Temperature influence on the repair of a hardfacing coating using laser metal deposition and assessment of the repair innocuity

被引:0
|
作者
Pacquentin, Wilfried [1 ]
Wident, Pierre [2 ]
Varlet, Jerome [2 ]
Cailloux, Thomas [2 ]
Maskrot, Hicham [2 ]
机构
[1] Univ Paris Saclay, CEA, Serv Physicochim, F-91191 Gif Sur Yvette, France
[2] Univ Paris Saclay, CEA, Serv Rech Mat & Proc Avances, F-91191 Gif sur Yvette, France
关键词
Additive manufacturing; Direct laser deposition; Hardfacing coating; Repair; Repair innocuity assessment; Mechanical characterization; STAINLESS-STEEL; THERMAL FATIGUE; CRACK FORMATION; MICROSTRUCTURE; TECHNOLOGY; SUPERALLOY; COMPONENTS; STRATEGIES; PARAMETERS; PATTERNS;
D O I
10.1016/j.jajp.2025.100284
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Additive manufacturing (AM) is a proven time- and cost-effective method for repairing parts locally damaged after e.g. repetitive friction wear or corrosion. Repairing a hardfacing coating using AM technologies presents however several simultaneous challenges arising from the complex geometry and a high probability of crack formation due to process-induced stress. We address the repair of a cobalt-based StelliteTM 6 hardfacing coating on an AISI 316L substrate performed using Laser Powder Directed Energy Deposition (LP-DED) and investigate the influence of key process features and parameters. We describe our process which successfully prevents crack formation both during and after the repair, highlighting the design of the preliminary part machining phase, induction heating of an extended part volume during the laser repair phase and the optimal scanning strategy. Local characterization using non-destructive testing, Vickers hardness measurements and microstructural examinations by scanning electron microscopy (SEM) show an excellent metallurgical quality of the repair and its interface with the original part. In addition, we introduce an innovative process qualification test assessing the repair quality and innocuity, which is based on the global response to induced cracks and probes the absence of crack attraction by the repair (ACAR1). Here this ACAR test reveals a slight difference in mechanical behavior between the repair and the original coating which motivates further work to eventually make the repair imperceptible.
引用
收藏
页数:19
相关论文
共 50 条
  • [31] Numerical and experimental investigation on laser metal deposition as repair technology for 316L stainless steel
    Zhan, M. J.
    Sun, G. F.
    Wang, Z. D.
    Shen, X. T.
    Yan, Y.
    Ni, Z. H.
    OPTICS AND LASER TECHNOLOGY, 2019, 118 : 84 - 92
  • [32] Repair of gas turbine engine components with laser powder deposition
    Miller, S
    Heath, M
    Woods, B
    Costello, A
    Sears, J
    TRENDS IN MATERIALS AND MANUFACTURING TECHNOLOGIES FOR TRANSPORTATION INDUSTRIES AND POWDER METALLURGY RESEARCH AND DEVELOPMENT IN THE TRANSPORTATION INDUSTRY, 2005, : 333 - 339
  • [33] Repair of Erosion Defects in Gun Barrels by Direct Laser Deposition
    Steffen Nowotny
    Joerg Spatzier
    Frank Kubisch
    Siegfried Scharek
    Jens Ortner
    Eckhard Beyer
    Journal of Thermal Spray Technology, 2012, 21 : 1173 - 1183
  • [34] Repair of Erosion Defects in Gun Barrels by Direct Laser Deposition
    Nowotny, Steffen
    Spatzier, Joerg
    Kubisch, Frank
    Scharek, Siegfried
    Ortner, Jens
    Beyer, Eckhard
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2012, 21 (06) : 1173 - 1183
  • [35] Electro-deposition as a repair method for embedded metal grids
    Oostra, A. Jolt
    Reddy, Anil
    Smits, Edsger C. P.
    Abbel, Robert
    Groen, Wilhelm A.
    Blom, Paulw. M.
    Michels, Jasper J.
    THIN SOLID FILMS, 2016, 603 : 202 - 205
  • [36] Geometry strategies for the repair of cylindrical gears teeth using laser-directed energy deposition
    Montoya-Zapata, Diego
    Ortiz, Igor
    Alvarez, Piera
    Azpeleta, Maria
    Garcia, Marta
    JOURNAL OF LASER APPLICATIONS, 2024, 36 (04)
  • [37] Repair of SiC coating on carbon/carbon composites by laser cladding technique
    Wang, Han-Hui
    Li, He-Jun
    Shi, Xiao-Hong
    Liu, Xue-Song
    Kong, Jing-An
    Zhou, Hang
    CERAMICS INTERNATIONAL, 2020, 46 (11) : 19537 - 19544
  • [38] Finite element investigation of residual stresses during laser powder deposition process as an innovative technique to repair worn rails
    Mortazavian, Ershad
    Wang, Zhiyong
    Teng, Hualiang
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART F-JOURNAL OF RAIL AND RAPID TRANSIT, 2023, 237 (01) : 21 - 32
  • [39] Laser metal deposition of AlSi10Mg for aeroengine casing repair: Microhardness, wear and corrosion behavior
    Dong, Enjie
    Chang, Tingyu
    Zhao, Linjie
    Xing, Yunhao
    Chen, Jiaxuan
    Chen, Mingjun
    Lu, Junwen
    Cheng, Jian
    MATERIALS TODAY COMMUNICATIONS, 2024, 38
  • [40] Novel Assessment Methodology for Laser Metal Deposition of New Metallic Alloys
    Cearsolo, Xabier
    Arrue, Mario
    Gabilondo, Maitane
    Sanchez, Jon Mikel
    Galarraga, Haize
    de Cortazar, Maider Garcia
    Girot Mata, Franck
    MATERIALS, 2023, 16 (02)