Voltage and temperature effects on low cobalt lithium-ion battery cathode degradation

被引:0
作者
Malabet, Hernando J. Gonzalez [1 ]
Gober, Megan [1 ]
Patel, Prehit [1 ]
L'Antigua, Alex [1 ]
Gabhart, Austin [1 ]
Amai, Joseah [1 ]
Xiao, Xianghui [2 ]
Nelson, George J. [1 ]
机构
[1] Univ Alabama, Dept Mech & Aerosp Engn, Huntsville, AL 35899 USA
[2] Brookhaven Natl Lab, Natl Synchrotron Lightsource 2, Upton, NY 11973 USA
来源
ENERGY ADVANCES | 2025年 / 4卷 / 02期
关键词
RELAXATION-TIMES; ELECTRODE THICKNESS; COMPOSITE CATHODES; AGING MECHANISMS; CELLS; STATE; DECONVOLUTION; PERFORMANCE; DISCHARGE; SURFACE;
D O I
10.1039/d4ya00530a
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Degradation of low cobalt lithium-ion cathodes was tested using a full factorial combination of upper cut-off voltage (4.0 V and 4.3 V vs. Li/Li+) and operating temperature (25 degrees C and 60 degrees C). Half-cell batteries were analyzed with electrochemical and microstructural characterization methods. Electrochemical performance was assessed with galvanostatic cycling, cyclic voltammetry (CV), and electrochemical impedance spectroscopy (EIS) supported by distribution of relaxation times (DRT) analysis. Electrode microstructure was characterized with scanning electron microscopy (SEM), X-ray diffraction (XRD), and X-ray absorption near edge structure (XANES) imaging. Higher cut-off voltage cycling shows presence of NiOx formation, a low diffusivity rock-salt phase, in both CV and XRD data. XRD patterns confirmed that the rock-salt phase was beginning to form at the low cut-off voltage at high temperature, but in much lower intensity than at the high cut-off voltage. Higher temperature accelerates degradation processes at both voltages. Degradation factors at high temperature include NiOx formation, cathode material dissolution, and electrolyte decomposition. SEM analysis suggests that supporting phases may isolate and disconnect active material particles reducing capacity retention and battery life cycle. DRT analysis and XANES imaging show that both high temperature samples revealed a NiOx phase based on an increased diffusive impedance and a visible shift in the XANES spectra. The low cut-off voltage, high temperature sample showed a split peak and shift to lower energies indicating early formation of the NiOx phase. The diffusive impedance, which hinders intercalation and deintercalation, is driven by the formation of the NiOx phase. While primarily driven by cut-off voltage, elevated temperature also contributes to this degradation mechanism.
引用
收藏
页码:304 / 319
页数:16
相关论文
共 90 条
  • [1] Proll J., Kohler R., Torge M., Ulrich S., Ziebert C., Bruns M., Seifert H.J., Pfleging W., Laser Microstructuring and Annealing Processes for Lithium Manganese Oxide Cathodes, Appl. Surf. Sci., 257, 23, pp. 9968-9976, (2011)
  • [2] Zheng H., Li J., Song X., Liu G., Battaglia V.S., A Comprehensive Understanding of Electrode Thickness Effects on the Electrochemical Performances of Li-Ion Battery Cathodes, Electrochim. Acta, 71, pp. 258-265, (2012)
  • [3] Proll J., Kim H., Pique A., Seifert H.J., Pfleging W., Laser-Printing and Femtosecond-Laser Structuring of LiMn<sub>2</sub>O<sub>4</sub> Composite Cathodes for Li-Ion Microbatteries, J. Power Sources, 255, pp. 116-124, (2014)
  • [4] Singh M., Kaiser J., Hahn H., Thick Electrodes for High Energy Lithium Ion Batteries, J. Electrochem. Soc., 162, 7, pp. A1196-A1201, (2015)
  • [5] Danner T., Singh M., Hein S., Kaiser J., Hahn H., Latz A., Thick Electrodes for Li-Ion Batteries: A Model Based Analysis, J. Power Sources, 334, pp. 191-201, (2016)
  • [6] Mangang M., Seifert H.J., Pfleging W., Influence of Laser Pulse Duration on the Electrochemical Performance of Laser Structured LiFePO<sub>4</sub> Composite Electrodes, J. Power Sources, 304, pp. 24-32, (2016)
  • [7] Ruan Y., Song X., Fu Y., Song C., Battaglia V., Structural Evolution and Capacity Degradation Mechanism of LiNi<sub>0.6</sub>Mn<sub>0.2</sub>Co<sub>0.2</sub>O<sub>2</sub> Cathode Materials, J. Power Sources, 400, pp. 539-548, (2018)
  • [8] Rajendra T., Mistry A.N., Patel P., Ausderau L.J., Xiao X., Mukherjee P.P., Nelson G.J., Quantifying Transport, Geometrical, and Morphological Parameters in Li-Ion Cathode Phases Using X-Ray Microtomography, ACS Appl. Mater. Interfaces, 11, 22, pp. 19933-19942, (2019)
  • [9] Zheng S., Hong C., Guan X., Xiang Y., Liu X., Xu G.-L., Liu R., Zhong G., Zheng F., Li Y., Zhang X., Ren Y., Chen Z., Amine K., Yang Y., Correlation between Long Range and Local Structural Changes in Ni-Rich Layered Materials during Charge and Discharge Process, J. Power Sources, 412, pp. 336-343, (2019)
  • [10] Chen K.-H., Namkoong M.J., Goel V., Yang C., Kazemiabnavi S., Mortuza S.M., Kazyak E., Mazumder J., Thornton K., Sakamoto J., Dasgupta N.P., Efficient Fast-Charging of Lithium-Ion Batteries Enabled by Laser-Patterned Three-Dimensional Graphite Anode Architectures, J. Power Sources, 471, (2020)