Synergistic impact of lanthanum and cerium co-doping ZnO for improved photocatalytic rhodamine B degradation efficiency under UV light
被引:2
作者:
Slimani, Yassine
[1
]
Khan, Abuzar
[2
]
Sivakumar, R.
[3
]
Nawaz, Muhammad
[4
]
Thakur, Atul
[5
]
机构:
[1] Imam Abdulrahman Bin Faisal Univ, Inst Res & Med Consultat IRMC, Dept Biophys, POB 1982, Dammam 31441, Saudi Arabia
[2] King Fahd Univ Petr & Minerals, Interdisciplinary Res Ctr Hydrogen Technol & Carbo, Box 5040, Dhahran 31261, Saudi Arabia
[3] Alagappa Univ, Dept Phys, Karaikkudi 630003, India
[4] Imam Abdulrahman Bin Faisal Univ, Inst Res & Med Consultat IRMC, Dept Nanomed Res, POB 1982, Dammam 31441, Saudi Arabia
[5] Amity Univ Haryana, Ctr Nanotechnol, Gurugram 122413, India
关键词:
Photocatalyst;
Rhodamine B dye;
Defects;
Charge carriers' recombination;
Photocatalytic degradation efficiency;
DOPED ZNO;
ZINC-OXIDE;
PARTICLE-SIZE;
TIO2;
CE;
PHOTOLUMINESCENCE;
LUMINESCENCE;
REDUCTION;
ARRAYS;
DOPANT;
D O I:
10.1016/j.molstruc.2024.140366
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
In this study, the influence of different La and Ce co-doping amounts on the structural, morphological, optical, and photodegradation properties of ZnO nanostructures was evaluated. Zn1-2xLaxCexO nanoparticles (NPs) were prepared using sol-gel auto-ignition process, where x = 0.00 (pure ZnO), 0.01 (LC1), 0.03 (LC3), and 0.05 (LC5). The X-ray diffraction (XRD) and Raman results revealed that the prepared ZnO NPs crystallize in the hexagonal wurtzite structure. The size of crystallites is affected by the increment of La and Ce and it decreased from 24.29 nm to 10.40 nm with the increase in the concentration of La and Ce. Transmission electron microscopy (TEM) showed that the samples exhibit an irregular distribution of NPs with a dominant spherical shape morphology. The simultaneous incorporation of La and Ce in ZnO NPs led to a slight variation in the absorption edge and a slight shift in the values of the band gap energy from 3.20 to 3.24 eV. Furthermore, a reduction in the recombination rate of photogenerated charge carriers and the creation of fewer additional defects upon the appropriate insertion of Ce and La ions are highlighted by the analysis of photoluminescence spectra, Nyquist plots, and transient photocurrent measurements. The photocatalytic activity of samples was evaluated against rhodamine B organic dye under UV light irradiation. The analysis showed that LC1 sample exhibited superior photocatalytic performance with 99.1 % degradation efficiency and a degradation rate constant of 0.0762 min(-1). This enhancement has been ascribed to the surface defects and the optimized crystallite size achieved, which help to generate reactive entities such as center dot OH and O-2(center dot-) in addition to the great role of holes (h(+)) and impede the recombination of charge carriers e(-)/h(+).