STRESS CORROSION CRACKING OF 18 Ni MARAGING STEEL IN CHLORIDE SOLUTIONS.

被引:0
|
作者
Craig, I.H.
Parkins, R.N.
机构
来源
British Corrosion Journal | 1984年 / 19卷 / 01期
关键词
CORROSION; -; Testing;
D O I
暂无
中图分类号
学科分类号
摘要
A variety of techniques involving electrochemical, hydrogen permeation and acoustic emission measurements have been used in studying initially smooth and pre-cracked specimens. In solutions having pH's in excess of 2, cracking of smooth specimens occurred in two regimes of potential separated by a region in which cracking did not occur, although cracking was induced in this latter region if the specimens were precracked or pre-pitted, or pitting was facilitated by non-metallic inclusions emerging at the surfaces by stressing the specimens transversely to the rolling direction. The evidence does not support the hypothesis that failure invariably results from the ingress of hydrogen following the creation of acidic conditions within an initiating pit or pre-crack. Rather it supports crack growth by dissolution at high potentials, and a hydrogen induced process at low potential. This conclusion is supported by electrochemical measurements and the effects of additions of chloroplatinic acid, sodium arsenate or thiourea to the chloride solutions, with or without applied polarization. Hydrogen permeation measurements under conditions of cathodic polarization confirmed the effects of these additions upon the uptake of hydrogen but when permeation membranes were subjected to anodic polarization they were perforated by dissolution and the apparent hydrogen permeation was due to the passage of solution through the membrane. Further support for hydrogen induced cracking dominating at lower potentials and dissolution being controlling at higher potentials was derived from acoustic emission experiments, which showed emission to be enhanced by cathodic but not by anodic polarization as crack growth occurred.
引用
收藏
页码:3 / 16
相关论文
共 50 条
  • [41] Environmentally Assisted Cracking Behavior of 18Ni 250 Maraging Steel Welds Obtained with and Without Flux in Chloride Media
    Gupta, Renu N.
    Agrawal, Rahul K.
    Gore, Poorwa
    Parmar, Uday
    Raja, V. S.
    CORROSION, 2021, 77 (01) : 85 - 96
  • [42] Stress Corrosion Cracking and Localized Corrosion of Carbon Steel in Nitrate Solutions
    Sridhar, N.
    Beavers, J. A.
    Rollins, B.
    Chawla, S.
    Evans, K.
    Li, X.
    CORROSION, 2016, 72 (07) : 927 - 942
  • [43] CORROSION RESISTANCE OF 18 Cr-37 Ni AUSTENITIC STEEL IN ALKALINE, ACID AND NEUTRAL SOLUTIONS.
    Ahmad, Zaki
    Davami, Parviz
    1600, (29):
  • [44] STRESS CORROSION CRACKING OF AUSTENITIC STAINLESS STEELS IN CHLORIDE SOLUTIONS
    SHIMOSE, T
    TAKAMURA, A
    MORI, K
    SHIMOGOR.K
    TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1965, 6 (02): : 83 - &
  • [45] STRESS CORROSION CRACKING AND POTENTIAL DEPENDENCE OF SUS 304 STEEL SINGLE CRYSTALS IN MgCl2 SOLUTIONS.
    Uchida, Hitoshi
    Koterazawa, Keiji
    Oshiro, Hitoshi
    Yamada, Iwao
    Zairyo/Journal of the Society of Materials Science, Japan, 1986, 35 (396) : 1037 - 1042
  • [46] STRESS-CORROSION CRACKING OF FE-CR-NI STAINLESS-STEELS IN CHLORIDE SOLUTIONS
    TOMASHOV, ND
    PROTECTION OF METALS, 1981, 17 (04): : 334 - 338
  • [47] INFLUENCE OF CHLORIDE CONCENTRATION ON STRESS-CORROSION CRACKING OF AUSTENITIC STAINLESS-STEEL IN LICL SOLUTIONS
    SHAMAKIAN, RL
    TROIANO, AR
    HEHEMANN, RF
    CORROSION, 1980, 36 (06) : 279 - 284
  • [48] Probabilistic assessment for the stress corrosion cracking lifetime of sensitized 304 stainless steel in sodium chloride solutions
    Nakayama, Gen
    Akashi, Masatsune
    Ohtomo, Akira
    1600, (31):
  • [49] Chemical aspects of stress corrosion cracking of AISI 321 stainless steel in hot aqueous chloride solutions
    Schneider, F
    Mummert, K
    METALS MATERIALS AND PROCESSES, 1996, 8 (03): : 229 - 238
  • [50] THEORY OF STRESS CORROSION CRACKING OF MILD STEEL IN NITRATE SOLUTIONS
    WABER, JT
    MCDONALD, HJ
    LONGTIN, B
    TRANSACTIONS OF THE ELECTROCHEMICAL SOCIETY, 1945, 87 : 209 - 236