Implementation of miniature tensile specimens in mechanical properties assessment of directed energy deposited Ti-6Al-4V: As-built and heat treated

被引:0
|
作者
Alipour, Saeid [1 ]
Wu, Sung-Heng [2 ]
Liou, Frank [2 ]
Emdadi, Arezoo [1 ]
机构
[1] Missouri Univ Sci & Technol, Dept Mat Sci & Engn, Rolla, MO 65409 USA
[2] Missouri Univ Sci & Technol, Dept Mech Engn, Rolla, MO 65409 USA
关键词
Ti-6Al-4V; DED; Miniature tensile test specimen; Heat treatment; Microstructure; MICROSTRUCTURE; ALPHA; BEHAVIOR; BETA;
D O I
10.1016/j.msea.2024.147593
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Within the last two decades, additive manufacturing (AM), a. k.a. 3D printing, has provided promising solutions for producing near-net-shape components with intricate geometries. From the material perspective, titanium alloys, one of humankind's most essential structural materials, are being considered the first candidate for AMed parts due to their unique characteristics in strength-weight-corrosion combinations. However, measuring the mechanical properties of designed geometry remains a challenge due to the ineffectiveness of conventional standard tensile specimens in assessing the site-specific and intricate geometries. In AM, the current approach often consists of evaluating standard-sized samples with the assumption that components with complex geometries possess comparable mechanical properties, even though they may have undergone different thermal processes in various situations. Hence, combining the microstructural characterization, this study aims to investigate the mechanical properties of direct energy deposition (DED) Ti-6Al-4V through a newly designed miniature tensile test (M-TT) specimen. The as-built specimen showed ultimate tensile strength (UTS) of similar to 1305.3 MPa and elongation of similar to 8.6 % with the mixed basketweave and alpha-colony microstructure. However, the DED Ti-6Al-4V specimen heat-treated at 850 degrees C exhibited the highest average elongation of similar to 13.2 % and decent UTS of similar to 1240.3 MPa with the alpha+beta microstructure.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] Tensile properties of Ti-6Al-4V as-built by laser metal deposition: The relationship between heat affected zone bands, strain localization and anisotropy in ductility
    Yvinec, T.
    Nait-Ali, A.
    Mellier, D.
    Bertheau, D.
    Cormier, J.
    Villechaise, P.
    Rat, L.
    Hemery, S.
    ADDITIVE MANUFACTURING, 2022, 55
  • [22] The Influence of As-Built Surface Conditions on Mechanical Properties of Ti-6Al-4V Additively Manufactured by Selective Electron Beam Melting
    Y. Y. Sun
    S. Gulizia
    C. H. Oh
    D. Fraser
    M. Leary
    Y. F. Yang
    M. Qian
    JOM, 2016, 68 : 791 - 798
  • [23] The Influence of As-Built Surface Conditions on Mechanical Properties of Ti-6Al-4V Additively Manufactured by Selective Electron Beam Melting
    Sun, Y. Y.
    Gulizia, S.
    Oh, C. H.
    Fraser, D.
    Leary, M.
    Yang, Y. F.
    Qian, M.
    JOM, 2016, 68 (03) : 791 - 798
  • [24] Tensile property and microstructure assessment of hydrogen treated Ti-6Al-4V alloy
    Vilane, V. N.
    Knutsen, R. D.
    Westraadt, J. E.
    MATERIALS CHARACTERIZATION, 2022, 184
  • [25] Mechanical properties of Ti-6Al-4V specimens produced by shaped metal deposition
    Baufeld, Bernd
    van der Biest, Omer
    SCIENCE AND TECHNOLOGY OF ADVANCED MATERIALS, 2009, 10 (01)
  • [26] Effect of microstructure and defects on fatigue behaviour of directed energy deposited Ti-6Al-4V
    Prabhu, A. W.
    Vincent, T.
    Chaudhary, A.
    Zhang, W.
    Babu, S. S.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2015, 20 (08) : 659 - 669
  • [27] Heat Treatment Variability Effects on the Mechanical Properties of Beta Solution Treated Ti-6Al-4V
    Calcaterra, J. R.
    THERMEC 2009, PTS 1-4, 2010, 638-642 : 401 - 406
  • [28] Microstructural Evolution and Mechanical Behavior of Heat Treated Ti-6Al-4V Powders
    Bhattiprolu V.S.
    Crawford G.A.
    Metallography, Microstructure, and Analysis, 2018, 7 (6) : 761 - 768
  • [29] Mechanical Performance of Heat Treated Ti-6Al-4V Friction Stir Welds
    Edwards, Paul
    Petersen, Marc
    Ramulu, M.
    Boyer, R.
    COST-AFFORDABLE TITANIUM III, 2010, 436 : 213 - +
  • [30] Effect of build orientation on the fatigue properties of as-built Electron Beam Melted Ti-6Al-4V alloy
    Persenot, Theo
    Burr, Alexis
    Martin, Guilhem
    Buffiere, Jean-Yves
    Dendievel, Remy
    Maire, Eric