Impact of Fire-Retardant coating on the residual compressive strength of hybrid Fibre-Reinforced polymer tubes exposed to elevated temperature
被引:0
|作者:
Abolfazli, Milad
[1
]
Bazli, Milad
[1
,2
]
Regmi, Sashidhar
[1
]
Shakiba, Milad
[1
]
Ojo, Caleb O.
[1
]
Rajabipour, Ali
[1
]
Hassanli, Reza
[3
]
Shahbazi, Ramin
[1
]
Arashpour, Mehrdad
[4
]
机构:
[1] Charles Darwin Univ, Fac Sci & Technol, Darwin, Australia
[2] Univ Queensland, Sch Mech & Min Engn, Brisbane, Qld, Australia
[3] Univ South Australia, UniSA STEM, Mawson Lakes, Australia
[4] Monash Univ, Dept Civil Engn, Melbourne, Vic 3800, Australia
关键词:
Hybrid fibre-reinforced polymer;
Elevated temperature;
Fire retardant coating;
Thermal degradation;
Mechanical properties;
Composite tubes;
MECHANICAL-PROPERTIES;
HYDRAULIC PRESSURE;
TENSILE-STRENGTH;
FRP;
COMPOSITES;
CONCRETE;
BEHAVIOR;
CARBON;
PERFORMANCE;
EPOXY;
D O I:
10.1016/j.compositesa.2025.108831
中图分类号:
T [工业技术];
学科分类号:
08 ;
摘要:
Enhancing the fire resistance of fibre-reinforced polymer (FRP) composites is vital for ensuring structural safety in fire-prone infrastructures. This study investigates the thermal degradation and residual compressive strength of filament-wound hybrid fibre-reinforced polymer (HFRP) tubes exposed to temperatures ranging from 25 degrees C to 350 degrees C. The tubes, composed of 50 % carbon fibre and 50 %E-glass fibre, with a 60:40 fibre-resin ratio, were subjected to thermal conditioning to simulate real-world fire exposure. For uncoated tubes, a balance between resin post-curing and pyrolytic degradation preserves compressive strength up to 200 degrees C, but strength sharply decreases beyond this threshold due to intensified pyrolysis, with virtually no residual strength at 350 degrees C. Fireretardant coatings, Nullifire SC902, activate above 200 degrees C, providing limited protection, and the samples retain 20-21 % of their original compressive strength at 350 degrees C. As revealed by complementary Scanning Electron Microscopy (SEM), Thermogravimetric Analysis (TGA), Differential Scanning Calorimetry (DSC), and Fourier Transform Infrared Spectroscopy (FTIR) analyses, key degradation mechanisms include matrix degradation and cracking and fibre exposure. Overall, the fire-retardant coating offers some benefits at higher temperatures, but its effectiveness is limited by activation thresholds and prolonged exposure. The findings show the need for further optimisation of fire-resistant systems for HFRP composites to improve their safety and durability in fireprone applications.