共 50 条
- [1] TENSILE AND IMPACT PROPERTIES OF 25MN-5CR-1NI AUSTENITIC STEEL AT LIQUID HELIUM TEMPERATURE. 1982, V 22 (N 8): : 577 - 585
- [4] HIGH TEMPERATURE TENSILE PROPERTIES OF NEUTRON IRRADIATED 20 CR-35 NI AUSTENITIC STEEL ZEITSCHRIFT FUR METALLKUNDE, 1967, 58 (04): : 258 - &
- [5] CLEAVAGE-LIKE FRACTURE ALONG SLIP PLANES IN Fe-18Cr-3Ni-13Mn-0. 37N AUSTENITIC STAINLESS STEEL AT LIQUID HELIUM TEMPERATURE. Metallurgical transactions. A, Physical metallurgy and materials science, 1988, 19 A (06): : 1626 - 1631
- [6] INFLUENCE OF MOLYBDENUM ON PROPERTIES OF AUSTENITIC CR-MN-NI-AL STEEL RUSSIAN METALLURGY-METALLY-USSR, 1971, (04): : 131 - &
- [8] Effect of Tensile Deformation on Austenitic Cr – Ni-Steel Structure and Magnetic Properties Metal Science and Heat Treatment, 2013, 55 : 328 - 334