The solution treatment temperature and duration regulate the SIMT mechanism in laser powder bed fusion Ti-10V-2Fe-3Al alloys

被引:0
作者
Yang, Ziwei [1 ,2 ]
Xu, Junqiang [1 ,2 ]
Zhou, Qi [1 ,2 ]
Li, Cong [1 ,2 ]
Kong, Jian [1 ,2 ]
Wang, Kehong [1 ]
机构
[1] Nanjing Univ Sci & Technol, Sch Mat Sci & Engn, Nanjing 210094, Peoples R China
[2] Minist Ind & Informat Technol, Key Lab Controlled Arc Intelligent Addit Mfg Techn, Nanjing 210094, Peoples R China
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
Laser powder bed fusion; Ti-10 V-2Fe-3Al alloy; Solution treatment; Stress-induced martensitic transformation (SIMT); Mechanical properties; INDUCED MARTENSITIC-TRANSFORMATION; PHASE-TRANSFORMATION; TITANIUM-ALLOY; HEAT-TREATMENT; ALPHA-PHASE; BETA; STRAIN; HOMOGENIZATION; KINETICS;
D O I
10.1016/j.matchar.2025.114948
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Heat treatment is a crucial postprocessing step to tailor the microstructure and enhance the mechanical properties of additively manufactured titanium alloys. This study investigated the effects of solution treatment temperature and duration on the microstructural and mechanical properties of LPBF-fabricated Ti-1023, focusing on the activation and regulation of the stress-induced martensitic transformation (SIMT) mechanism. The as- fabricated sample exhibited a dual-phase ((3 + wiso). Increasing the solution temperature from 600 degrees C to 800 degrees C reduced alpha phase content from 52.7 % to 15.3 %. A prolonged duration at 900 degrees C(10-40 min) induced substantial (3 grain coarsening, maintaining a ((3 + w) phase. The as-fabricated sample displayed brittle fracture, whereas the solution treatments significantly improved elongation. At 800 degrees C, the elongation reached 16.6 %, and further extending the duration at 900 degrees C increased it to 23.0 %, due to SIMT activation. During LPBF processing, repeated thermal cycles lead to a high density of dislocations (average KAM = 0.67 degrees) and promote the transformation of the preprecipitated w into a hard and brittle wiso, both of which contribute to brittle fracture. Solution treatment eliminated dislocations and facilitated wiso -> alpha phase transformation (325-410 degrees C), whereas alpha phase precipitation stabilized (3 through Al depletion and Fe/V enrichment. The SIMT is influenced by (3 phase stability ([Mo]eq) and grain size. Increasing the solution temperature reduced [Mo]eq from 23.0 to 14.8, with the critical [Mo]eq range for SIMT activation being 14.8-15.4. At 900 degrees C, [Mo]eq stabilized at 10.1, while lager grain size reduced alpha '' martensite content and elongation. Additionally, solution treatment promotes elemental homogenization, with optimal homogenization achieved after 2.4 min at 900 degrees C, resulting in the maximum elongation.
引用
收藏
页数:16
相关论文
共 50 条
  • [21] Study on the deformation behavior of β phase in Ti-10V-2Fe-3Al alloy by micro-indentation
    Ma, Xinkai
    Li, Fuguo
    Cao, Jun
    Sun, Zhankun
    Wan, Qiong
    Li, Jinghui
    Yuan, Zhanwei
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 703 : 298 - 308
  • [22] Effect of double annealing treatments on Ti-10V-2Fe-3Al alloy by directed energy deposition
    Deng, Hongwen
    Jiao, Zongge
    Cheng, Xu
    Qi, Shijie
    Tian, Xiangjun
    Wang, Yudai
    Zhang, Shuquan
    MATERIALS SCIENCE AND TECHNOLOGY, 2023, 39 (14) : 1792 - 1801
  • [23] Origin of Surface Irregularities on Ti-10V-2Fe-3Al Beta Titanium Alloy
    Utama, Muhammad Iman
    Ammar, Abdul Aziz
    Park, Nokeun
    Baek, Eung Ryul
    METALS AND MATERIALS INTERNATIONAL, 2018, 24 (02) : 291 - 299
  • [24] Massive transformation in dual-laser powder bed fusion of Ti6Al4V alloys
    Karimi, J.
    Zhao, C.
    Prashanth, K. G.
    JOURNAL OF MANUFACTURING PROCESSES, 2024, 119 : 282 - 292
  • [25] Hydrogen sintering, microstructure, and mechanical properties of Ti-10V-2Fe-3Al alloys prepared by the blended elemental method
    Tian, Qinghua
    Liu, Hanning
    Guo, Xueyi
    Dong, Zhaowang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 968
  • [26] Thermal stability of bulk nanocrystalline Ti-10V-2Fe-3Al alloy
    Chen, Wei
    Sun, Qiaoyan
    Xiao, Lin
    Sun, Jun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 536 : 223 - 230
  • [27] MACHINABILITY OF β-TITANIUM ALLOY TI-10V-2FE-3AL WITH DIFFERENT MICROSTRUCTURES
    Machai, Christian
    Abrahams, Hendrik
    Biermann, Dirk
    TMS 2012 141ST ANNUAL MEETING & EXHIBITION - SUPPLEMENTAL PROCEEDINGS, VOL 1: MATERIALS PROCESSING AND INTERFACES, 2012, : 919 - 926
  • [28] Effect of process parameters on the mechanical behavior of Ti6Al4V alloys fabricated by laser powder bed fusion method
    Baskin, Niyazi
    Yuce, Celalettin
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 30 : 7006 - 7019
  • [29] An in-situ neutron diffraction investigation of martensitic transformation in a metastable β Ti-10V-2Fe-3Al alloy during uniaxial tension
    Ducreux, Carla Isabel Pinilla
    Saleh, Ahmed A.
    Gazder, Azdiar A.
    Pereloma, Elena, V
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 869
  • [30] Characterization of the Anisotropy in the Microstructure and Mechanical Properties of Laser Powder Bed Fusion Ti6Al4V Alloys
    Huang, Qing
    Ge, Jinguo
    Wang, Yao
    Bao, Jiading
    He, Siliang
    Zhang, Zhenjie
    Zhang, Liang
    ADVANCED ENGINEERING MATERIALS, 2023, 25 (04)