Effect of 0.12wt%Sr Addition on Structural, Mechanical and Tribological Properties of Al-12Si+10wt%Zn Alloy

被引:0
|
作者
Hekimoglu, Ali Pasa [1 ]
Zimitoglu, Sueha [1 ]
Haciosmanoglu, Murat [1 ]
机构
[1] Recep Tayyip Erdogan Univ, Fac Engn & Architecture, Mech Engn Dept, Rize, Turkiye
关键词
Al-12Si-based alloy; microstructure; strength properties; friction; wear; DRY SLIDING WEAR; AL-SI-CU; HEAT-TREATMENT; EUTECTIC MODIFICATION; GRAIN-REFINEMENT; ALUMINUM-ALLOYS; AS-CAST; MICROSTRUCTURE; BEHAVIOR; FRICTION;
D O I
10.1007/s40962-025-01564-0
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The effects of 0.12wt%Sr additive on some material properties of Al-12Si+10wt%Zn alloy were examined in this study. Al-12Si+10wt%Zn and Al-12Si+10wt%Zn+0.12wt%Sr alloys were manufactured by permanent mold casting. Microstructures of these alloys were examined with both optic and scanning electron microscopes. Phases in the alloys were identified by energy-dispersive spectroscopy and X-ray diffraction analyses. Hardness measurements were performed with the Brinell method. Mechanical and tribological properties of the alloys were investigated with tensile and friction-wear tests, respectively. The microstructure of the Al-12Si+10wt%Zn alloy consists of alpha-Al, eutectic Al-Si mixture, primary Si and beta phases. Al-12Si+10wt%Zn+0.12wt%Sr alloy includes the Al-Zn-Fe-Si and Sr-Al-Si phases in addition to phases observed in the Al-12Si+10wt%Zn alloy. Sr addition resulted in the eutectic silicon particles becoming thinner and a spherical-like shape. The Sr addition to the Al-12Si+10wt%Zn alloy caused the hardness, yield strength and tensile strength to increase from 97 HBN to 138 HBN, 163 MPa to 233 MPa and 215 MPa to 240 MPa, respectively. The addition of Sr also caused coefficient of friction and wear volume of the Al-12Si-10Zn alloy to decrease from 0.5189 to 0.4621 and 4.488 mm3 to 4.025 mm3, respectively. Effects of Sr additive on the material properties of the Al-12Si+10wt%Zn alloy were discussed based on the microstructural changes.
引用
收藏
页数:13
相关论文
共 50 条
  • [31] Effect of Ti Addition on the Microstructure and Mechanical Properties of SiC Matrix Composites Infiltrated by Al-Si (10 wt.%)-xTi Alloy
    Yu, Yajun
    Du, An
    Zhao, Xue
    Fan, Yongzhe
    Ma, Ruina
    Li, Shijie
    Wang, Wei
    Cui, Yaqi
    Cao, Xiaoming
    MATERIALS, 2019, 12 (02):
  • [32] Investigation of mechanical, electrical, and thermal properties of a Zn-1.26 wt% Al alloy
    Cadirli, Emin
    Sahin, Mevlut
    JOURNAL OF MATERIALS SCIENCE, 2011, 46 (05) : 1414 - 1423
  • [33] Investigation of the effects of T5 and T6 heat treatments on the structural, mechanical, and tribological properties of Zn-40Al-2Cu-0.1Sr alloy
    Hekimoglu, Ali Pasa
    Haciosmanoglu, Murat
    Tellioglu, Murat
    Savaskan, Temel
    JOURNAL OF THE FACULTY OF ENGINEERING AND ARCHITECTURE OF GAZI UNIVERSITY, 2024, 39 (04): : 2187 - 2196
  • [34] Effect of EMS Process on the Primary Si Refinement, Tensile and Fatigue Properties of Hyper-eutectic Al-15wt.%Si Alloy
    Baek, Min-Seok
    Kang, Tae-Hoon
    Kim, Jong-Ho
    Park, Jun-Pyo
    Euh, Kwangjun
    Lee, Kee-Ahn
    KOREAN JOURNAL OF METALS AND MATERIALS, 2022, 60 (05): : 360 - 369
  • [35] The effect of Mg content on microstructure in Al-12wt. %Zn-x Mg Alloy
    Suarez, M. A.
    Campillo, B.
    Rodriguez-Diaz, R. A.
    Alvarez-Fregoso, O.
    Juarez-Islas, J. A.
    JOURNAL OF APPLIED RESEARCH AND TECHNOLOGY, 2009, 7 (02) : 153 - 162
  • [36] Effect of Vanadium addition to Al-Si alloy on its mechanical, tribological and microstructure properties
    Kumar, Aakash
    Sasikumar, C.
    MATERIALS TODAY-PROCEEDINGS, 2017, 4 (02) : 307 - 313
  • [37] Effect of Strontium on the Microstructure, Mechanical, and Tribological Properties of the Zn–40Al–2Cu Alloy
    Murat Hacıosmanoğlu
    Murat Tellioğlu
    Ali Paşa Hekimoğlu
    International Journal of Metalcasting, 2023, 17 : 3133 - 3142
  • [38] Effect of Sc addition on the microstructure, mechanical properties, and damping capacity of Al-20Zn alloy
    Chen, Y.
    Liu, C. Y.
    Ma, Z. Y.
    Huang, H. F.
    Peng, Y. H.
    Hou, Y. F.
    MATERIALS CHARACTERIZATION, 2019, 157
  • [39] Effect of Isothermal Treatment on Mechanical and Tribological Properties of Alloy Zn – 40% Al – 2% Cu – 2% Si
    Temel Savaşkan
    Ali Paşa Hekimoğlu
    Zeki Azaklı
    Metal Science and Heat Treatment, 2023, 65 : 254 - 261
  • [40] Solidification microstructure and mechanical properties of an Al-11wt%Si alloy modified with Nb and Sb
    Obara, Thomas J.
    Minei, Raphael O.
    Kakitani, Rafael
    Spinelli, Jose E.
    Garcia, Amauri
    Cheung, Noe
    JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 2023, 181