Resistance to embrittlement in ferritic/martensitic steel with TaWVCr coating in oxygen-saturated lead-bismuth eutectic at 350 °C

被引:1
|
作者
Li, Shijiang [1 ]
Tong, Zhenfeng [1 ]
Cheng, Shuo [1 ]
Shen, Zhao [2 ]
Sun, Lu [1 ]
Gong, Aoxiang [1 ]
Long, Bin [3 ]
Qin, Bo [3 ]
Wang, Yaqiang [4 ]
Lu, Shenghui [3 ]
Sun, Jun [4 ]
机构
[1] North China Elect Power Univ, Sch Nucl Sci & Engn, Beijing 102206, Peoples R China
[2] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, Shanghai 200240, Peoples R China
[3] China Inst Atom Energy, Beijing 102413, Peoples R China
[4] Xi An Jiao Tong Univ, State Key Lab Mech Behav Mat, Xian 710049, Peoples R China
基金
中国国家自然科学基金;
关键词
Ferritic/martensitic steel; Complex concentrated alloy coating; Lead bismuth eutectic; Liquid metal embrittlement; Oxide cracks; FERRITIC-MARTENSITIC STEEL; LIQUID-METAL EMBRITTLEMENT; CORROSION BEHAVIOR; CRACK-PROPAGATION; T91; STEEL; MECHANICAL-PROPERTIES; TENSILE PROPERTIES; PB-BI; CONTACT; LBE;
D O I
10.1016/j.surfcoat.2025.131729
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Ferritic/martensitic (F/M) steels are potentially applied as structural materials in the lead cooled fast reactor, a promising fourth-generation reactor that adopts lead bismuth eutectic (LBE) as coolant. However, the F/M steels normally suffer from a LBE sensitivity, showing a liquid metal embrittlement when exposed to the LBE. Here in present work, TaWVCr complex concentrated alloy coating was deposited by using magnetron sputtering to protect the F/M steels from liquid metal embrittlement. For this purpose, 12Cr F/M steel coated and uncoated TaWVCr were tested in a static oxygen-saturated LBE at 350 degrees C by corrosion testing and slow strain rate tension testing, respectively, for comparison. The TaWVCr-coated 12Cr F/M steel exhibited a tensile elongation of similar to 19.6 %, over three times of the uncoated 12Cr F/M steel one (< 5.1 %). It was demonstrated that the TaWVCr coating, even in thickness of about 5 mu m, is effective in securing the F/M steel against embrittling. Comprehensive microstructural characterizations were conducted, to reveal the mechanisms responsible for embrittlement resistance. It was revealed that the embrittlement of 12Cr F/M steel is primarily associated with cracking of the surface oxide scale, which propagates into the matrix and hence provides a channel for LBE to wet the matrix. On the contrary, the TaWVCr coating substantially preserves the 12Cr F/M steel from being punctured by oxidation cracks and concomitantly reduces the sensitivity to liquid metal embrittlement. As a result, the fracture pattern changes from a brittle fracture to ductile fracture with the introduction of TaWVCr coating.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] General corrosion behavior and mechanism of ferritic/martensitic steel with and without TaWVCr coating in static oxygen-saturated lead bismuth eutectic at 550 °C
    Li, Shijiang
    Sun, Lu
    Cheng, Shuo
    Gong, Aoxiang
    Yang, Wenping
    Tong, Zhenfeng
    SURFACE & COATINGS TECHNOLOGY, 2024, 488
  • [2] Correlation between impact angle and corrosion-erosion damage behavior of ferritic/martensitic steel exposed to flowing oxygen-saturated lead-bismuth eutectic
    Sun, Qi
    Zheng, Xuechao
    Qin, Yu
    He, Jifan
    Liang, Yanxiang
    Zhu, Minhao
    JOURNAL OF NUCLEAR MATERIALS, 2023, 587
  • [3] Liquid lead-bismuth eutectic embrittlement effect on the tensile properties of T91 steel at 350°C
    Liu, Jing
    Xiao, Zunqi
    Jiang, Zhizhong
    Luo, Lin
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2022, 73 (02): : 207 - 216
  • [4] Effect of pre-deformation on the oxidation resistance of a high Si ferritici/martensitic steel in oxygen-saturated stagnant lead-bismuth eutectic at 550 °C
    Dong, Hong
    Wang, Pei
    Li, Dianzhong
    Li, Yiyi
    CORROSION SCIENCE, 2017, 118 : 129 - 142
  • [5] Initiation of LME crack in ferritic martensitic steel in liquid lead-bismuth
    Hojna, Anna
    Di Gabriele, Fosca
    Chocholousek, Michal
    Spirit, Zbynek
    Halodova, Patricie
    Lorincik, Jan
    JOURNAL OF NUCLEAR MATERIALS, 2018, 511 : 459 - 472
  • [6] Liquid metal embrittlement of an Fe10Cr4Al ferritic alloy exposed to oxygen-depleted and -saturated lead-bismuth eutectic at 350°C
    Gong, Xing
    Chen, Jiajun
    Hu, Feiyu
    Xiang, Congying
    Yu, Zhiyang
    Xiao, Jun
    Wang, Hui
    Gong, Haoran
    Wang, Hao
    Liu, Chaohong
    Deng, Yangbin
    Pang, Bo
    Huang, Xi
    Li, Yongchun
    Yin, Yuan
    CORROSION SCIENCE, 2020, 165
  • [7] Corrosion behavior of Al-O coating in oxygen-saturated lead-bismuth eutectic at 550 ° C
    Zhang, Tianhao
    Ma, Jiaojiao
    Liu, Weizheng
    Meng, Chuiyi
    Qi, Wei
    Wang, Hui
    He, Xiujie
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 30 : 4123 - 4136
  • [8] Embrittlement effects on ferritic/martensitic steels by liquid lead-bismuth eutectic
    高雯
    LONG Bin
    DAI Yong
    Journal of Chongqing University(English Edition), 2013, 12 (04) : 163 - 169
  • [9] New insights into oxidation mechanism and kinetics of 9Cr-1Mo ferritic-martensitic steel in oxygen-saturated liquid lead-bismuth eutectic
    Zhou, Zhikun
    Tian, Chenwen
    Du, Juan
    Peng, Xuhao
    Liu, Yunpeng
    Yu, Xiaofei
    Mi, Xue
    Pu, Zhuo
    Xie, Hai
    Wahab, Magd Abdel
    Chen, Ziguang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 997
  • [10] Liquid metal embrittlement of 12Cr ferritic/martensitic steel thin-walled tubes exposed to liquid lead-bismuth eutectic
    Wang, Hao
    Gong, Xing
    Xiao, Jun
    Chai, Linjiang
    Yu, Zhiyang
    Chen, Haitao
    Zhao, Ke
    Zhou, Jun
    Liu, Guiliang
    Chen, Yong
    Qiu, Shaoyu
    CORROSION SCIENCE, 2022, 195