Investigating Hot corrosion, CMAS, and Thermal Shock Behaviour of Double-layer YSZ/La2Ce2O7 + YSZ Thermal Barrier Coatings

被引:4
作者
Pakseresht, Amirhossein [1 ]
Ariharan, S. [1 ,2 ]
Sekar, Anusha [1 ]
Parchoviansky, Milan [1 ]
机构
[1] Alexander Dubcek Univ Trencin, Ctr Funct & Surface Functionalized Glass, Trencin 91150, Slovakia
[2] Vikram Sarabhai Space Ctr, Mat & Mech Ent, Thiruvananthapuram, Kerala, India
基金
欧盟地平线“2020”;
关键词
CMAS corrosion; hot corrosion; TBCs; thermal shock resistance; ALUMINO-SILICATE CMAS; BARRIER COATINGS; FAILURE; TEMPERATURE; ZIRCONIA; POWDER; DELAMINATION; MULTILAYER; MECHANISM; SUBJECT;
D O I
10.1007/s11666-024-01845-w
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this work, new double-layer YSZ/La2Ce2O7 (LC) + YSZ coatings were developed using air plasma spraying (APS). The surface of the prepared coatings was relatively smooth and consisted of melted and partially melted areas. Their resistance to hot corrosion, CaO-MgO-Al2O3-SiO2 (CMAS), and thermal shock were examined. YSZ was added to the upper layer to enhance the lanthanum cerate (La2Ce2O7, LC) properties. During the hot corrosion tests, the corrosion salt reacted with the upper layer, and the CeO2 phase and new corrosion products were identified. The main phase was LaVO4, and the secondary phases were CeVO4 and YVO4. SEM confirmed the formation of new, cuboidal-shaped corrosion products. The infiltration of CMAS led to the formation of additional new products: Ca(4)MgxAl(4)Si(6-x-gamma)O-14 and Ca-2.8(LaxCe1-x).(6)(SiO4)O6-4x. SEM revealed CMAS infiltration through the upper layer in the form of islands. Following the thermal shock resistance tests, the upper layer gradually peeled off, and the coating survived 67 cycles. Possible failure mechanisms were identified, and failure was attributed to the spallation of the upper layer from the surface layer by layer. After all tests, the top layer showed partial spalling and delamination. This was mainly caused by the reaction of corrosive salt or CMAS with the top layer, which changed its composition, leading to the formation and propagation of cracks and, ultimately, the separation of part of the upper layer. Peeling of the upper layer through mainly horizontal cracks was observed after hot corrosion, CMAS and thermal shocks. The NiCrAlY bond coat and YSZ interlayer remained undamaged.
引用
收藏
页码:809 / 822
页数:14
相关论文
共 50 条
  • [31] Improving CMAS-corrosion resistance of YSZ-based thermal barrier coatings with Al2O3 addition
    Han, Jiasen
    Zou, Yong
    Wu, Dongting
    Chen, Ji
    Zhang, Yongang
    SURFACE & COATINGS TECHNOLOGY, 2022, 446
  • [32] Improved hot corrosion resistance of plasma sprayed YSZ/Gd2Zr2O7 thermal barrier coating over single layer YSZ
    Lashmi, P. G.
    Majithia, Sumil
    Shwetha, V.
    Balaji, N.
    Aruna, S. T.
    MATERIALS CHARACTERIZATION, 2019, 147 : 199 - 206
  • [33] Hot corrosion performance and electrochemical study of CoNiCrAlY/YSZ/YSZ-La2O3 multilayer thermal barrier coatings in the presence of molten salt
    Khajezadeh, Mohammad Hossein
    Mohammadi, Majid
    Ghatee, Mojtaba
    MATERIALS CHEMISTRY AND PHYSICS, 2018, 220 : 23 - 34
  • [34] Enhanced CMAS and hot corrosion degradation of YSZ thermal barrier coating with nano powders
    Ozcelik, Abdulkadir
    Eker, Aysegul Akdogan
    Karabas, Muhammet
    Avci, Ali
    Kucukyildirim, Bedri Onur
    SURFACE & COATINGS TECHNOLOGY, 2024, 481
  • [35] Oxidation Behavior of the Monolayered La2Zr2O7, Composite La2Zr2O7+8YSZ, and Double-Ceramic Layered La2Zr2O7/La2Zr2O7+8YSZ/8YSZ Thermal Barrier Coatings
    Jasik, Anna
    Moskal, Grzegorz
    Mikuskiewicz, Marta
    Tomaszewska, Agnieszka
    Jucha, Sebastian
    Migas, Damian
    Myalska, Hanna
    MATERIALS, 2020, 13 (14)
  • [36] Hot corrosion behavior of YSZ, Gd2Zr2O7 and YSZ/Gd2Zr2O7 thermal barrier coatings exposed to molten sulfate and vanadate salt
    Ozgurluk, Yasin
    Doleker, Kadir Mert
    Karaoglanli, Abdullah Cahit
    APPLIED SURFACE SCIENCE, 2018, 438 : 96 - 113
  • [37] Degradation of YSZ thermal barrier coatings by CMAS and CMAS-Na2SO4 between 1250°C and 1350°C
    Dou, Mengfan
    Gao, Wei
    Xue, Ting
    Wu, Dongting
    Zou, Yong
    Zhang, Yongang
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2025, 45 (11)
  • [38] Hot Corrosion Behavior of YSZ Thermal Barrier Coatings Modified by Laser Remelting and Al Deposition
    Zhang, Panpan
    Zhang, Xiaofeng
    Li, Fuhai
    Zhang, Zhihui
    Wang, Yueliang
    Li, Hong
    Ren, Luquan
    Liu, Min
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2019, 28 (06) : 1225 - 1238
  • [39] Design, Preparation, and Characterization of Graded YSZ/La2Zr2O7 Thermal Barrier Coatings
    Chen, Hongfei
    Liu, Yun
    Gao, Yanfeng
    Tao, Shunyan
    Luo, Hongjie
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2010, 93 (06) : 1732 - 1740
  • [40] Thermal shock resistance of double-layer thermal barrier coatings
    Feng, Yang
    Dong, Tian-shun
    Fu, Bin-guo
    Li, Guo-lu
    Liu, Qi
    Wang, Ran
    JOURNAL OF MATERIALS RESEARCH, 2020, 35 (20) : 2808 - 2816