Two methods for assessment of residual life of HK-40 furnace tubes

被引:0
|
作者
Shen, F.Z. [1 ]
Ma, G.X. [1 ]
Ling, X. [1 ]
Yang, X. [1 ]
Zhang, X.Z. [1 ]
Ruan, J. [1 ]
Lu, Y. [1 ]
机构
[1] Nanjing Univ of Chemical Technology, Nanjing, China
来源
关键词
Computer simulation - Cyclic loads - Furnaces - Petrochemical plants - Service life - Steel - Thermal cycling;
D O I
暂无
中图分类号
学科分类号
摘要
Two methods were used: one is test-analysis method that is mainly based on the creep rupture tests on postservice specimens. Specimens were taken from the tubes, which had been in service for different times. Kachanov-Robinson's damage summation concept was employed, however with a modified factor K(ts) to account for prior damage in the specimens. If the foregone total life corresponds with real condition, all of the test data modified by K (ts) should be distributed uniformly nearby the master curve of the new material. The other is computer simulation method that considers all of the operating conditions that influence the life. The finite element method with iterative calculation was used in the analysis. The variation rates of critical damage element along the wall thickness were determined as a function of the service temperature and current damage. A special program designed based on the method predicts well the residual life of furnace tubes, so long as the maximum depth of critical damage in radius direction of tubes has been detected by ultrasonic techniques.
引用
收藏
页码:105 / 112
相关论文
共 46 条
  • [1] TWO METHODS FOR ASSESSMENT OF RESIDUAL LIFE OF HK-40 FURNACE TUBES
    F.Z. Shen. G.X. Ma and X. Ling Nanjing University of Chemical Technology
    Acta Metallurgica Sinica(English Letters), 1999, (01) : 108 - 115
  • [2] Welding of HK-40 centripetal casting furnace tubes
    2001, Lanzhou Petroleum Machinery Research Institute (30):
  • [3] HOW TO REPAIR WELD HK-40 FURNACE TUBES
    VOELKER, CH
    ZEIS, LA
    HYDROCARBON PROCESSING, 1972, 51 (04): : 121 - &
  • [4] A STUDY OF CREEP CRACK-PROPAGATION OF HK-40 FURNACE TUBES WITH C-SHAPED SPECIMENS
    WANG, YL
    SHEN, FZ
    TU, ST
    ENGINEERING FRACTURE MECHANICS, 1994, 47 (01) : 39 - &
  • [5] ULTRASONIC INSPECTION OF CAST HK-40 TUBES FOR CREEP FISSURES
    DALTON, RR
    MATERIALS EVALUATION, 1974, 32 (12) : 264 - 268
  • [6] RADIOGRAPHIC INSPECTION OF CAST HK-40 TUBES FOR CREEP FISSURES .2.
    DALTON, RR
    MATERIALS EVALUATION, 1972, 30 (12) : 249 - &
  • [7] METHOD FOR ESTIMATING RESIDUAL CREEP LIVES OF CAST HK-40 REFORMER TUBINGS.
    Kasahara, Komei
    Tetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan, 1979, 65 (07): : 975 - 984
  • [8] Assessment of residual life for furnace tubes by an analogue computing method
    Shen, FZ
    Cai, RY
    Ma, GX
    Chen, K
    Liu, TS
    Yang, X
    CASE HISTORIES ON INTEGRITY AND FAILURES IN INDUSTRY, 1999, : 851 - 862
  • [9] PROPERTY DEGRADATION AND RESIDUAL LIFE ASSESSMENT OF SERVICE EXPOSED REFORMER TUBES
    Han, Zhiyuan
    Xie, Guoshan
    Cao, Luowei
    Wang, Likun
    Sun, Guohao
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, 2019, VOL 3, 2019,
  • [10] Life assessment of alloy 800H tubes in primary reformer furnace
    Shibasaki, T
    Takemura, K
    Mohri, T
    AMMONIA PLANT SAFETY & RELATED FACILITIES, VOL 37, 1997, 37 : 228 - 238