共 50 条
- [33] Interface and performance of CLAM steel/aluminum clad tube prepared by explosive bonding method The International Journal of Advanced Manufacturing Technology, 2016, 82 : 543 - 548
- [35] Design of flexible copper clad laminate with outstanding adhesion strength induced by chemical bonding Journal of Materials Science: Materials in Electronics, 2014, 25 : 5446 - 5451
- [36] Effect of Ni layer thickness on bonding strength of hot rolled clad steel plate Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2015, 36 (01): : 80 - 85
- [37] Effect of surface treatment on bonding strength of hot rolled steel aluminum clad plate 19TH INTERNATIONAL CONFERENCE ON METAL FORMING, MF 2022, 2022, 1270
- [38] DEVELOPMENT OF ROLLED TITANIUM CLAD STEEL .2. ROLLING CONDITION AND BONDING STRENGTH TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (13): : 1654 - 1654
- [40] Solid–liquid interdiffusion bonding of Cu/In/Ni microjoints Journal of Materials Science: Materials in Electronics, 2022, 33 : 18751 - 18757