Investigating Hot corrosion, CMAS, and Thermal Shock Behaviour of Double-layer YSZ/La2Ce2O7 + YSZ Thermal Barrier Coatings

被引:4
作者
Pakseresht, Amirhossein [1 ]
Ariharan, S. [1 ,2 ]
Sekar, Anusha [1 ]
Parchoviansky, Milan [1 ]
机构
[1] Alexander Dubcek Univ Trencin, Ctr Funct & Surface Functionalized Glass, Trencin 91150, Slovakia
[2] Vikram Sarabhai Space Ctr, Mat & Mech Ent, Thiruvananthapuram, Kerala, India
基金
欧盟地平线“2020”;
关键词
CMAS corrosion; hot corrosion; TBCs; thermal shock resistance; ALUMINO-SILICATE CMAS; BARRIER COATINGS; FAILURE; TEMPERATURE; ZIRCONIA; POWDER; DELAMINATION; MULTILAYER; MECHANISM; SUBJECT;
D O I
10.1007/s11666-024-01845-w
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this work, new double-layer YSZ/La2Ce2O7 (LC) + YSZ coatings were developed using air plasma spraying (APS). The surface of the prepared coatings was relatively smooth and consisted of melted and partially melted areas. Their resistance to hot corrosion, CaO-MgO-Al2O3-SiO2 (CMAS), and thermal shock were examined. YSZ was added to the upper layer to enhance the lanthanum cerate (La2Ce2O7, LC) properties. During the hot corrosion tests, the corrosion salt reacted with the upper layer, and the CeO2 phase and new corrosion products were identified. The main phase was LaVO4, and the secondary phases were CeVO4 and YVO4. SEM confirmed the formation of new, cuboidal-shaped corrosion products. The infiltration of CMAS led to the formation of additional new products: Ca(4)MgxAl(4)Si(6-x-gamma)O-14 and Ca-2.8(LaxCe1-x).(6)(SiO4)O6-4x. SEM revealed CMAS infiltration through the upper layer in the form of islands. Following the thermal shock resistance tests, the upper layer gradually peeled off, and the coating survived 67 cycles. Possible failure mechanisms were identified, and failure was attributed to the spallation of the upper layer from the surface layer by layer. After all tests, the top layer showed partial spalling and delamination. This was mainly caused by the reaction of corrosive salt or CMAS with the top layer, which changed its composition, leading to the formation and propagation of cracks and, ultimately, the separation of part of the upper layer. Peeling of the upper layer through mainly horizontal cracks was observed after hot corrosion, CMAS and thermal shocks. The NiCrAlY bond coat and YSZ interlayer remained undamaged.
引用
收藏
页码:809 / 822
页数:14
相关论文
共 50 条
  • [21] Thermal shock behavior of 8YSZ and double-ceramic-layer La2Zr2O7/8YSZ thermal barrier coatings fabricated by atmospheric plasma spraying
    Wang, L.
    Wang, Y.
    Sun, X. G.
    He, J. Q.
    Pan, Z. Y.
    Wang, C. H.
    CERAMICS INTERNATIONAL, 2012, 38 (05) : 3595 - 3606
  • [22] Corrosion behaviour of La2Hf2O7 thermal barrier coatings against molten CMAS melts at 1300 and 1500 °C
    Wu, Yiming
    Zhong, Xin
    Hong, Du
    Liang, Ruihui
    Fan, Dong
    Wang, Lujie
    Niu, Yaran
    Zheng, Xuebin
    CERAMICS INTERNATIONAL, 2023, 49 (22) : 36724 - 36733
  • [23] CMAS corrosion resistance of YSZ thermal barrier coatings enhanced by Pt-Al films
    Wang, Jinshuang
    Lu, Xianjun
    Shu, Chaoxi
    Duan, Zhixing
    Dong, Shujuan
    Lu, Guoqiang
    Zhang, Yixing
    Yuan, Fuhe
    Cao, Xueqiang
    CERAMICS INTERNATIONAL, 2024, 50 (03) : 5111 - 5120
  • [24] CMAS corrosion behavior of Sc doped Gd2Zr2O7 /YSZ thermal barrier coatings and their corrosion resistance mechanisms
    Li, Bowen
    Sun, Jingyong
    Guo, Lei
    CORROSION SCIENCE, 2021, 193
  • [25] Preparation and Thermal Shock Resistance of Gd2O3 Doped La2Ce2O7 Thermal Barrier Coatings
    Gao, Lihua
    Jia, Fang
    Lu, Xiaoliang
    COATINGS, 2021, 11 (10)
  • [26] Hot corrosion behavior of Al2O3 laser clad plasma barrier coatings sprayed YSZ thermal barrier coatings
    Soleimanipour, Zohre
    Baghshahi, Saeid
    Shoja-razavi, Reza
    Salehi, Mehdi
    CERAMICS INTERNATIONAL, 2016, 42 (15) : 17698 - 17705
  • [27] Hot Corrosion Behavior of Plasma-Sprayed Gd2Zr2O7/YSZ Functionally Graded Thermal Barrier Coatings
    Manogaran, Rajasekaramoorthy
    Alagu, Karthikeyan
    Arul, Anderson
    Jesuraj, Anandh
    Devarajan, Dinesh Kumar
    Murugadoss, Govindhasamy
    Mosas, Kamalan Kirubaharan Amirtharaj
    CERAMICS-SWITZERLAND, 2024, 7 (02): : 579 - 595
  • [28] Thermal shock resistance of YSZ, YSZ-Al2O3 and YSZ-Al2O3/YSZ coatings
    Song, Xuemei
    Zhang, Jimei
    Liu, Ziwei
    Jiang, Caifen
    Lin, Chucheng
    Zeng, Yi
    VACUUM, 2019, 162 : 150 - 155
  • [29] Comparison of corrosion behaviors and wettability of CMAS on Ta2O5-Y2O3 co-stabilized ZrO2 and YSZ thermal barrier coatings
    Wang, Jinshuang
    Wang, Yinghui
    Lu, Xianjun
    Hu, Mengqiu
    Chen, Mengdi
    Shu, Chaoxi
    Zhang, Hao
    Tian, Yongshang
    Liu, Bing
    Jing, Qiangshan
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (13) : 5636 - 5651
  • [30] A comparative study on hot corrosion resistance of three types of thermal barrier coatings:: YSZ, YSZ + Al2O3 and YSZ/Al2O3
    Afrasiabi, Abbas
    Saremi, Mohsen
    Kobayashi, Akira
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 478 (1-2): : 264 - 269