Oxidation mechanism and high-temperature strength of Mo-B-C-coated diamonds in the 700°C-1200 °C temperature range

被引:0
|
作者
Mao, Xinyue [1 ]
Meng, Qingnan [1 ,2 ,3 ]
Wang, Sifan [1 ]
Huang, Shiyin [1 ]
Yuan, Mu [1 ]
Qiu, Yuting [1 ]
机构
[1] Jilin Univ, Coll Construct Engn, Key Lab Minist Nat Resources Drilling & Exploitat, Changchun 130026, Peoples R China
[2] Jilin Univ, State Key Lab Superhard Mat, Changchun 130026, Peoples R China
[3] 938 Ximinzhu St, Changchun, Jilin, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 33卷
关键词
Diamond; Mo-B-C coating; Antioxidant; Compressive strength; B; 2; O; 3; THERMAL-CONDUCTIVITY; FLEXURAL STRENGTH; COMPOSITE; GRAPHITIZATION; RESISTANCE; INTERFACE; MICROSTRUCTURE; CERAMICS; COATINGS; BEHAVIOR;
D O I
10.1016/j.jmrt.2024.10.249
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To effectively inhibit the thermal oxidation and thermal failure of diamonds when working in a high-temperature aerobic environment, a Mo-B-C coating was designed and prepared to protect diamonds from oxidation. A two-step synthesis method was used to form coatings with different B contents on diamonds by adjusting the reaction temperature, and the oxidation kinetics and oxidation mechanism of the coated diamonds were investigated in the temperature range of 700 degrees C-1200 degrees C. The mechanism of diamond protection in this study was the preferential oxidative sacrifice of Mo-B-C coatings to form a stable oxide layer on the diamond surface. For low-B coatings, the four stages of coating oxidation, low-temperature volatilization of MoO3, stable protection by B2O3, and rapid evaporation of B2O3 were experienced sequentially with an increase in temperature. For high-B coatings, the preferential self-healing flow of B2O3 not only inhibited the volatilization of MoO3 but also provided a reducing environment for MoO3 to generate high melting-point MoO2 and Mo2C, which resulted in the formation of a double synergistic protective oxide layer and greatly enhanced the oxidation resistance of diamonds. Meanwhile, the protection of the oxide layer also maintained the compressive strength of diamonds under a high-temperature oxidizing atmosphere, indicating its excellent high temperature applicability. This study provides an effective method for enhancing the high-temperature oxidation resistance and strength of diamonds, which can be effectively applied to the extreme environmental use of diamond tools.
引用
收藏
页码:7829 / 7841
页数:13
相关论文
共 50 条
  • [41] On the oxidation mechanism of pure tungsten in the temperature range 600-800 °C
    Cifuentes, S. C.
    Monge, M. A.
    Perez, P.
    CORROSION SCIENCE, 2012, 57 : 114 - 121
  • [42] High-temperature oxidation behavior and pore structure of porous TiAl3 intermetallics at 650?C to 900?C
    Jiao, Xinyang
    Zhang, Yu
    Wu, Qingli
    Shang, Zhichao
    Yu, Yang
    Zhang, Xiaoxiao
    Feng, Peizhong
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 22 : 2398 - 2408
  • [43] Preparation of Mo-C-N-Si Coating on Mo Substrate and Its Oxidation Property at High Temperature
    Gu Siyong
    Zhang Houan
    Wu Yihui
    Xie Nengping
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (05) : 1219 - 1223
  • [44] High-Temperature Heat Treatment of Plasma Sprayed Ti-Si-C-Mo Coatings
    He, Jining
    Liu, Jialin
    Zhao, Hongjian
    Qin, Yanfang
    Fan, Jiawei
    Balazsi, Csaba
    COATINGS, 2024, 14 (01)
  • [45] High temperature oxidation of Zr-1Nb alloy with plasma electrolytic oxidation coating in 900-1200 °C steam environment
    Wang, Xingping
    Wei, Kejian
    Guan, Haohao
    Xu, Chi
    Xue, Wenbin
    Zhang, Yanwei
    Wang, Rongshan
    SURFACE & COATINGS TECHNOLOGY, 2021, 407
  • [46] High-temperature oxidation response of Mo-Si-B composites with TiO2w/SiCw addition
    Li, Bin
    Wang, Juan
    Chen, Xuan
    Li, Xiaohui
    Li, Rui
    Zhang, Guojun
    CERAMICS INTERNATIONAL, 2019, 45 (13) : 16046 - 16053
  • [47] High-temperature oxidation resistance behavior and mechanism of HfSiO 4-modified C/SiC composites
    Qiu, Jintao
    Yang, Huiyong
    Huang, Juntong
    Wang, Lianyi
    Luo, Ruiying
    Chen, Zhi
    Li, Wei
    Deng, Chengmou
    Li, Wenpeng
    Zhang, Jinxuan
    Tao, Zejian
    Zhong, Shujun
    Teng, Wenhao
    CERAMICS INTERNATIONAL, 2024, 50 (12) : 21755 - 21766
  • [48] Oxidation resistant Si-Mo-Al coating for C/SiC coated carbon/carbon composites at high temperature
    Zhang, Y. -L.
    Li, H. -J.
    Yao, X. -Y.
    Li, K. -Z.
    Qiang, X. -F.
    SURFACE ENGINEERING, 2012, 28 (04) : 257 - 260
  • [49] Microstructural characterizations of γ-TiAl alloy after high-temperature steam oxidations at 900, 1000, 1100 and 1200 °C
    Xu, Chi
    Zhu, Minghao
    Gao, Chuanli
    Guan, Haohao
    Wang, Xingping
    Jin, Xiaoyue
    Du, Jiancheng
    Xue, Wenbin
    MATERIALS CHARACTERIZATION, 2022, 189
  • [50] Effect of molybdenum on the oxidation resistance of FeCrAl alloy in lower temperature (400 °C) and higher temperature (1200 °C) steam environments
    Qu, Haozheng J.
    Chikhalikar, Atharva S.
    Abouelella, Hamdy
    Roy, Indranil
    Rajendran, Rupesh
    Nagothi, Bhavani S.
    Umretiya, Rajnikant
    Hoffman, Andrew K.
    Rebak, Raul B.
    CORROSION SCIENCE, 2024, 229