Effect of N2+ ion implantation on the corrosion behavior of pure titanium

被引:0
|
作者
Kato, Masahiko [1 ]
Wang, Rongguang [2 ]
Nakasa, Keijiro [1 ]
机构
[1] Dept. of Mech. Eng., Hiroshima Univ., Higashi-Hiroshima, 739-8527, Japan
[2] Hiroshima Univ., Higashi-Hiroshima, 739-8527, Japan
关键词
Aging of materials - Anodic protection - Corrosion resistance - Current density - Electric potential - Electrochemical corrosion - Ion implantation - Nitrogen - Passivation - Precipitation (chemical) - Surface treatment - Titanium nitride;
D O I
暂无
中图分类号
学科分类号
摘要
N2+ ions were implanted into commercially supplied pure titanium with different doses ranging from 5×1016 to 1×1018 ions/cm2, and the corrosion behavior was investigated in 70% sulphuric acid solution. Anodic polarization curves show that the peak anodic current density, passivation current density, and corrosion potential increase with increase in implantation dose when the dose is less than 1×1017 ions/cm2. When the implanted dose is 5×1017 ions/cm2, the corrosion resistance decreases though it is still larger than no implanted titanium. X-ray diffraction analysis shows the formation of titanium nitride on the implanted surface, i.e., Ti2N is found when the implanted dose is larger than 5×1016 ions/cm2 and both Ti2N and TiN when the implanted dose is 1×1018 ions/cm2. The aging at 673 K after ion implantation largely increases the corrosion resistance, which corresponds to the enhanced precipitation of Ti2N and TiN. AFM observation shows fine particles of titanium nitrides on the implanted surface. It is considered that the precipitation of Ti2N or TiN decreases the effective corrosion area to make the corrosion resistance higher.
引用
收藏
页码:483 / 488
相关论文
共 50 条
  • [1] Effect of N2+ ion implantation on the hydride formation behavior of pure titanium
    Wang, RG
    Kato, M
    Nakasa, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1999, 63 (08) : 1015 - 1021
  • [2] High temperature oxidation behavior N2+ ion implanted pure titanium in air and water vapor
    Wang, RG
    Kato, M
    Nakasa, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2000, 64 (02) : 125 - 133
  • [3] EFFECT OF ION-IMPLANTATION ON CORROSION BEHAVIOR OF PURE IRON .2. CHROMIUM ION-IMPLANTATION
    ASHWORTH, V
    BAXTER, D
    GRANT, WA
    PROCTER, RPM
    CORROSION SCIENCE, 1976, 16 (10) : 775 - 786
  • [4] Effect of N+ ion implantation on the corrosion behavior of titanium sputter-coated with TiN
    Wang, RG
    Kato, M
    Nakasa, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2000, 64 (10) : 887 - 894
  • [5] Effect of titanium ion implantation on the corrosion behavior of zircaloy-4
    Qian Wan
    Xinde Bai
    Xiaoyang Liu
    Journal of Materials Science, 2006, 41 : 2133 - 2135
  • [6] Effect of titanium ion implantation on the corrosion behavior of zircaloy-4
    Wan, Q
    Bai, XD
    Liu, XY
    JOURNAL OF MATERIALS SCIENCE, 2006, 41 (07) : 2133 - 2135
  • [7] Observation of surface of N2+ ion implanted pure titanium by atomic force microscope
    Wang, RG
    Kato, M
    Nakasa, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2000, 64 (08) : 616 - 624
  • [8] Passivation of uranium towards air corrosion by N2+ and C+ ion implantation
    Arkush, R
    Mintz, MH
    Shamir, N
    JOURNAL OF NUCLEAR MATERIALS, 2000, 281 (2-3) : 182 - 190
  • [9] EFFECT OF ION-IMPLANTATION ON CORROSION BEHAVIOR OF PURE IRON .1. ARGON ION-IMPLANTATION
    ASHWORTH, V
    GRANT, WA
    PROCTER, RPM
    WELLINGTON, TC
    CORROSION SCIENCE, 1976, 16 (06) : 393 - 403
  • [10] EFFECT OF ION-IMPLANTATION ON CORROSION BEHAVIOR OF PURE IRON .3. TANTALUM ION-IMPLANTATION
    ASHWORTH, V
    BAXTER, D
    GRANT, WA
    PROCTER, RPM
    CORROSION SCIENCE, 1977, 17 (12) : 947 - 960