Transient Liquid-Phase Bonding Using Sn/Ni/Sn Laminated Metal Preform for Power Device Packaging

被引:0
|
作者
Lee, Dong-Bok [1 ]
Seo, Young-Jin [1 ]
Yoon, Jeong-Won [1 ]
机构
[1] Chungbuk Natl Univ, Dept Adv Mat Engn, 1 Chungdae Ro, Cheongju 28644, Chungbuk, South Korea
基金
新加坡国家研究基金会;
关键词
Intermetallic compounds; soldering; electronic packaging; thermo-compression bonding; microstructure; laminated metal preform; SOLDER; MICROSTRUCTURE; EVOLUTION;
D O I
10.1007/s11664-025-11738-5
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Intermetallic compound (IMC) joints formed via transient liquid-phase (TLP) bonding offer excellent high-temperature durability. However, IMC formation at the joint requires long bonding times and high pressures. In this study, to reduce the bonding time and pressure required for IMC formation, a Sn/Ni/Sn laminated metal preform was fabricated by inserting Ni foil between Sn foils, and this material was used to bond a chip to a substrate. The microstructure of the joint cross-section was analyzed using field-emission scanning electron microscopy and energy-dispersive x-ray spectroscopy. The Sn foil was completely converted to 7 mu m Ni3Sn4 within 15 min, forming a stable TLP-bonded joint. After bonding, a shear test was conducted to evaluate the mechanical properties of the joints, which revealed high shear strength, exceeding 46 MPa.
引用
收藏
页码:1592 / 1601
页数:10
相关论文
共 50 条
  • [41] Au-Sn Transient Liquid Phase Bonding for Hermetic Sealing and Getter Activation
    Giudice, S.
    Bosshard, Ch.
    2013 EUROPEAN MICROELECTRONICS PACKAGING CONFERENCE (EMPC), 2013,
  • [42] The bonding time effects on the transient liquid phase bonding of Inconel 718 using nickel-based sintered brazing preform
    Yan, Guangxu
    Bhowmik, Ayan
    Nagarajan, Balasubramanian
    Song, Xu
    Tan, Sung Chyn
    Tan, Ming Jen
    APPLIED SURFACE SCIENCE, 2019, 495
  • [43] Alteration of Cu3Sn growth and retention of multi-orientation Cu6Sn5 during thermal aging in Cu-xNi-yZn/Sn3.5Ag/Cu transient liquid-phase bonding
    Wu, Zih-You
    Lee, Yin-Ku
    Tsai, Su-Yueh
    Chen, Po-Yu
    Duh, Jenq-Gong
    MATERIALS CHARACTERIZATION, 2024, 207
  • [44] Fabrication of Sn-plated Cu foam for high-efficiency transient-liquid-phase bonding
    Liu, Jiaxin
    Lei, Zhenyu
    Wang, Qing
    Mou, Yun
    Chen, Mingxiang
    MATERIALS TODAY COMMUNICATIONS, 2022, 30
  • [45] Microstructure Characteristics of Transient Liquid Phase Diffusion Bonding Super-Ni/NiCr Laminated Composite to TC4 Alloy
    Xu Xiaohan
    Li Yajiang
    Liu Kun
    Wang Juan
    SCIENCE OF ADVANCED MATERIALS, 2019, 11 (09) : 1252 - 1258
  • [46] Microstructure and mechanical properties of Cu/Sn-In/Cu joints obtained by ultrasonic-assisted transient liquid phase bonding in air
    Bi, Yan
    Nie, Yong
    Wang, Qian
    Han, Jian
    Cai, Yangchuan
    ADVANCES IN MECHANICAL ENGINEERING, 2020, 12 (10)
  • [47] Microstructure, interfacial reactions and mechanical properties of Co/Sn/Co and Cu/Sn/Cu joints produced by transient liquid phase bonding
    Tian, Shuang
    Zhou, Jian
    Xue, Feng
    Cao, Ruihua
    Wang, Fengjiang
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2018, 29 (19) : 16388 - 16400
  • [48] TRANSIENT LIQUID-PHASE BONDING FOR NI-BASE SUPERALLOYS, MAR-M247 AND IN939
    NAKAHASHI, M
    SUENAGA, S
    SHIROKANE, M
    TAKEDA, H
    MATERIALS TRANSACTIONS JIM, 1992, 33 (01): : 60 - 65
  • [49] Transient liquid phase bonding of Ni3Al based superalloy using Mn-Ni-Cr filler
    Yuan, Lin
    Ren, Jin
    Xiong, Jiangtao
    Zhao, Wei
    Shi, Junmiao
    Li, Jinglong
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 11 : 1583 - 1593
  • [50] Growth kinetics of interfacial intermetallic layer of In-48Sn/Cu solder joint by transient liquid phase bonding
    Zhang, Yaocheng
    Liu, Zheng
    Meng, Tao
    Lu, Kaijian
    Yang, Li
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2025, 36 (02)