Study on the fretting wear performance of oxide layer and Cr coating on zirconium alloy in high-temperature water

被引:1
|
作者
Jiao, Yong-jun [1 ,2 ]
Li, Zheng-yang [2 ]
Pu, Zeng-ping [2 ]
Zheng, Mei-yin [2 ]
Ren, Quan-yao [2 ]
Cai, Zhen-bing [3 ]
Wu, Yin-wei [1 ]
Qiu, Sui-zheng [1 ]
机构
[1] Xi An Jiao Tong Univ, State Key Lab Multiphase Flow Power Engn, Xian 710049, Peoples R China
[2] Nucl Power Inst China, Sci & Technol Reactor Syst Design Technol Lab, Chengdu 610213, Peoples R China
[3] Southwest Jiaotong Univ, Tribol Res Inst, Key Lab Adv Technol Mat, Chengdu 610031, Peoples R China
基金
中国国家自然科学基金;
关键词
Oxide layer; Cr coating; Fretting wear; Wear mechanism; BEHAVIOR; CLADDINGS;
D O I
10.1016/j.wear.2024.205597
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Grid-to-rod fretting wear is an important factor causing the fuel failure in nuclear power plants. Accident tolerant fuel (ATF) Cr coating and oxide ceramic coating have been developed to improve the fretting wear performance. In this research, two different oxide layers and Cr coating were prepared on zirconium (Zr) alloy, and the fretting wear performance were studied. The morphology, microstructure, tribo-corrosion reaction, and wear characteristics were analyzed. The oxide layer formed at high-temperature pressurized water (HTPW) has the lowest wear rate of 0.11 x 103 mu m3/Nm due to the high hardness and compact structure, which leads to the corresponding friction pairs presenting the highest wear rate of 8.42 x 103 mu m3/Nm. The wear depth of oxide layer formed at HTPW is about 5 times lower than that of as-received Zr alloy, and it is also less than the thickness of oxide layer. The oxide layer formed at HTPW after fretting has a larger thickness than the initial state because the plastic deformation layer caused by shear stress can quickly oxidize to zirconia in high-temperature water, and the wear rate of oxide layer is lower than the formation rate of oxide layer. The wear mechanism of two different oxide layers is delamination and abrasive wear, and that of Cr coating is abrasive wear and fatigue wear.
引用
收藏
页数:17
相关论文
共 50 条
  • [1] Characterization and fretting wear behavior of zirconium alloy treated in high temperature water
    Li, Zheng-yang
    Zheng, Mei-yin
    Ren, Quan-yao
    Cai, Zhen-bing
    Jiao, Yong-jun
    WEAR, 2023, 532
  • [2] Effect of temperature on the fretting wear behavior of Cr-coated Zircaloy cladding in high-temperature pressurized water
    Wang, Jun
    Li, Haojie
    Li, Zhengyang
    Lei, Yujie
    Ren, Quanyao
    Jiao, Yongjun
    Cai, Zhenbing
    JOURNAL OF NUCLEAR MATERIALS, 2023, 584
  • [3] Effect of micro-arc oxidation on fretting wear behavior of zirconium alloy exposed to high temperature water
    Lai, Ping
    Zhang, Hao
    Zhang, Lefu
    Zeng, Qifeng
    Lu, Junqiang
    Guo, Xianglong
    WEAR, 2019, 424 : 53 - 61
  • [4] High Temperature Oxidation Resistance of Cr Based Coating on Zirconium Alloy
    Shan W.
    Wang Y.
    Li J.
    Xiong L.
    Du X.
    Liu S.
    Cailiao Yanjiu Xuebao/Chinese Journal of Materials Research, 2022, 36 (09): : 699 - 705
  • [5] High-temperature oxidation of Zr-1Nb zirconium alloy with protective Cr/Mo coating
    Syrtanov, M. S.
    Kashkarov, E. B.
    Abdulmenova, A., V
    Sidelev, D., V
    SURFACE & COATINGS TECHNOLOGY, 2022, 439
  • [6] Evolution of fretting wear characteristics of Cr-coated cladding under high-temperature pressurized water environment
    Wang, Jun
    Li, Ke
    Wu, Yuchun
    Xie, Yujie
    Ni, Jing
    Zhu, Zefei
    Cai, Zhenbing
    NUCLEAR ENGINEERING AND DESIGN, 2024, 430
  • [7] High-temperature Oxidation and Tensile Behaviors of CrAl Coating on Zirconium Alloy
    Wei Donghui
    Wu Yawen
    He Xiujie
    Ma Xianfeng
    Wang Hui
    Shi Huiji
    CHINA SURFACE ENGINEERING, 2019, 32 (02) : 44 - 53
  • [8] Fretting corrosion fatigue of Alloy 690 in high-temperature pure water
    Liao, Jiapeng
    Wu, Xinqiang
    Tan, Jibo
    Tang, Lichen
    Qian, Hao
    Xie, Yongcheng
    CORROSION SCIENCE, 2018, 133 : 423 - 431
  • [9] Fretting wear behavior of alloy 690 tubes in high temperature steam and water
    Lai, Ping
    Zhang, Lefu
    Guo, Xianglong
    Tang, Lichen
    PROCEEDINGS OF ASIA INTERNATIONAL CONFERENCE ON TRIBOLOGY 2018 (ASIATRIB 2018), 2018, : 188 - 189
  • [10] Fretting Wear Characteristics of Nuclear Fuel Cladding in High-Temperature Pressurized Water
    Jun Wang
    Haojie Li
    Zhengyang Li
    Yujie Lei
    Quanyao Ren
    Yongjun Jiao
    Zhenbing Cai
    Chinese Journal of Mechanical Engineering, 36