Impact of Fire-Retardant coating on the residual compressive strength of hybrid Fibre-Reinforced polymer tubes exposed to elevated temperature

被引:0
|
作者
Abolfazli, Milad [1 ]
Bazli, Milad [1 ,2 ]
Regmi, Sashidhar [1 ]
Shakiba, Milad [1 ]
Ojo, Caleb O. [1 ]
Rajabipour, Ali [1 ]
Hassanli, Reza [3 ]
Shahbazi, Ramin [1 ]
Arashpour, Mehrdad [4 ]
机构
[1] Charles Darwin Univ, Fac Sci & Technol, Darwin, Australia
[2] Univ Queensland, Sch Mech & Min Engn, Brisbane, Qld, Australia
[3] Univ South Australia, UniSA STEM, Mawson Lakes, Australia
[4] Monash Univ, Dept Civil Engn, Melbourne, Vic 3800, Australia
关键词
Hybrid fibre-reinforced polymer; Elevated temperature; Fire retardant coating; Thermal degradation; Mechanical properties; Composite tubes; MECHANICAL-PROPERTIES; HYDRAULIC PRESSURE; TENSILE-STRENGTH; FRP; COMPOSITES; CONCRETE; BEHAVIOR; CARBON; PERFORMANCE; EPOXY;
D O I
10.1016/j.compositesa.2025.108831
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Enhancing the fire resistance of fibre-reinforced polymer (FRP) composites is vital for ensuring structural safety in fire-prone infrastructures. This study investigates the thermal degradation and residual compressive strength of filament-wound hybrid fibre-reinforced polymer (HFRP) tubes exposed to temperatures ranging from 25 degrees C to 350 degrees C. The tubes, composed of 50 % carbon fibre and 50 %E-glass fibre, with a 60:40 fibre-resin ratio, were subjected to thermal conditioning to simulate real-world fire exposure. For uncoated tubes, a balance between resin post-curing and pyrolytic degradation preserves compressive strength up to 200 degrees C, but strength sharply decreases beyond this threshold due to intensified pyrolysis, with virtually no residual strength at 350 degrees C. Fireretardant coatings, Nullifire SC902, activate above 200 degrees C, providing limited protection, and the samples retain 20-21 % of their original compressive strength at 350 degrees C. As revealed by complementary Scanning Electron Microscopy (SEM), Thermogravimetric Analysis (TGA), Differential Scanning Calorimetry (DSC), and Fourier Transform Infrared Spectroscopy (FTIR) analyses, key degradation mechanisms include matrix degradation and cracking and fibre exposure. Overall, the fire-retardant coating offers some benefits at higher temperatures, but its effectiveness is limited by activation thresholds and prolonged exposure. The findings show the need for further optimisation of fire-resistant systems for HFRP composites to improve their safety and durability in fireprone applications.
引用
收藏
页数:17
相关论文
共 44 条
  • [1] Residual compressive strength of filament wound hybrid glass/carbon fibre reinforced polymer tubes after exposure to elevated temperature
    Abolfazli, Milad
    Bazli, Milad
    Rajabipour, Ali
    Heitzmann, Michael
    Pourasiabi, Hamid
    Wang, Hao
    Arashpour, Mehrdad
    COMPOSITE STRUCTURES, 2023, 316
  • [2] Residual compressive section capacity of filament wound carbon, glass, and basalt fibre-reinforced polymer tubes: Influence of elevated temperatures
    Abolfazli, Milad
    Bazli, Milad
    Rajabipour, Ali
    Heitzmann, Michael T.
    Amirzadeh, Zhila
    COMPOSITE STRUCTURES, 2023, 304
  • [3] Tensile strength retention of fibre-reinforced polymer composites exposed to elevated temperatures: A meta-analysis review
    Machello, Chiara
    Bazli, Milad
    Santos, Josiah
    Rajabipour, Ali
    Arashpour, Mehrdad
    Hassanli, Reza
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 438
  • [4] Tree-based machine learning approach to modelling tensile strength retention of Fibre Reinforced Polymer composites exposed to elevated temperatures
    Machello, Chiara
    Baghaei, Keyvan Aghabalaei
    Bazli, Milad
    Hadigheh, Ali
    Rajabipour, Ali
    Arashpour, Mehrdad
    Rad, Hooman Mahdizadeh
    Hassanli, Reza
    COMPOSITES PART B-ENGINEERING, 2024, 270
  • [5] Residual compressive strength of seawater sea sand concrete filled hybrid carbon-glass fibre reinforced polymer tubes under seawater: Effects of fibre type and orientation
    Bazli, Milad
    Benny, Benzen
    Rajabipour, Ali
    Pourasiabi, Hamid
    Heitzmann, Michael T.
    Arashpour, Mehrdad
    JOURNAL OF BUILDING ENGINEERING, 2023, 70
  • [6] Circular fibre-reinforced polymer (FRP)-concrete-steel hybrid multitube concrete columns: Compressive behaviour
    Chan, C. W.
    Zhang, S. S.
    Yu, T.
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 272
  • [7] Residual Strength Characteristics of Polymer Fibre Concrete Exposed To Elevated Temperature
    Thirumurugan, Sengottaiyan
    Anandan, Sivakumar
    ENGINEERING JOURNAL-THAILAND, 2015, 19 (04): : 117 - 131
  • [8] Predicting residual strength of hybrid fibre-reinforced Self-compacting concrete (HFR-SCC) exposed to elevated temperatures using machine learning
    Khan, Muhammad Saud
    Ma, Liqiang
    Bin Inqiad, Waleed
    Khan, Majid
    Khan, Naseer Muhammad
    Alarifi, Saad S.
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2025, 22
  • [9] STRENGTH AND BOND CHARACTERISTICS OF HYBRID FIBRE REINFORCED CONCRETE SUBJECTED TO ELEVATED TEMPERATURE
    Krishna, Arathi
    Kaliyaperumal, Saravana Raja Mohan
    REVISTA ROMANA DE MATERIALE-ROMANIAN JOURNAL OF MATERIALS, 2021, 51 (04): : 543 - 551
  • [10] Flexural response of steel beams strengthened by fibre-reinforced plastic plate and fire retardant coating at elevated temperatures
    Ahmed, Alim Al Ayub
    Kharnoob, Majid M.
    Akhmadeev, Ravil
    Sevbitov, Andrei
    Jalil, Abduladheem Turki
    Kadhim, Mustafa M.
    Hansh, Zahra J.
    Mustafa, Yasser Fakri
    Akhmadullina, Irina
    STRUCTURAL ENGINEERING AND MECHANICS, 2022, 83 (04) : 551 - 561