EFFECT OF HEAT AND CHEMICOTHERMAL TREATMENT ON THE PROPERTIES OF POWDER HARD ALLOYS.

被引:0
|
作者
Pirso, Yu.Yu. [1 ]
Kyubarsepp, Ya.P. [1 ]
机构
[1] Tallin Polytechnic Inst, USSR, Tallin Polytechnic Inst, USSR
关键词
CHROMIUM COMPOUNDS - Heat Treatment - HEAT TREATMENT - Annealing - TITANIUM CARBIDE - Heat Treatment - WEAR OF MATERIALS;
D O I
暂无
中图分类号
学科分类号
摘要
A study was made of effect of different forms of heat and chemicothermal treatment on the strength in bending and hydroabrasive wear resistance of tungsten carbide (VK15), chromium carbide (KKhN25) and titanium carbide with a steel binder KTZhKh-50 (50% TiC plus 50% steel Kh15). The wear resistance may be increased by strengthening the binder phase. Bulk alloying of the binder to a considerable amount is not applicable as a result of its embrittlement and a reduction in strength. Phosphatizing is recommended in order to improve the wear resistance of chromium carbide and titanium carbide powder hard alloys.
引用
收藏
页码:211 / 213
相关论文
共 50 条
  • [1] EFFECT OF HEAT AND CHEMICOTHERMAL TREATMENT ON THE PROPERTIES OF POWDER HARD ALLOYS
    PIRSO, YY
    KYUBARSEPP, YP
    METAL SCIENCE AND HEAT TREATMENT, 1987, 29 (3-4) : 211 - 213
  • [2] HYDROABRASIVE WEAR OF HARD POWDER ALLOYS.
    Val'dma, L.E.
    Soviet Journal of Friction and Wear (English translation of Trenie i Iznos), 1984, 5 (05): : 74 - 78
  • [3] Effect of Welding, Heat Treatment, and Corrosion on the Properties of Nimonic Alloys.
    Galan, Paul
    Potakovskyj, Leo
    Schweisstechnik (Vienna), 1974, 28 (06): : 117 - 121
  • [4] Effect of Heat Treatment of the Charge Materials on the Properties of Aluminum-Silicon Alloys.
    Torshilova, S.I.
    Nikitin, V.I.
    Gulyaev, B.B.
    Krushenko, G.G.
    Izvestiya Vysshikh Uchebnykh Zavedenij. Tsvetnaya Metallurgiya, 1976, (04): : 126 - 128
  • [5] HEAT TREATMENT AND MAGNETIC PROPERTIES OF SOME ALNICO ALLOYS.
    Prakash, Ved
    Tewari, C.R.
    TISCO (Tata Iron and Steel Co), 1977, 24 (03): : 97 - 102
  • [6] EFFECT OF HEAT TREATMENT ON MECHANICAL PROPERTIES AND CHARACTER OF FAILURE OF SHEET MOLYBDENUM ALLOYS.
    Bukhanovskii, V.V.
    Kartyshov, N.G.
    Polishchuk, E.P.
    Kharchenko, V.K.
    Chikunov, M.I.
    Problemy Prochnosti, 1987, (08): : 53 - 57
  • [7] EFFECT OF THERMOMECHANICAL PROCESSING AND HEAT TREATMENT ON TENSILE AND CREEP PROPERTIES OF TITANIUM ALLOYS.
    Saha, R.L.
    Mukherji, D.
    Transactions of the Indian Institute of Metals, 1983, 37 (05): : 523 - 533
  • [8] Effect of the Heat-Treatment Regime on the Fatigue Properties of Internally Oxidized Silver Alloys.
    Vol'fson, T.Ya.
    Machul'skaya, G.A.
    Shpichinetskii, E.S.
    1600,
  • [9] EFFECT OF Ni ON THE MECHANICAL PROPERTIES OF Fe, Mo BORIDE HARD ALLOYS.
    Takagi, Kenichi
    Komai, Masao
    Ide, Tsuneyuki
    Watanabe, Tadao
    Kondo, Yoshikazu
    International Journal of Powder Metallurgy (Princeton, New Jersey), 1987, 23 (03): : 157 - 161
  • [10] EFFECT OF HEAT TREATMENT ON FERROMAGNETIC CRYSTALLINE ANISOTROPY OF PdCo ALLOYS.
    Miyata, Nahonori
    Hagiwara, Makoto
    Ichiyanagi, Yuko
    Kuwahara, Kuniaki
    Matsufuji, Hoji
    1600, (55):