Deciphering the Impacts of Al, Fe, Li Sulfate Impurities on the Synthesis and Performances of LiNi0.6Mn0.2Co0.2O2 Cathode Materials

被引:0
作者
Chable, Johann [1 ]
Bohn, Nicole [1 ]
Raab, Monika [1 ]
Al-Tobul, Shadi [1 ]
Bergfeldt, Thomas [1 ]
Mueller, Marcus [1 ]
Binder, Joachim R. [1 ]
机构
[1] Karlsruhe Inst Technol, Inst Appl Mat, Energy Storage Syst, Hermann Von Helmholtz Pl 1, D-76344 Eggenstein Leopoldshafen, Germany
关键词
ELECTROCHEMICAL PERFORMANCE; LITHIUM; HYDROXIDE; LINI0.8CO0.15AL0.05O2; COPRECIPITATION; BATTERIES; NICKEL; X=0;
D O I
10.1149/1945-7111/adb64e
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The recycling of LiNi0.6Mn0.2Co0.2O2 cathode active material (CAM) from Li-ion batteries cannot avoid the presence of impurities in the recycled Ni-, Co-, or Mn sulfates. The precise understanding of the impurities influence on the resynthesis is of uttermost importance. To tackle this goal, this study simulated the resynthesis process by adding on purpose and separately Al-, Fe-, and Li-sulfate in the regular CAM synthesis. Their effects on the morphology, elemental composition, crystal structure, and electrochemical performances of Ni0.6Mn0.2Co0.2Mx(OH)2 and LiNi0.6Mn0.2Co0.2MxO2 were systematically investigated for x = 0.0005, 0.005, and 0.05. The in-house reference material synthesized via a coprecipitation reaction allowed to produce a well-characterized basis. Above xAl = 0.0005, the hydroxide secondary particles lost their spherical form and above xFe = 0.005, the crystal structure was affected. Both effects led to cell capacity decay, contrary to the discrete influence of Li. The absence of any positive effects reported by similar studies, the complexity of the various influences of these foreign ions and the limitations of the coin cells tests were pointed out. These results are a solid groundwork for future academic and industrial studies in the field of circular economy, by determining a tolerance threshold for each impurity. Impurities leftovers in resynthesis of Li-ion cathode materialsPrecise purity requirements in industrially recycled battery materialsAluminium is very detrimental for the morphologyIron disturbs the crystal structureLithium induces subtle changes
引用
收藏
页数:13
相关论文
共 64 条
[1]   A Roadmap for Transforming Research to Invent the Batteries of the Future Designed within the European Large Scale Research Initiative BATTERY 2030+ [J].
Amici, Julia ;
Asinari, Pietro ;
Ayerbe, Elixabete ;
Barboux, Philippe ;
Bayle-Guillemaud, Pascale ;
Behm, R. Juergen ;
Berecibar, Maitane ;
Berg, Erik ;
Bhowmik, Arghya ;
Bodoardo, Silvia ;
Castelli, Ivano E. ;
Cekic-Laskovic, Isidora ;
Christensen, Rune ;
Clark, Simon ;
Diehm, Ralf ;
Dominko, Robert ;
Fichtner, Maximilian ;
Franco, Alejandro A. ;
Grimaud, Alexis ;
Guillet, Nicolas ;
Hahlin, Maria ;
Hartmann, Sarah ;
Heiries, Vincent ;
Hermansson, Kersti ;
Heuer, Andreas ;
Jana, Saibal ;
Jabbour, Lara ;
Kallo, Josef ;
Latz, Arnulf ;
Lorrmann, Henning ;
Lovvik, Ole Martin ;
Lyonnard, Sandrine ;
Meeus, Marcel ;
Paillard, Elie ;
Perraud, Simon ;
Placke, Tobias ;
Punckt, Christian ;
Raccurt, Olivier ;
Ruhland, Janna ;
Sheridan, Edel ;
Stein, Helge ;
Tarascon, Jean-Marie ;
Trapp, Victor ;
Vegge, Tejs ;
Weil, Marcel ;
Wenzel, Wolfgang ;
Winter, Martin ;
Wolf, Andreas ;
Edstrom, Kristina .
ADVANCED ENERGY MATERIALS, 2022, 12 (17)
[2]   A review of contemporary and emerging recycling methods for lithium-ion batteries with a focus on NMC cathodes [J].
Azimi, Gisele ;
Chan, Ka Ho .
RESOURCES CONSERVATION AND RECYCLING, 2024, 209
[3]   Understanding the effect of nonmetallic impurities in regenerated cathode materials for lithium-ion battery recycling by tracking down impurity elements [J].
Beak, Mincheol ;
Park, Jangho ;
Park, Sanghyuk ;
Jeong, Seongdeock ;
Kang, Jingu ;
Choi, Woosung ;
Yoon, Won-Sub ;
Kwon, Kyungjung .
JOURNAL OF HAZARDOUS MATERIALS, 2022, 425
[4]   Key Challenges and Opportunities for Recycling Electric Vehicle Battery Materials [J].
Beaudet, Alexandre ;
Larouche, Francois ;
Amouzegar, Kamyab ;
Bouchard, Patrick ;
Zaghib, Karim .
SUSTAINABILITY, 2020, 12 (14)
[5]   Investigation of the Particle Formation Mechanism during Coprecipitation of Ni-Rich Hydroxide Precursor for Li-Ion Cathode Active Material [J].
Berk, Rafael B. ;
Beierling, Thorsten ;
Metzger, Lukas ;
Gasteiger, Hubert A. .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2023, 170 (11)
[6]   Impact of Sulfate Adsorption on Particle Morphology during the Precipitation of Ni-Rich Hydroxide Precursors for Li-Ion Battery Cathode Active Materials [J].
Berk, Rafael B. ;
Beierling, Thorsten ;
Metzger, Lukas ;
Gasteiger, Hubert A. .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2023, 170 (11)
[7]   A routine for the determination of the microstructure of stacking-faulted nickel cobalt aluminium hydroxide precursors for lithium nickel cobalt aluminium oxide battery materials [J].
Bette, Sebastian ;
Hinrichsen, Bernd ;
Pfister, Daniela ;
Dinnebier, Robert E. .
JOURNAL OF APPLIED CRYSTALLOGRAPHY, 2020, 53 :76-87
[8]   NEW COMPOSITIONAL AND STRUCTURAL DATA VALIDATE THE STATUS OF JAMBORITE [J].
Bindi, Luca ;
Christy, Andrew G. ;
Mills, Stuart J. ;
Ciriotti, Marco E. ;
Bittarello, Erica .
CANADIAN MINERALOGIST, 2015, 53 (05) :791-802
[9]   The Twelve Principles of Circular Hydrometallurgy [J].
Binnemans, Koen ;
Jones, Peter Tom .
JOURNAL OF SUSTAINABLE METALLURGY, 2023, 9 (01) :1-25
[10]   Recovery of lithium, cobalt and other metals from lithium-ion batteries [J].
Celep, Oktay ;
Yazici, Ersin Y. ;
Deveci, Haci ;
Dorfling, Christie .
PAMUKKALE UNIVERSITY JOURNAL OF ENGINEERING SCIENCES-PAMUKKALE UNIVERSITESI MUHENDISLIK BILIMLERI DERGISI, 2023, 29 (04) :384-400