Superplasticity Deformation of Sn-Bi-Based Solder Alloys

被引:0
作者
Yamauchi, Akira [1 ]
Kurose, Masashi [1 ]
机构
[1] Gunma Coll, Inst Technol, Mech Engn, Maebashi, Japan
来源
TMS 2024 153RD ANNUAL MEETING & EXHIBITION: SUPPLEMENTAL PROCEEDINGS | 2024年
关键词
Low-temperature solder; Pb-free solder; Sn-Bi alloy; Superplasticity; Strain-rate sensitivity;
D O I
10.1007/978-3-031-50349-8_147
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Low-temperature solder alloys have drawn a large amount of attention. Because using low-temperature soldering also reduces the energy cost of fabrication processes. It allows the fabrication of inexpensive assembly materials, such as printed circuit boards, without high-assembly temperature resistance and temperature-sensitive components, such as LEDs, by avoiding thermal damage. The superplasticity mechanism of Sn-based alloys has not yet been clearly established. Therefore, this study investigated the effects of third-element addition on the microstructure and superplastic behavior of Sn-Bi-based alloys. Low-melting-point Pb-free Sn-BiSb and Sn-Bi-Zn solder alloys were used in this study. Tensile tests were carried out on the alloys under various cooling rates, temperatures (25, 40, 60, and 80 degrees C), and strain rates (10(-3)-10(-1)/s). The Sb- and Zn-added Sn-Bi-based alloys demonstrated superplastic deformation at 80 degrees C. The strain-rate sensitivity index of the Sn-Bi-based alloys at 80 degrees C exceeded 3, which is the threshold considered for superplastic deformation behavior. These results suggest that the superplastic deformation of Sn-Bi-based alloys is independent of the grain size of the primary Sn phase.
引用
收藏
页码:1715 / 1721
页数:7
相关论文
共 50 条
[1]   Effects of minor Cu and Zn additions on the thermal, microstructure and tensile properties of Sn-Bi-based solder alloys [J].
Shen, Jun ;
Pu, Yayun ;
Yin, Henggang ;
Luo, Dengjun ;
Chen, Jie .
JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 614 :63-70
[2]   Effect of Sb and Zn Addition on the Microstructures and Tensile Properties of Sn-Bi-Based Alloys [J].
Yamauchi, Akira ;
Kurose, Masashi .
MATERIALS, 2022, 15 (03)
[3]   The Effect of Gallium Addition on the Microstructure and Superconducting Properties of In-Bi-Sn Solder Alloys [J].
Zhou, Jiye ;
Shahbazi, Mahboobeh ;
Poitras, Jordan T. ;
Tan, Xin Fu ;
Mcdonald, Stuart D. ;
Nogita, Kazuhiro .
JOURNAL OF ELECTRONIC MATERIALS, 2025, 54 (04) :2628-2637
[4]   Effect of aging treatment on microstructure and creep behaviour of Sn-Ag and Sn-Ag-Bi solder alloys [J].
Abd El-Rehim, A. F. ;
Zahran, H. Y. .
MATERIALS SCIENCE AND TECHNOLOGY, 2014, 30 (04) :434-438
[5]   Stationary stage of hot deformation and superplasticity of aluminium alloys [J].
Vainblat, Y ;
Davydov, V ;
Sharshagin, N .
ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 2000, 331-3 :471-476
[6]   Effects of Bi content on mechanical properties and bump interconnection reliability of Sn-Ag solder alloys [J].
Tateyama, K ;
Ubukata, H ;
Yamaoka, Y ;
Takahashi, K ;
Yamada, H ;
Saito, M .
1999 INTERNATIONAL SYMPOSIUM ON MICROELECTRONICS, PROCEEDINGS, 1999, 3906 :722-727
[7]   Eutectic orientation relationships in Sn-Bi solder [J].
Shen, X. ;
Zois, A. ;
Douglas, J. O. ;
Gourlay, C. M. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1035
[8]   Mechanisms of Creep Deformation in Pure Sn Solder Joints [J].
Lee, K. -O. ;
Morris, J. W., Jr. ;
Hua, Fay .
JOURNAL OF ELECTRONIC MATERIALS, 2013, 42 (03) :516-526
[9]   Mechanisms of Creep Deformation in Pure Sn Solder Joints [J].
K. -O. Lee ;
J. W. Morris ;
Fay Hua .
Journal of Electronic Materials, 2013, 42 :516-526
[10]   Indentation creep of lead-free Sn-9Zn and Sn-8Zn-3Bi solder alloys [J].
Mahmudi, R. ;
Geranmayeh, A. R. ;
Khanbareh, H. ;
Jahangiri, N. .
MATERIALS & DESIGN, 2009, 30 (03) :574-580