Beijing Forestry Univ, Key Lab State Forestry Adm Forestry Equipment & Au, Beijing 100083, Peoples R China
[3] State Key Lab Efficient Prod Forest Resources, Beijing 100083, Peoples R China
[4] Quanzhou Maritime Museum Fujian, Quanzhou 362000, Peoples R China
关键词
Marine archaeological wooden artifacts; Acid environment; Molecular mechanisms; Optimal moisture content; Molecular dynamics simulation; MOLECULAR-DYNAMICS; DEFORMATION; CRYSTALLINE; CONSERVATION;
D O I
10.1016/j.culher.2024.10.017
中图分类号
K85 [文物考古];
学科分类号
0601 ;
摘要
The prolonged burial of marine archaeological wood in seawater mudflats results in the internal saturation of the wood with water, acidification, and salt deposition. Despite the application of desalination, deacidification, and drainage treatments to archaeological wood following excavation, the effects of such environments on wood are irreversible. To understand the effects of moisture content, acidic environments, and insoluble salts (Fe2 S) on the mechanical properties of marine archaeological wood, this study employed molecular dynamics simulations to analyze the tensile performance of wood cell walls under various conditions. The results indicate that, compared to completely dry wood, water molecules can significantly enhance the tensile strength of wood cell walls. However, in systems with a 12 % moisture content, the tensile strength is lower than in systems with a 4 % moisture content. The worst tensile performance of wood cell walls occurs in acidic and salt-deposition conditions. This is mainly due to the fact that an appropriate amount of moisture enhances the interconnections between wood fibers, whereas acidic and salt deposition conditions disrupt these connections. Additionally, the impact of varying quantities of moisture molecules on the mechanical properties of wood also varies. Further exploring the optimal moisture content for the preservation of waterlogged wooden artifacts, using archaeological fir wood as an example, we constructed models of amorphous wood fibers and matrices with moisture content varying from 0 % to 36 %. The results indicate that the system with 8 % moisture content exhibits optimal mechanical performance. Specifically, the shear modulus and chain-direction elastic modulus reach 4.52 GPa and 12.93 GPa, respectively, representing an increase of 25.2 % and 45.1 % compared to completely dry systems. The molecular mechanism by which moisture content influence the mechanical properties of wood was analyzed through parameters such as mean square displacement, diffusion coefficient, and free volume. It is hypothesised that an appropriate amount of water molecules can fill the gaps between fibers, enhancing the inter-fiber bonding and stiffness, and thereby improving the mechanical properties of wood. However, as water molecules continue to be added, this positive effect diminishes. The objective of our study is to gain insight into the mechanical behavior of archaeological wood cell walls from a molecular perspective. This paves the way for multiscale studies to determine the optimal moisture content for preserving wooden artifacts and to identify environmental conditions that can maximize the mechanical performance of archaeological wooden objects. (c) 2024 Elsevier Masson SAS. All rights are reserved, including those for text and data mining, AI training, and similar technologies.
引用
收藏
页码:431 / 440
页数:10
相关论文
共 35 条
[1]   Mesoscale mechanics of wood cell walls under axial strain [J].
Adler, David C. ;
Buehler, Markus J. .
SOFT MATTER, 2013, 9 (29) :7138-7144
[2]   LIGNIN CHEMISTRY - PAST, PRESENT AND FUTURE [J].
ADLER, E .
WOOD SCIENCE AND TECHNOLOGY, 1977, 11 (03) :169-218
[3]   MOLECULAR-DYNAMICS WITH COUPLING TO AN EXTERNAL BATH [J].
BERENDSEN, HJC ;
POSTMA, JPM ;
VANGUNSTEREN, WF ;
DINOLA, A ;
HAAK, JR .
JOURNAL OF CHEMICAL PHYSICS, 1984, 81 (08) :3684-3690
[4]   The structure of galactoglucomannan impacts the degradation under alkaline conditions [J].
Berglund, Jennie ;
Azhar, Shoaib ;
Lawoko, Martin ;
Lindstroem, Mikael ;
Vilaplana, Francisco ;
Wohlert, Jakob ;
Henriksson, Gunnar .
CELLULOSE, 2019, 26 (03) :2155-2175
[5]   Changes in Moisture Characteristics of Waterlogged Archaeological Wood Owing to Microbial Degradation [J].
Cao, Huimin ;
Gao, Xin ;
Chen, Jiabao ;
Xi, Guanglan ;
Yin, Yafang ;
Guo, Juan .
FORESTS, 2023, 14 (01)
[6]   Facile Tailoring of Structures for Controlled Release of Paracetamol from Sustainable Lignin Derived Platforms [J].
Culebras, Mario ;
Pishnamazi, Mahboubeh ;
Walker, Gavin M. ;
Collins, Maurice N. .
MOLECULES, 2021, 26 (06)
[7]  
Dan L., 2020, 2020 IEEE INT C HIGH
[8]   New attempts with the keratin-metal/magnesium process for the conservation of archaeological waterlogged wood [J].
Endo, Rie ;
Sugiyama, Junji .
JOURNAL OF CULTURAL HERITAGE, 2022, 54 :53-58
[9]   Cellulose: A Review of Water Interactions, Applications in Composites, and Water Treatment [J].
Etale, Anita ;
Onyianta, Amaka J. ;
Turner, Simon R. ;
Eichhorn, Stephen J. .
CHEMICAL REVIEWS, 2023, 123 (05) :2016-2048
[10]   Static and dynamic behavior of CO2 enhanced oil recovery in nanoslits: Effects of mineral type and oil components [J].
Fang, Timing ;
Zhang, Yingnan ;
Ding, Bin ;
Yan, Youguo ;
Zhang, Jun .