Non-destructive evaluation of early strength of concrete with slag thermally activated using electrical cable

被引:0
作者
Antonova, Anna [1 ]
Illarionova, Ekaterina [1 ]
Punkki, Jouni [1 ]
机构
[1] Aalto Univ, Dept Civil Engn, Rakentajanaukio 4, Espoo 02150, Finland
关键词
Cable heating; Thermal activation; Non-destructive tests; Slag; Early strength development; BLAST-FURNACE SLAG; ULTRASONIC PULSE VELOCITY; MECHANICAL-PROPERTIES; CURING TEMPERATURE; HYDRATION; HEAT; MICROSTRUCTURE; LIMESTONE;
D O I
10.1016/j.conbuildmat.2025.140170
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
High levels of clinker substitution by supplementary cementitious materials, such as slag, are necessary to decrease the CO2 emissions of concrete manufacturing. However, this leads to low early concrete strength, delaying construction schedules. In cold regions, heating is an essential part of accelerating the early hydration, thus, the strength of concrete. Therefore, this study analysed the effect of thermal activation of the concrete with 45% and 70% slag in the binder using internal electrical cable heating utilised in construction by evaluating compressive strength and heat development. In addition, non-destructive test methods, such as rebound hammer and ultrasound pulse velocity meter, were introduced to widen their application in estimating early strength development using the SonReb approach. The heating with the power of 20 Wand 30 W during the first 10-15 h (11.1-16.7 kWh/m3) effectively improved the early strength of concrete with 45% and 70% slag up to 14% and 60%, respectively during the first 24 h without any strength losses at the later ages. However, considering the initially low strength values (2.5-10 MPa) of concrete with 70% slag, the heat curing resulted in about a 1 - 4 MPa increase, with a maximum rise of 7 MPa, requiring additional strategies for slag activation, for example, alkali activation, to fulfil construction requirements.
引用
收藏
页数:13
相关论文
共 51 条
[1]   Slag uses in making an ecofriendly and sustainable concrete: A review [J].
Amran, Mugahed ;
Murali, G. ;
Khalid, Nur Hafizah A. ;
Fediuk, Roman ;
Ozbakkaloglu, Togay ;
Lee, Yeong Huei ;
Haruna, Sani ;
Lee, Yee Yong .
CONSTRUCTION AND BUILDING MATERIALS, 2021, 272 (272)
[2]  
[Anonymous], 2021, Testing Concrete in Structures-Part 4: Determination of Ultrasonic Pulse Velocity
[3]  
[Anonymous], 2004, Testing concrete in structures-Part 4: Determination of ultrasonic pulse velocity
[4]  
[Anonymous], 2019, TESTING HARDENED CON
[5]   Strength development of mortars containing ground granulated blast-furnace slag: Effect of curing temperature and determination of apparent activation energies [J].
Barnett, SJ ;
Soutsos, MN ;
Millard, SG ;
Bungey, JH .
CEMENT AND CONCRETE RESEARCH, 2006, 36 (03) :434-440
[6]   Low clinker systems-Towards a rational use of SCMs for optimal performance [J].
Ben Haha, Mohsen ;
Termkhajornkit, Pipat ;
Ouzia, Alexandre ;
Uppalapati, Siva ;
Huet, Bruno .
CEMENT AND CONCRETE RESEARCH, 2023, 174
[7]   SonReb concrete assessment for spatially correlated NDT data [J].
Breccolotti, Marco ;
Bonfigli, Massimo Federico ;
Materazzi, Annibale Luigi .
CONSTRUCTION AND BUILDING MATERIALS, 2018, 192 :391-402
[8]   Factors affecting the reactivity of slag at early and late ages [J].
Briki, Yosra ;
Zajac, Maciej ;
Ben Haha, Mohsen ;
Scrivener, Karen .
CEMENT AND CONCRETE RESEARCH, 2021, 150
[9]   The effect of w/b and temperature on the hydration and strength of blastfurnace slag cements [J].
Castellano, C. C. ;
Bonavetti, V. L. ;
Donza, H. A. ;
Irassar, E. F. .
CONSTRUCTION AND BUILDING MATERIALS, 2016, 111 :679-688
[10]   Evolution of mechanical properties of concrete containing ground granulated blast furnace slag and effects on the scaling resistance test at 28 days [J].
Chidiac, S. E. ;
Panesar, D. K. .
CEMENT & CONCRETE COMPOSITES, 2008, 30 (02) :63-71