Understanding interfacial bonding properties and mechanical properties of in situ synthesis of Cf/ZrB2-ZrC-SiC composite

被引:0
作者
Liu, Yingjun [1 ,2 ]
Fu, Yuanzhe [2 ]
Zu, Yufei [3 ]
Zhang, Yang [1 ,2 ]
Dong, Hongfeng [1 ,2 ]
Li, Wenhu [1 ,2 ]
Ai, Taotao [1 ,2 ]
Sha, Jianjun [4 ]
机构
[1] Shaanxi Univ Technol, Natl & Local Joint Engn Lab Slag Comprehens Utiliz, Hanzhong 116024, Peoples R China
[2] Shaanxi Univ Technol, Sch Mat Sci & Engn, Hanzhong, Peoples R China
[3] Dalian Univ Technol, Sch Mat Sci & Engn, Dalian, Peoples R China
[4] Dalian Univ Technol, State Key Lab Struct Anal Ind Equipment, Dalian 116024, Peoples R China
基金
中国国家自然科学基金; 国家重点研发计划;
关键词
ceramic matrix composites; interfaces; mechanical properties; ultra-high temperature ceramics; CERAMIC-MATRIX COMPOSITES; FIBER COATING THICKNESS; C-F/ZRB2-SIC COMPOSITE; RESIDUAL-STRESS; BEHAVIOR; MICROSTRUCTURE; INFILTRATION; OXIDATION; ABLATION; PERFORMANCE;
D O I
10.1111/jace.20411
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The relationship between the interfacial bonding properties and the mechanical properties of carbon fiber reinforced ZrB2-ZrC-SiC composites (Cf/ZrB2-ZrC-SiC) is currently under investigation. In this study, Cf/ZrB2-ZrC-SiC composites with varying fiber-matrix interfacial bonding properties were prepared using slurry infiltration and in-situ reactive hot pressing. Polydopamine-derived carbon with different thicknesses was employed as the interphase to create various interfacial bonding properties, where interfacial bonding properties were evaluated using the single-fiber push-out method. Results indicated that a uniform and dense ZrB2-ZrC-SiC matrix was constructed, and low-porosity composites without fiber degradation were obtained. For composites with a higher interfacial shear strength (ISS) of 342 MPa, flexural strength and fracture toughness were 209 MPa and 7.5 MPa<middle dot>m1/2, respectively. For composites with a lower ISS of 64 MPa, flexural strength and fracture toughness increased by 41% and 13%, with showing non-brittle behavior and work of fracture up to 10 kJ<middle dot>m2. By combining analyses of thermal expansion behavior, residual thermal stresses, and thermal shock properties at ultrahigh temperatures, thermal mismatch and thermal damage can be minimized through the modulation of ISS. This approach is beneficial for optimizing the mechanical properties of fiber-reinforced ceramic composites.
引用
收藏
页数:13
相关论文
共 46 条
  • [1] Milling time and sintering parameters optimization to fabricate ZrB2-30 vol% SiC composite with highest thermal shock resistance
    Akhlaghi, Nima
    Balak, Zohre
    Birgani, Ebrahim Najafi
    [J]. MATERIALS RESEARCH EXPRESS, 2019, 6 (05)
  • [2] Synergetic effects of SiC and Csf in ZrB2-based ceramic composites. Part II: Grain growth
    Asl, Mehdi Shahedi
    Kakroudi, Mandi Ghassemi
    Farahbakhsh, Iman
    Mazinani, Babak
    Balak, Zohre
    [J]. CERAMICS INTERNATIONAL, 2016, 42 (16) : 18612 - 18619
  • [3] Ablation behaviour of carbon fibre ultra-high temperature composites at oblique angles of attack
    Baker, B.
    Venkatachalam, V.
    Zoli, L.
    Vinci, A.
    Failla, S.
    Sciti, D.
    Binner, J.
    [J]. MATERIALS & DESIGN, 2021, 212
  • [4] Open porosity and grain size effect on the mechanical property of ZrB2-30SiC containing HfB2
    Balak, Zohre
    [J]. MATERIALS RESEARCH EXPRESS, 2019, 6 (09)
  • [5] Ablation behavior of three-dimensional Cf/SiC-ZrC-ZrB2 composites prepared by a joint process of sol-gel and reactive melt infiltration
    Chen, Xiaowu
    Feng, Qian
    Zhou, Haijun
    Dong, Shaoming
    Wang, Jingxiao
    Cao, Yanpeng
    Kan, Yanmei
    Ni, Dewei
    [J]. CORROSION SCIENCE, 2018, 134 : 49 - 56
  • [6] Interphase degradation of three-dimensional Cf/SiC-ZrC-ZrB2 composites fabricated via reactive melt infiltration
    Chen, Xiaowu
    Feng, Qian
    Gao, Le
    Zhang, Xiangyu
    Dong, Shaoming
    Wang, Jingxiao
    Zhong, Qiang
    Kan, Yanmei
    Ni, Dewei
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2017, 100 (10) : 4816 - 4826
  • [7] Microstructure and mechanical properties of three dimensional Cf/SiC-ZrC-ZrB2 composites prepared by reactive melt infiltration method
    Chen, Xiaowu
    Dong, Shaoming
    Kan, Yanmei
    Jin, Xihai
    Zhou, Haijun
    Ni, Dewei
    Wang, Dengke
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2016, 36 (16) : 3969 - 3976
  • [8] Ultra-high-temperature mechanical behaviors of two-dimensional carbon fiber reinforced silicon carbide composites: Experiment and modeling
    Cheng, Tianbao
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2021, 41 (04) : 2335 - 2346
  • [9] Using PyC modified 3D carbon fiber to reinforce UHTC under low temperature sintering without pressure
    Du, Baihe
    Cheng, Yuan
    Xun, Liancai
    Zhang, Shuchang
    Tong, Jing
    Lv, Qingrong
    Zhou, Shanbao
    Hu, Ping
    Zhang, Xinghong
    [J]. JOURNAL OF ADVANCED CERAMICS, 2021, 10 (04) : 871 - 884
  • [10] Toughening effect of non-periodic fiber distribution on crack propagation energy of UHTC composites
    Failla, S.
    Galizia, P.
    Zoli, L.
    Vinci, A.
    Sciti, D.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 777 : 612 - 618