Joint Interface Characteristics and Phase Transformations in Laser Brazed Steel

被引:0
作者
Zhao, Xiaoye [1 ]
Yang, Hanwen [1 ]
Lopes, J. G. [2 ,3 ]
Oliveira, J. P. [2 ,3 ]
Gerlich, Adrian [1 ]
Zhou, Y. Norman [1 ]
机构
[1] Univ Waterloo, Ctr Adv Mat Joining, Dept Mech & Mechatron Engn, 200 Univ Ave West, Waterloo, ON N2L 3G1, Canada
[2] Univ Nova Lisboa, NOVA Sch Sci & Technol, Dept Mech & Ind Engn, UNIDEMI, P-2829516 Caparica, Portugal
[3] Univ NOVA Lisboa, NOVA Sch Sci & Technol, Dept Mat Sci, CENIMAT I3N, P-2829516 Caparica, Portugal
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2025年 / 56卷 / 04期
基金
加拿大自然科学与工程研究理事会;
关键词
HEAT-AFFECTED ZONE; CU-SI; SOLIDIFICATION; GEOMETRY; INDUSTRY; METALS; ALLOYS; ARC;
D O I
10.1007/s11661-025-07708-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Zn-coated steel was laser brazed in a flare V-groove configuration, and the interfacial joining microstructure and solidification pathway were investigated for different wire feed rates (WFRs) with the assistance of thermodynamic calculations. Thermodynamic calculations indicate that Si atoms diffuse toward the steel substrate and this Si-enrichment layer along the steel/bead interface further promoted the formation of an alpha-Fe(Si) reaction layer, which was thin (similar to 1.9 to 2.9 mu m) and uniform at the laser direct irradiation region, and thick at the molten-Fe-enrichment region. Multiple phases are formed in the joint with a precipitation sequence involving alpha-Fe/alpha-Fe(Si), Cu and other phases (FeSi, Cu56Si11, Mn5Si3) in the braze bead. More molten Fe was stirred into the bead for the laser brazed joint when a low WFR of 3.5 m/min is applied and an Fe-based liquid phase appeared in addition to the Cu-based liquid according to the Scheil-Gulliver calculation results. The alpha-Fe/alpha-Fe(Si) phase was first precipitated from the Fe-based liquid at 1227 degrees C and then precipitated from the Cu-based liquid during the solidification process. However, when applying a WFR of 5 m/min, the alpha-Fe/alpha-Fe(Si) phase was directly precipitated from the Cu-based liquid at 1051 degrees C. As a results of these differences in phase types and content of precipitates within the bead, the microhardness of the bead decreased with WFR, reaching average values of 143 +/- 2.5 and 117 +/- 2.3 HV at WFRs of 3.5 and 5 m/min, respectively.
引用
收藏
页码:1310 / 1326
页数:17
相关论文
共 50 条
  • [41] Laser-induced infrared characteristic analysis for evaluating joint deviation during austenitic stainless steel laser welding
    Gao, Xiangdong
    Liu, Yingying
    Lan, Chongzhou
    Xiao, Zhenlin
    Chen, Xiaohui
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2017, 88 (5-8) : 1877 - 1888
  • [42] Characteristics of hot cracking in dissimilar joint of A690 overlay and stainless steel clad
    Ko, Gyoungback
    Seo, Kang Myung
    Kim, Hee Jin
    Hong, Hyunuk
    WELDING IN THE WORLD, 2017, 61 (05) : 945 - 953
  • [43] Yb: YAG laser welding of dual phase steel to aluminium alloy
    Indhu, R.
    Soundarapandian, S.
    Vijayaraghavan, L.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2018, 262 : 411 - 421
  • [44] The role of metallurgical solid state phase transformations on the formation of residual stress in laser cladding and heating
    Cottam, R.
    Luzin, V.
    Thorogood, K.
    Wong, Y. C.
    Brandt, M.
    MECHANICAL STRESS EVALUATION BY NEUTRONS AND SYNCHROTRON RADIATION VII, 2014, 777 : 19 - +
  • [45] Interface Formation and Bonding Mechanisms of Laser Welding of PMMA Plastic and 304 Austenitic Stainless Steel
    Huang, Yijie
    Gao, Xiangdong
    Ma, Bo
    Zhang, Yanxi
    METALS, 2021, 11 (09)
  • [46] THE INFLUENCE OF THE KINETICS OF PHASE TRANSFORMATIONS DURING TEMPERING ON THE MICROSTRUCTURE DEVELOPMENT IN TOOL STEEL WITH DIFFERENT CARBON CONTENT
    Bala, Piotr
    METAL 2013: 22ND INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2013, : 689 - 694
  • [47] A comparison of dilatometry and in-situ neutron diffraction in tracking bulk phase transformations in a martensitic stainless steel
    Christien, F.
    Telling, M. T. F.
    Knight, K. S.
    MATERIALS CHARACTERIZATION, 2013, 82 : 50 - 57
  • [48] Effect of parameters on interface of the brazed ZrO2 ceramic and Ti-6Al-4V joint using Ti-based amorphous filler
    Liu, Yuhua
    Hu, Jiandong
    Zhang, Yaping
    Guo, Zuoxing
    Yang, Yue
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2012, 25 (02) : 89 - 94
  • [49] Effect of laser spot offset on microstructure and properties of laser welded joint of medium Mn/DP980 dissimilar steel
    Liu, Hongning
    Wang, Yanjun
    Zhang, Jiazhi
    Zhu, Zhengqiang
    Yang, Shanglu
    MATERIALS LETTERS, 2024, 363
  • [50] Laser beam welding of dual-phase DP1000 steel
    Alves, P. H. O. M.
    Lima, M. S. F.
    Raabe, D.
    Sandim, H. R. Z.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2018, 252 : 498 - 510