Solar-induced photocatalytic degradation of textile dyes using composite of indium oxide and silver vanadate

被引:0
|
作者
Shahid, Tazeen [1 ]
Yasmin, Nazia [1 ]
Kosar, Shazia [1 ]
Khalid, Arooma [1 ]
Naz, Rubina [1 ]
Maria, Hafiza [1 ]
Safdar, Muhammad [2 ]
Mirza, Misbah [1 ]
机构
[1] Women Univ, Dept Phys, Multan, Pakistan
[2] Khawaja Fareed Univ Engn & Informat Technol, Dept Basic Sci & Humanities, Rahim Yar Khan, Pakistan
关键词
Key words: metal vanadate; methylene blue; textile dyes; photocatalytic degradation; N-N HETEROJUNCTION; GOLD NANOPARTICLES; METHYLENE-BLUE; EFFICIENT; TIO2; NANOSTRUCTURES; NANOCOMPOSITES;
D O I
10.1139/cjc-2024-0078
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
In the present study, the synthesized samples indium oxide (In2O3), silver vanadate (Ag3VO4), and composite (In2O3/Ag3VO4) are prepared by using co-precipitation method. These samples showed a very effective photocatalytic response for the degradation of a dye methylene blue (MB) in the presence of sunlight. The physical properties of samples are characterized by XRD, scanning electron microscopy (SEM), FTIR, and ultraviolet (UV) spectroscopy. The structure analysis and crystalline size of prepared samples were examined by XRD. Debye Scherrer's formula had been used to calculate the crystalline size and its value is 19.1 nm of In2O3, 10.8 nm of Ag3VO4, and 1.65 nm of In2O3/Ag3VO4. FTIR absorption spectroscopy was carried out in the range of 500-4000 cm(-1) to verify the synthesized material's structural properties. FTIR spectrum also provides the information about the material's functional groups. The morphology of indium oxide, silver vanadate, and composite was analyzed by SEM. The calculated grain sizes of indium oxide, silver vanadate, and In2O3/Ag3VO4 composite are 0.13, 0.72, and 0.56 mu m, respectively. The optical properties indicate a small band gap for composite, which is 1.65 eV and showed strong absorption for sunlight. The photocatalytic degradation of MB was performed by using prepared catalysts in the presence of sunlight at wavelength 300-900 nm by UV spectroscopy. Indium oxide degraded MB to 76.5% and silver vanadate degraded MB to 71%, while the composite degraded MB to 85.5%. The results of UV spectroscopy showed that the composite is very effective in photocatalytic degradation MB dye.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] Solar-Induced Photocatalytic Degradation of Reactive Red and Turquoise Dyes Using a Titanium Oxide/Xanthan Gum Composite
    Alwared, Abeer I.
    Mohammed, Noor A.
    Al-Musawi, Tariq J.
    Mohammed, Ahmed A.
    SUSTAINABILITY, 2023, 15 (14)
  • [2] Solar/UV-induced photocatalytic degradation of three commercial textile dyes
    Neppolian, B
    Choi, HC
    Sakthivel, S
    Arabindoo, B
    Murugesan, V
    JOURNAL OF HAZARDOUS MATERIALS, 2002, 89 (2-3) : 303 - 317
  • [3] Solar-induced heterogeneous photocatalytic degradation of methyl-paraben
    Velegraki, Theodora
    Hapeshi, Evroula
    Fatta-Kassinos, Despo
    Poulios, Ioannis
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2015, 178 : 2 - 11
  • [4] Photocatalytic degradation of textile dyes using phycosynthesised ZnO nanoparticles
    Prerna
    Agarwal, Harshit
    Goyal, Dinesh
    INORGANIC CHEMISTRY COMMUNICATIONS, 2022, 142
  • [5] Solar light induced photocatalytic degradation of textile dyes using solvothermally synthesized SnO2 impregnated pumice stone
    Rajput, Rekha B.
    Salunkhe, Abhaysinh
    Kale, Rohidas B.
    PHYSICA SCRIPTA, 2023, 98 (10)
  • [6] Solar photocatalytic degradation of textile dyes in TiO2 suspended solutions
    Ye, Yu-Li
    Xiao, Zhi-Xue
    Liu, Lian-Hui
    Hong, Yong-Zhe
    Guocheng Gongcheng Xuebao/The Chinese Journal of Process Engineering, 2006, 6 (SUPPL. 2): : 342 - 348
  • [7] SOLAR PHOTOCATALYTIC DEGRADATION OF TEXTILE DYES ON DYNAMIC PILOT PLANT USING SUPPORTED TiO2
    Barka, Noureddine
    Qourzal, Samir
    Assabbane, Ali
    Ait-Ichou, Yhya
    Nounah, Abderrahman
    Lachheb, Hinda
    Houas, Ammar
    ARABIAN JOURNAL FOR SCIENCE AND ENGINEERING, 2010, 35 (2A) : 131 - 137
  • [8] MA Photocatalytic Degradation of Textile Reactive Dyes-A Comparative Study Using Nano Silver Decorated Titania-Silica Composite Photocatalysts
    Ramamoorthy, Vaithiyanathan
    Kannan, Kathiravan
    Thiripuranthagan, Sivakumar
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2018, 18 (04) : 2921 - 2930
  • [9] Synthesis and characterization of silver-indium and antimony selenide: role in photocatalytic degradation of dyes
    Yasmin, N.
    Liaqat, A.
    Ali, G.
    Kalsoom, A.
    Safdar, M.
    Mirza, M.
    HELIYON, 2022, 8 (10)
  • [10] Photocatalytic degradation of Rhodamine dyes using zinc oxide nanoparticles
    Dodoo-Arhin, D.
    Asiedu, T.
    Agyei-Tuffour, B.
    Nyankson, E.
    Obada, D.
    Mwabora, J. M.
    MATERIALS TODAY-PROCEEDINGS, 2021, 38 : 809 - 815