Damage evolution and failure behavior of 3D needled Carbon/Carbon composites under compressive at ultra-high temperatures up to 2800 °C

被引:0
作者
Wang, Kunjie [1 ]
Xu, Chenghai [1 ]
Gao, Bo [1 ]
Zhao, Xinliang [1 ]
Wang, Boyi [1 ]
Meng, Songhe [1 ]
机构
[1] Harbin Inst Technol, Ctr Composite Mat & Struct, Sci & Technol Adv Composites Special Environm Lab, Harbin 150080, Peoples R China
基金
中国国家自然科学基金;
关键词
3D needled Carbon/Carbon composite; Ultra-high temperature; Compressive property; Fracture behavior; C/C COMPOSITES; CARBON-FIBERS; THERMAL-EXPANSION; MECHANICAL-PROPERTIES; TENSILE; STRENGTH; SHEAR; STRESS;
D O I
10.1016/j.jeurceramsoc.2025.117183
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this paper, the compressive properties of 3D needled Carbon/Carbon composites at high temperatures up to 2800 degrees C were revealed from the perspective of damage evolution and fracture behavior. At ambient temperature, the results of loading-unloading and in-situ X-ray computed tomography experiments show that cracks originate from the needle-punched region on the surface when the strain threshold exceeds 0.3 %. With further loading, the material exhibits nonlinear and cumulative damage characteristics. At ultra-high temperature, the compressive strength increases first and then decreases with the increase of temperature, and reaches the maximum at 1800 degrees C. Meanwhile, the fracture mechanism of temperature control is divided into two categories. Below 2400 degrees C, the bonding of the interface improves with the increase of temperature, and the shear bands and delamination lead to catastrophic failure. At higher temperatures, the material exhibits plastic buckling, accompanied by fiber breakage, fiber kink bands, transverse cracks and delamination.
引用
收藏
页数:9
相关论文
共 49 条
[41]   Experimental study of ultra-high temperature interlaminar tensile strengths of 3D-needled C/C composites using the V-shaped notched specimen compression method [J].
Xu Chenghai ;
Han Xinxing ;
Cheng Guangyi ;
Meng Songhe ;
Jin Hua .
MECHANICS OF MATERIALS, 2018, 126 :26-35
[42]   In situ characterization of the flexural behavior and failure mechanism of 2D needle-punched carbon/carbon composites by digital image correlation [J].
Xu, Hao ;
Li, Lu ;
Li, Guodong ;
Zheng, Ruixiao ;
Yao, Xiyuan ;
Ma, Chaoli .
JOURNAL OF MATERIALS SCIENCE, 2022, 57 (24) :11077-11091
[43]   Failure and strength of 2D-C/SiC composite under in-plane shear loading at elevated temperatures [J].
Yan, K. F. ;
Zhang, C. Y. ;
Qiao, S. R. ;
Li, M. ;
Han, D. .
MATERIALS & DESIGN, 2011, 32 (06) :3504-3508
[44]   In-plane shear strength of a carbon/carbon composite at different loading rates and temperatures [J].
Yan, K. F. ;
Zhang, C. Y. ;
Qiao, S. R. ;
Han, D. ;
Li, M. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (03) :1458-1462
[45]   Novel uncured epoxy resin/CaCO3 nanocomposites [J].
Yu, Haojie ;
Wang, Li ;
Shi, Quan ;
Zhao, Zhenrong ;
Jiang, Guohua .
POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, 2006, 45 (07) :809-813
[46]   Theoretical prediction of temperature-dependent fracture strength for ultra-high temperature ceramic composites considering the evolution of damage and thermal residual stress [J].
Zhang, Xin ;
Li, Weiguo ;
Deng, Yong ;
Shao, Jiaxing ;
Zhang, Xuyao ;
Zhang, Xianhe ;
Kou, Haibo ;
Tao, Yong ;
Qu, Zhaoliang .
CERAMICS INTERNATIONAL, 2018, 44 (18) :22656-22663
[47]   Comparison on failure behavior of three-dimensional woven carbon/carbon composites joints subjected to out-of-plane loading at room and high temperature [J].
Zhang, Yanfeng ;
Zhou, Zhengong ;
Pan, Shidong ;
Tan, Zhiyong .
COMPOSITES COMMUNICATIONS, 2021, 23
[48]   Fracture characteristics and in-situ damage mechanism of PIP-C/SiC composites to various temperatures and loading velocities [J].
Zhao, Guicheng ;
Jiang, Zhonghe ;
Qu, Zhaoliang ;
Xi, Huifeng ;
Ai, Shigang .
ENGINEERING FRACTURE MECHANICS, 2023, 286
[49]   Microstructure evolution and oxidation mechanism of HfB2-SiC coating on SiC-coated C/C composites at 1173 K and 1773 K [J].
Zhu, Xiaofei ;
Zhang, Yulei ;
Zhang, Jian ;
Li, Tao ;
Zhang, Pei ;
Chen, Ruicong .
CERAMICS INTERNATIONAL, 2022, 48 (20) :30807-30816