Effect of Pouring and Preheating Temperature on Shrinkage Cavity and Porosity Defects of Nickel-Based Cast Superalloy

被引:0
|
作者
Zhao, Long [1 ,2 ]
Liu, Zhongqiu [1 ,2 ]
Zhang, Yingqi [2 ]
Zhang, Long [3 ]
Ma, Yingche [3 ]
Li, Baokuan [2 ]
机构
[1] Northeastern Univ, Key Lab Ecol Met Multimet Mineral, Minist Educ, Shenyang 110819, Peoples R China
[2] Northeastern Univ, Sch Met, Shenyang 110819, Peoples R China
[3] Chinese Acad Sci, Inst Met Res, Shenyang 110016, Peoples R China
来源
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE | 2025年
基金
中国国家自然科学基金;
关键词
SOLIDIFICATION; PREDICTION; PRESSURE; GAS;
D O I
10.1007/s11663-024-03420-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A three-dimensional flow-heat transfer-solidification coupled model was developed based on the finite element method to simulate the shrinkage cavity and porosity defects of a novel nickel-based cast superalloy K4800. The influence of pouring and preheating temperatures on shrinkage volume, Niyama value at the solidification front, temperature gradient, and cooling rate were investigated. Wire cutting experiments on ingots obtained by casting in molds made of 45-gage steel, which were then polished to capture images of shrinkage and shrinkage defects within them. By comparing the simulation results with this image, we found that the model has high accuracy, and the critical value of the Niyama criterion is determined to be 33.75 ( degrees C<middle dot>s)1/2/cm. The results indicate that the temperature gradient exerts a significantly greater influence than the cooling rate within the Niyama criterion. The effect of pouring temperature on the Niyama value is concentrated in the part of the ingot above 87 cm, and the effect of preheating temperature is negligible. Increasing the pouring temperature from 1400 degrees C to 1500 degrees C dramatically reduces shrinkage cavity volume, reaching its minimum at 1500 degrees C. The effect of preheating temperature on shrinkage cavity volume is significantly less compared to pouring temperature. The shrinkage cavity volume decreases only slightly with increasing preheating temperature, and its effect can be disregarded when pouring temperature is high. The comparison of shrinkage cavity volume values under different process parameters reveals that the volume is minimized at a pouring temperature of 1500 degrees C and a preheating temperature of 35 degrees C.
引用
收藏
页码:1316 / 1333
页数:18
相关论文
共 44 条
  • [21] Effect of micron-scale nonmetallic inclusions on fatigue crack nucleation in a nickel-based superalloy
    Liu, Pengfei
    Jiang, He
    Dong, Jianxin
    Chen, Zhanghua
    INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 2023, 279
  • [22] Effect of deposition temperature on morphology and properties of nickel-based composite coatings
    Liu, Heng
    Zhang, Chenming
    Qiu, Yun
    Aday, Xieeryazidan
    Wei, Yanxiang
    BULLETIN OF MATERIALS SCIENCE, 2025, 48 (01)
  • [23] Effect of cellular recrystallization on tensile properties of a nickel-based single crystal superalloy containing Re and Ru
    Shi, Zhen-xue
    Liu, Shi-zhong
    Yue, Xiao-dai
    Hu, Li-jie
    Yang, Wan-peng
    Wang, Xiao-guang
    Li, Jia-rong
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2017, 24 (10) : 1059 - 1064
  • [24] Judgment criterion of the dominant factor of creep-fatigue crack growth in a nickel-based superalloy at elevated temperature
    Zhang, Meng
    Zhang, Yongxiang
    Liu, Hao
    Zou, Quanle
    INTERNATIONAL JOURNAL OF FATIGUE, 2019, 118 : 176 - 184
  • [25] Experimental and numerical investigation of mixed-mode fatigue crack growth in nickel-based superalloy at high temperature
    Xie, Qikun
    Qi, Hongyu
    Li, Shaolin
    Yang, Xiaoguang
    Shi, Duoqi
    ENGINEERING FRACTURE MECHANICS, 2022, 273
  • [26] Effect of diffusion heat treatment on microstructure and mechanical properties of a boron-containing nickel-based superalloy
    Yu, Xingfu
    Hu, Chenyang
    Liu, Hongxiu
    Liu, Weijun
    Liu, Fang
    Sun, Wenrun
    Su, Yong
    JOURNAL OF MATERIALS SCIENCE, 2022, 57 (16) : 7965 - 7979
  • [27] Effect of Orientation Deviation on Microstructure and Mechanical Properties of Nickel-Based Single Crystal Superalloy Brazing Joints
    Zhao Xu
    Sun Yuan
    Hou Xingyu
    Zhang Hongyu
    Zhou Yizhou
    Ding Yutian
    ACTA METALLURGICA SINICA, 2020, 56 (02) : 171 - 181
  • [28] Accelerating homogenization kinetics and enhancing hot-workability of as-cast nickel-based superalloy via prior hot-deformation
    Chen, Jia-jun
    Zhou, Yang
    Han, Hao-ran
    Zhang, Xian-guang
    Miyamoto, Goro
    Tang, Ping-mei
    Xiao, Dong-ping
    Fu, Jian-hui
    Shi, Peng
    Pei, Yi-wu
    Zhang, Jian
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2025, 32 (01) : 215 - 226
  • [29] A Two-Stage Constitutive Model and Microstructure Evolution Simulation of a Nickel-Based Superalloy during High Temperature Deformation
    Zhu, Qiang
    Chen, Linjun
    Chen, Gang
    Wang, Chuanjie
    Qin, Heyong
    Zhang, Peng
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (08) : 3378 - 3389
  • [30] Effect of inclusions on low cycle fatigue lifetime in a powder metallurgy nickel-based superalloy FGH96
    Hu, Dianyin
    Wang, Tao
    Ma, Qihang
    Liu, Xi
    Shang, Lihong
    Li, Da
    Pan, Jinchao
    Wang, Rongqiao
    INTERNATIONAL JOURNAL OF FATIGUE, 2019, 118 : 237 - 248